Resumo:
OBJECTIVE: To evaluate the clinical performance of glass-ceramic/zirconia crowns fabricated using intraoral digital impressions - a retrospective study with a three-year follow-up. METHODS: 70 consecutive patients with a total of 86 glass-ceramic/zirconia crowns were treated by a single clinician using standardized clinical and laboratory protocols. A complete digital workflow was adopted for the purpose except for the veneering procedure for the glass-ceramic crowns. Occlusal adjustments were made before the ceramic glazing procedure. Before cementation, all abutments where carefully cleaned with a 70% alcoholic solution and air dried. Cementation was performed using dual-curing, self-adhesive resin cement. Patients were re-examined after 12, 24 and 36 months, to assess crown chipping/fractures. RESULTS: After the three-year follow-up, none of the zirconia-based restoration was lost ("apparent" survival rate 100%) otherwise, the chipping rate of the veneering material increased from 9.3% after 12 months, to 14% after 24 months to 30.2% after 36 months. As a consequence, the "real" success rate after 3 years was 69.8%. CONCLUSIONS: After 3 years the success rate of zirconia-based crowns was 69.8%, while the incidence of the chipping was 30.2%. Assuming an exponential increase in chipping rate between 12 and 36 months it can be argued that, among others, the fatigue-mechanism could be advocated as the main factor for the failure of glass-ceramic veneered zirconia especially after 24 months.
Resumo:
OBJECTIVES: To carry out a meta-analysis in order to assess the influencing factors on retention loss and marginal discoloration of cervical restorations made of composites and glass ionomer (derivates). METHODS: The literature was searched for prospective clinical studies on cervical restorations with an observation period of at least 18 months. RESULTS: Fifty clinical studies involving 40 adhesive systems matched the inclusion criteria. On average, 10% of the cervical fillings were lost and 24% exhibited marginal discoloration after 3 years. The variability ranged from 0% to 50% for retention loss and from 0% to 74% for marginal discoloration. Hardly any secondary caries was detected. When linear mixed models with a study and experiment effect were used, the analysis revealed that the adhesive/restorative class had the most significant influence, with 2-step self-etching adhesive systems performing best and 1-step self-etching adhesive systems performing worst; 3-step etch-and-rinse systems, glass ionomers/resin-modified glass ionomers, 2-step etch-and-rinse systems and polyacid-modified resin composites were ranked in between. Restorations placed in teeth whose dentin/enamel had been prepared/roughened showed a statistically significant higher retention rate than those placed in teeth with unprepared dentin (p<0.05). Beveling of the enamel and the type of isolation used (rubberdam/cotton rolls) had no significant influence. SIGNIFICANCE: The clinical performance of cervical restorations is significantly influenced by the type of adhesive system used and/or the adhesive class to which the system belonged and whether the dentin/enamel is prepared or not. 2-Step self-etching- and 3-step etch&rinse systems shall be chosen over 1-step self-etching systems and glass ionomer derivates. The dentin (and enamel) surface shall be roughened before placement of the restoration.
Resumo:
Les résultats des recherches contemporaines, montrant notamment l'importance du raisonnement fluide, de la mémoire de travail (IMT) et de la vitesse de traitement (IVT) dans le fonctionnement cognitif, ont conduit les concepteurs de la WAIS-IV à introduire de nouvelles épreuves pour renforcer l'évaluation de ces dimensions cognitives. L'interprétation des scores de la WAIS-IV repose maintenant sur quatre indices factoriels (ICV, IRP, IMT et IVT), ainsi que sur le QIT. Les concepteurs de la WAIS-IV indiquent que l'un des objectifs de la révision consistait à actualiser les fondements théoriques de cette échelle. Pourtant, la structure globale de la WAIS-IV ne correspond que partiellement à celle proposée dans le modèle qui fait consensus aujourd'hui, le modèle de Cattell-Horn-Carroll (CHC). Par exemple, la WAIS-IV ne propose pas d'indice de raisonnement fluide, bien que les constructeurs soulignent l'importance de cette dimension dans le fonctionnement cognitif. Dans cet article, nous proposons, pour la WAIS-IV, les normes francophones de cinq scores composites CHC, à savoir le raisonnement fluide (Gf), compréhension-connaissances (Gc), le traitement visuel (Gv), la mémoire à court terme (Gsm), et l'IVT (Gs). Ces normes ont été établies en utilisant une procédure d'approximation statistique. À l'instar des scores CHC que nous avons proposés pour le WISCIV, ces normes pour la WAIS-IV permettent aux cliniciens de basculer vers une grille d'interprétation basée sur le modèle dominant et d'utiliser les cinq scores composites CHC en complément des quatre indices standard dans le cadre d'analyses normatives et ipsatives.
Resumo:
OBJECTIVES: (1) To evaluate the changes in surface roughness and gloss after simulated toothbrushing of 9 composite materials and 2 ceramic materials in relation to brushing time and load in vitro; (2) to assess the relationship between surface gloss and surface roughness. METHODS: Eight flat specimens of composite materials (microfilled: Adoro, Filtek Supreme, Heliomolar; microhybrid: Four Seasons, Tetric EvoCeram; hybrid: Compoglass F, Targis, Tetric Ceram; macrohybrid: Grandio), two ceramic materials (IPS d.SIGN and IPS Empress polished) were fabricated according to the manufacturer's instructions and optimally polished with up to 4000 grit SiC. The specimens were subjected to a toothbrushing (TB) simulation device (Willytec) with rotating movements, toothpaste slurry and at three different loads (100g/250g/350g). At hourly intervals from 1h to 10h TB, mean surface roughness Ra was measured with an optical sensor and the surface gloss (Gl) with a glossmeter. Statistical analysis was performed for log-transformed Ra data applying two-way ANOVA to evaluate the interaction between load and material and load and brushing time. RESULTS: There was a significant interaction between material and load as well as between load and brushing time (p<0.0001). The microhybrid and hybrid materials demonstrated more surface deterioration with higher loads, whereas with the microfilled resins Heliomolar and Adoro it was vice versa. For ceramic materials, no or little deterioration was observed over time and independent of the load. The ceramic materials and 3 of the composite materials (roughness) showed no further deterioration after 5h of toothbrushing. Mean surface gloss was the parameter which discriminated best between the materials, followed by mean surface roughness Ra. There was a strong correlation between surface gloss and surface roughness for all the materials except the ceramics. The evaluation of the deterioration curves of individual specimens revealed a more or less synchronous course suspecting hinting specific external conditions and not showing the true variability in relation to the tested material. SIGNIFICANCE: The surface roughness and gloss of dental materials changes with brushing time and load and thus results in different material rankings. Apart from Grandio, the hybrid composite resins were more prone to surface changes than microfilled composites. The deterioration potential of a composite material can be quickly assessed by measuring surface gloss. For this purpose, a brushing time of 10h (=72,000 strokes) is needed. In further comparative studies, specimens of different materials should be tested in one series to estimate the true variability.
Resumo:
Bien que le manuel du WISC-IV fasse référence à la théorie de Cattell-Horn-Carroll (CHC), les indices calculés à partir de cette batterie (ICV, IRP, IMT et IVT) n'ont pas été définis sur la base du modèle CHC. Afin d'apporter un éclairage complémentaire sur les performances observées, nous recommandons néanmoins d'examiner les scores des subtests du WISC-IV en référence à la nomenclature des aptitudes cognitives proposées dans le modèle CHC. La première partie de cet article présente les normes francophones pour cinq facteurs CHC du WISC-IV, à savoir le raisonnement fluide (Gf), compréhension-connaissances (Gc), le traitement visuel (Gv), la mémoire à court terme (Gsm) et la vitesse de traitement (Gs), établies en utilisant une procédure d'approximation statistique. La seconde partie présente l'examen de la validité de ces normes, confrontées à des données recueillies sur un échantillon de 250 enfants. Nos résultats montrent que les corrélations entre les indices classiques du WISC-IV (ICV, IRP, IMT et IVT) et les scores composites CHC sont élevées, attestant de la validité des scores CHC. Ces normes permettent de calculer et d'utiliser les scores composites CHC en complément des indices standard, dans le cadre d'analyses normatives et ipsatives.
Resumo:
OBJECTIVE: The purpose of the present study was to submit the same materials that were tested in the round robin wear test of 2002/2003 to the Alabama wear method. METHODS: Nine restorative materials, seven composites (belleGlass, Chromasit, Estenia, Heliomolar, SureFil, Targis, Tetric Ceram) an amalgam (Amalcap) and a ceramic (IPS Empress) have been submitted to the Alabama wear method for localized and generalized wear. The test centre did not know which brand they were testing. Both volumetric and vertical loss had been determined with an optical sensor. After completion of the wear test, the raw data were sent to IVOCLAR for further analysis. The statistical analysis of the data included logarithmic transformation of the data, the calculation of relative ranks of each material within each test centre, measures of agreement between methods, the discrimination power and coefficient of variation of each method as well as measures of the consistency and global performance for each material. RESULTS: Relative ranks of the materials varied tremendously between the test centres. When all materials were taken into account and the test methods compared with each other, only ACTA agreed reasonably well with two other methods, i.e. OHSU and ZURICH. On the other hand, MUNICH did not agree with the other methods at all. The ZURICH method showed the lowest discrimination power, ACTA, IVOCLAR and ALABAMA localized the highest. Material-wise, the best global performance was achieved by the leucite reinforced ceramic material Empress, which was clearly ahead of belleGlass, SureFil and Estenia. In contrast, Heliomolar, Tetric Ceram and especially Chromasit demonstrated a poor global performance. The best consistency was achieved by SureFil, Tetric Ceram and Chromasit, whereas the consistency of Amalcap and Heliomolar was poor. When comparing the laboratory data with clinical data, a significant agreement was found for the IVOCLAR and ALABAMA generalized wear method. SIGNIFICANCE: As the different wear simulator settings measure different wear mechanisms, it seems reasonable to combine at least two different wear settings to assess the wear resistance of a new material.
Resumo:
Purpose: The aim of this study was to evaluate the clinical fracture rate of crowns fabricated with the pressable, leucite-reinforced ceramic IPS Empress, and relate the results to the type of tooth restored. Materials and Methods: The database SCOPUS was searched for clinical studies involving full-coverage crowns made of IPS Empress. To assess the fracture rate of the crowns in relation to the type of restored tooth and study, Poisson regression analysis was used. Results: Seven clinical studies were identified involving 1,487 adhesively luted crowns (mean observation time: 4.5 +/- 1.7 years) and 81 crowns cemented with zinc-phosphate cement (mean observation time: 1.6 +/- 0.8 years). Fifty-seven of the adhesively luted crowns fractured (3.8%). The majority of fractures (62%) occurred between the third and sixth year after placement. There was no significant influence regarding the test center on fracture rate, but the restored tooth type played a significant role. The hazard rate (per year) for crowns was estimated to be 5 in every 1,000 crowns for incisors, 7 in every 1,000 crowns for premolars, 12 in every 1,000 crowns for canines, and 16 in every 1,000 crowns for molars. One molar crown in the zinc-phosphate group fractured after 1.2 years. Conclusion: Adhesively luted IPS Empress crowns showed a low fracture rate for incisors and premolars and a somewhat higher rate for molars and canines. The sample size of the conventionally luted crowns was too small and the observation period too short to draw meaningful conclusions. Int J Prosthodont 2010;23:129-133.
Resumo:
Different anchoring groups have been studied with the aim of covalently binding organic linkers to the surface of alumina ceramic foams. The results suggested that a higher degree of functionalization was achieved with a pyrogallol derivative - as compared to its catechol analogue - based on the XPS analysis of the ceramic surface. The conjugation of organic ligands to the surface of these alumina materials was corroborated by DNP-MAS NMR measurements.
Resumo:
OBJECTIVES: This is the first meta-analysis on the efficacy of composite resin restorations in anterior teeth. The objective of the present meta-analysis was to verify whether specific material classes, tooth conditioning methods and operational procedures influence the result for Class III and Class IV restorations. MATERIAL AND METHODS: The database SCOPUS and PubMed were searched for clinical trials on anterior resin composites without restricting the search to the year of publication. The inclusion criteria were: (1) prospective clinical trial with at least 2 years of observation; (2) minimal number of restorations at last recall=20; (3) report on drop-out rate; (4) report of operative technique and materials used in the trial, and (5) utilization of Ryge or modified Ryge evaluation criteria. For the statistical analysis, a linear mixed model was used with random effects to account for the heterogeneity between the studies. p-Values smaller than 0.05 were considered to be significant. RESULTS: Of the 84 clinical trials, 21 studies met the inclusion criteria, 14 of them for Class III restorations, 6 for Class IV restorations and 1 for closure of diastemata; the latter was included in the Class IV group. Twelve of the 21 studies started before 1991 and 18 before 2001. The estimated median overall success rate (without replacement) after 10 years for Class III composite resin restorations was 95% and for Class IV restorations 90%. The main reason for the replacement of Class IV restorations was bulk fractures, which occurred significantly more frequently with microfilled composites than with hybrid and macrofilled composites. Caries adjacent to restorations was infrequent in most studies and accounted only for about 2.5% of all replaced restorations after 10 years irrespective of the cavity class. Class III restorations with glass ionomer derivates suffered significantly more loss of anatomical form than did fillings with other types of material. When the enamel was acid-etched and no bonding agent was applied, significantly more restorations showed marginal staining and detectable margins compared to enamel etching with enamel bonding or the total etch technique; fillings with self-etching systems were in between of these two outcome variables. Bevelling of the enamel was associated with a significantly reduced deterioration of the anatomical form compared to no bevelling but not with less marginal staining or less detectable margins. The type of isolation (absolute/relative) had a statistically significant influence on marginal caries which, however, might be a random finding.
Resumo:
PURPOSE: To meta-analyze the literature on the clinical performance of Class V restorations to assess the factors that influence retention, marginal integrity, and marginal discoloration of cervical lesions restored with composite resins, glass-ionomer-cement-based materials [glass-ionomer cement (GIC) and resin-modified glass ionomers (RMGICs)], and polyacid-modified resin composites (PMRC). MATERIALS AND METHODS: The English literature was searched (MEDLINE and SCOPUS) for prospective clinical trials on cervical restorations with an observation period of at least 18 months. The studies had to report about retention, marginal discoloration, marginal integrity, and marginal caries and include a description of the operative technique (beveling of enamel, roughening of dentin, type of isolation). Eighty-one studies involving 185 experiments for 47 adhesives matched the inclusion criteria. The statistical analysis was carried out by using the following linear mixed model: log (-log (Y /100)) = β + α log(T ) + error with β = log(λ), where β is a summary measure of the non-linear deterioration occurring in each experiment, including a random study effect. RESULTS: On average, 12.3% of the cervical restorations were lost, 27.9% exhibited marginal discoloration, and 34.6% exhibited deterioration of marginal integrity after 5 years. The calculation of the clinical index was 17.4% of failures after 5 years and 32.3% after 8 years. A higher variability was found for retention loss and marginal discoloration. Hardly any secondary caries lesions were detected, even in the experiments with a follow-up time longer than 8 years. Restorations placed using rubber-dam in teeth whose dentin was roughened showed a statistically significantly higher retention rate than those placed in teeth with unprepared dentin or without rubber-dam (p < 0.05). However, enamel beveling had no influence on any of the examined variables. Significant differences were found between pairs of adhesive systems and also between pairs of classes of adhesive systems. One-step self-etching had a significantly worse clinically index than two-step self-etching and three-step etch-and-rinse (p = 0.026 and p = 0.002, respectively). CONCLUSION: The clinical performance is significantly influenced by the type of adhesive system and/or the adhesive class to which the system belongs. Whether the dentin/enamel is roughened or not and whether rubberdam isolation is used or not also significantly influenced the clinical performance. Composite resin restorations placed with two-step self-etching and three-step etch-and-rinse adhesive systems should be preferred over onestep self-etching adhesive systems, GIC-based materials, and PMRCs.