8 resultados para Glass ionomer

em Université de Lausanne, Switzerland


Relevância:

60.00% 60.00%

Publicador:

Resumo:

OBJECTIVES: To carry out a meta-analysis in order to assess the influencing factors on retention loss and marginal discoloration of cervical restorations made of composites and glass ionomer (derivates). METHODS: The literature was searched for prospective clinical studies on cervical restorations with an observation period of at least 18 months. RESULTS: Fifty clinical studies involving 40 adhesive systems matched the inclusion criteria. On average, 10% of the cervical fillings were lost and 24% exhibited marginal discoloration after 3 years. The variability ranged from 0% to 50% for retention loss and from 0% to 74% for marginal discoloration. Hardly any secondary caries was detected. When linear mixed models with a study and experiment effect were used, the analysis revealed that the adhesive/restorative class had the most significant influence, with 2-step self-etching adhesive systems performing best and 1-step self-etching adhesive systems performing worst; 3-step etch-and-rinse systems, glass ionomers/resin-modified glass ionomers, 2-step etch-and-rinse systems and polyacid-modified resin composites were ranked in between. Restorations placed in teeth whose dentin/enamel had been prepared/roughened showed a statistically significant higher retention rate than those placed in teeth with unprepared dentin (p<0.05). Beveling of the enamel and the type of isolation used (rubberdam/cotton rolls) had no significant influence. SIGNIFICANCE: The clinical performance of cervical restorations is significantly influenced by the type of adhesive system used and/or the adhesive class to which the system belonged and whether the dentin/enamel is prepared or not. 2-Step self-etching- and 3-step etch&rinse systems shall be chosen over 1-step self-etching systems and glass ionomer derivates. The dentin (and enamel) surface shall be roughened before placement of the restoration.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

OBJECTIVE: To determine if the results of resin-dentin microtensile bond strength (µTBS) is correlated with the outcome parameters of clinical studies on non-retentive Class V restorations. METHODS: Resin-dentin µTBS data were obtained from one test center; the in vitro tests were all performed by the same operator. The µTBS testing was performed 8h after bonding and after 6 months of storing the specimens in water. Pre-test failures (PTFs) of specimens were included in the analysis, attributing them a value of 1MPa. Prospective clinical studies on cervical restorations (Class V) with an observation period of at least 18 months were searched in the literature. The clinical outcome variables were retention loss, marginal discoloration and marginal integrity. Furthermore, an index was formulated to be better able to compare the laboratory and clinical results. Estimates of adhesive effects in a linear mixed model were used to summarize the clinical performance of each adhesive between 12 and 36 months. Spearman correlations between these clinical performances and the µTBS values were calculated subsequently. RESULTS: Thirty-six clinical studies with 15 adhesive/restorative systems for which µTBS data were also available were included in the statistical analysis. In general 3-step and 2-step etch-and-rinse systems showed higher bond strength values than the 2-step/3-step self-etching systems, which, however, produced higher values than the 1-step self-etching and the resin modified glass ionomer systems. Prolonged water storage of specimens resulted in a significant decrease of the mean bond strength values in 5 adhesive systems (Wilcoxon, p<0.05). There was a significant correlation between µTBS values both after 8h and 6 months of storage and marginal discoloration (r=0.54 and r=0.67, respectively). However, the same correlation was not found between µTBS values and the retention rate, clinical index or marginal integrity. SIGNIFICANCE: As µTBS data of adhesive systems, especially after water storage for 6 months, showed a good correlation with marginal discoloration in short-term clinical Class V restorations, longitudinal clinical trials should explore whether early marginal staining is predictive for future retention loss in non-carious cervical restorations.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

OBJECTIVES: This is the first meta-analysis on the efficacy of composite resin restorations in anterior teeth. The objective of the present meta-analysis was to verify whether specific material classes, tooth conditioning methods and operational procedures influence the result for Class III and Class IV restorations. MATERIAL AND METHODS: The database SCOPUS and PubMed were searched for clinical trials on anterior resin composites without restricting the search to the year of publication. The inclusion criteria were: (1) prospective clinical trial with at least 2 years of observation; (2) minimal number of restorations at last recall=20; (3) report on drop-out rate; (4) report of operative technique and materials used in the trial, and (5) utilization of Ryge or modified Ryge evaluation criteria. For the statistical analysis, a linear mixed model was used with random effects to account for the heterogeneity between the studies. p-Values smaller than 0.05 were considered to be significant. RESULTS: Of the 84 clinical trials, 21 studies met the inclusion criteria, 14 of them for Class III restorations, 6 for Class IV restorations and 1 for closure of diastemata; the latter was included in the Class IV group. Twelve of the 21 studies started before 1991 and 18 before 2001. The estimated median overall success rate (without replacement) after 10 years for Class III composite resin restorations was 95% and for Class IV restorations 90%. The main reason for the replacement of Class IV restorations was bulk fractures, which occurred significantly more frequently with microfilled composites than with hybrid and macrofilled composites. Caries adjacent to restorations was infrequent in most studies and accounted only for about 2.5% of all replaced restorations after 10 years irrespective of the cavity class. Class III restorations with glass ionomer derivates suffered significantly more loss of anatomical form than did fillings with other types of material. When the enamel was acid-etched and no bonding agent was applied, significantly more restorations showed marginal staining and detectable margins compared to enamel etching with enamel bonding or the total etch technique; fillings with self-etching systems were in between of these two outcome variables. Bevelling of the enamel was associated with a significantly reduced deterioration of the anatomical form compared to no bevelling but not with less marginal staining or less detectable margins. The type of isolation (absolute/relative) had a statistically significant influence on marginal caries which, however, might be a random finding.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

PURPOSE: To meta-analyze the literature on the clinical performance of Class V restorations to assess the factors that influence retention, marginal integrity, and marginal discoloration of cervical lesions restored with composite resins, glass-ionomer-cement-based materials [glass-ionomer cement (GIC) and resin-modified glass ionomers (RMGICs)], and polyacid-modified resin composites (PMRC). MATERIALS AND METHODS: The English literature was searched (MEDLINE and SCOPUS) for prospective clinical trials on cervical restorations with an observation period of at least 18 months. The studies had to report about retention, marginal discoloration, marginal integrity, and marginal caries and include a description of the operative technique (beveling of enamel, roughening of dentin, type of isolation). Eighty-one studies involving 185 experiments for 47 adhesives matched the inclusion criteria. The statistical analysis was carried out by using the following linear mixed model: log (-log (Y /100)) = β + α log(T ) + error with β = log(λ), where β is a summary measure of the non-linear deterioration occurring in each experiment, including a random study effect. RESULTS: On average, 12.3% of the cervical restorations were lost, 27.9% exhibited marginal discoloration, and 34.6% exhibited deterioration of marginal integrity after 5 years. The calculation of the clinical index was 17.4% of failures after 5 years and 32.3% after 8 years. A higher variability was found for retention loss and marginal discoloration. Hardly any secondary caries lesions were detected, even in the experiments with a follow-up time longer than 8 years. Restorations placed using rubber-dam in teeth whose dentin was roughened showed a statistically significantly higher retention rate than those placed in teeth with unprepared dentin or without rubber-dam (p < 0.05). However, enamel beveling had no influence on any of the examined variables. Significant differences were found between pairs of adhesive systems and also between pairs of classes of adhesive systems. One-step self-etching had a significantly worse clinically index than two-step self-etching and three-step etch-and-rinse (p = 0.026 and p = 0.002, respectively). CONCLUSION: The clinical performance is significantly influenced by the type of adhesive system and/or the adhesive class to which the system belongs. Whether the dentin/enamel is roughened or not and whether rubberdam isolation is used or not also significantly influenced the clinical performance. Composite resin restorations placed with two-step self-etching and three-step etch-and-rinse adhesive systems should be preferred over onestep self-etching adhesive systems, GIC-based materials, and PMRCs.

Relevância:

20.00% 20.00%

Publicador: