55 resultados para Nickel alloys
Resumo:
Geometric parameters of binary (1:1) PdZn and PtZn alloys with CuAu-L10 structure were calculated with a density functional method. Based on the total energies, the alloys are predicted to feature equal formation energies. Calculated surface energies of PdZn and PtZn alloys show that (111) and (100) surfaces exposing stoichiometric layers are more stable than (001) and (110) surfaces comprising alternating Pd (Pt) and Zn layers. The surface energy values of alloys lie between the surface energies of the individual components, but they differ from their composition weighted averages. Compared with the pure metals, the valence d-band widths and the Pd or Pt partial densities of states at the Fermi level are dramatically reduced in PdZn and PtZn alloys. The local valence d-band density of states of Pd and Pt in the alloys resemble that of metallic Cu, suggesting that a similar catalytic performance of these systems can be related to this similarity in the local electronic structures.
Resumo:
We have observed a type of giant magnetoresistance (GMR) in magnetic granular Co10Cu90 alloys. The asymmetric GMR depends strongly on the size of magnetic Co particles, which exhibit superparamagnetic behavior at given measured temperature. The asymmetric GMR points to a metastable state that develops when the sample is field-cooled, which is lost after recycling. We propose that high-field cooling produces more effective parallel alignment of small unblocked Co particle moments and interfacial magnetizations, which contributes to the further decrease of the resistance in comparison with the samples zero-field-cooled, and then applied to the same field.
Resumo:
The Heusler alloy Ni50 Mn37 Sn13 was successfully produced as ribbon flakes of thickness around 7-10 μm melt spinning. Fracture cross section micrographs in the ribbon show the formation of a microcrystalline columnarlike microstructure, with their longer axes perpendicular to the ribbon plane. Phase transition temperatures of the martensite-austenite transformation were found to be MS =218 K, Mf =207 K, AS =224 K, and Af =232 K; the thermal hysteresis of the transformation is 15 K. Ferromagnetic L 21 bcc austenite phase shows a Curie point of 313 K, with cell parameter a=0.5971 (5) nm at 298 K, transforming into a modulated 7M orthorhombic martensite with a=0.6121 (7) nm, b=0.6058 (8) nm, and c=0.5660 (2) nm, at 150 K
Resumo:
The most extensively studied Heusler alloys are those based on the Ni-Mn-Ga system. However, to overcome the high cost of Gallium and the usually low martensitic transformation temperature, the search for Ga-free alloys has been recently attempted, particularly, by introducing In, Sn or Sb. In this work, two alloys (Mn50Ni35.5In14.5 and Ni50Mn35In15) have been obtained by melt spinning. We outline their structural and thermal behaviour. Mn50Ni35.5In14.5 alloy has the transformation above room temperature whereas Ni50Mn35In15 does not have this transformation in the temperature range here analyzed
Resumo:
We present results from both, calorimetric and dilatometric studies of the isothermal ordering process taking place in a Cu-Zn-Al shape memory alloy after quenches from Tq temperatures ranging from 350 K to 1200 K. The dissipated energy and the length variations of the system are obtained during the process. The change of these quantities in the whole process have been compared with the difference [MATH] between Ms, measured after the relaxation and Ms measured just after the quench. We obtain that these three quantities present, as a function of Tq, the same qualitative behaviour. These changes are then associated with changes of the L21 ordering after the quench in the system. The relaxational process does not follow a single exponential decay. Instead, a continuous slowing down is observed. A relaxation time [MATH] has been defined to characterize the relaxation rate. We show that [MATH] depends on both the annealing and the quenching (Tq [MATH] 800 K) temperatures through an Arrhenius law.
Resumo:
Magnetization versus temperature in the temperature interval 2-200 K was measured for amorphous alloys of three different compositions: Fe 81.5B14.5Si4, Fe40Ni38 Mo4B18, and Co70Fe5Ni 2Mo3B5Si15. The measurements were performed by means of a SQUID (superconducting quantum interference device) magnetometer. The aim was to extract information about the different mechanisms contributing to thermal demagnetization. A powerful data analysis technique based on successive minimization procedures has demonstrated that Stoner excitations of the strong ferromagnetic type play a significant role in the Fe-Ni alloy studied. The Fe-rich and Co-rich alloys do not show a measurable contribution from single-particle excitations.
Resumo:
A thermally controlled transport device was designed and tested. As hot food needs to be transported at temperatures between 60 and 70ºC in order to avoid contamination by microorganisms, the use of Molecular Alloy Phase Change Materials (MAPCM) can lead to improvements in this field of application. A heat transfer numerical simulation of the box used for transporting the food was conducted. Despite obvious simplifications, a good agreement between numerical simulation and experimental results was obtained. Furthermore, we compared our experimental results with those from other experiments related to the transport of hot food. Here, pizza is taken as the example, and it is shown that delivering time can be increased three-fold.
Resumo:
A Monte Carlo simulation study of the vacancy-assisted domain growth in asymmetric binary alloys is presented. The system is modeled using a three-state ABV Hamiltonian which includes an asymmetry term. Our simulated system is a stoichiometric two-dimensional binary alloy with a single vacancy which evolves according to the vacancy-atom exchange mechanism. We obtain that, compared to the symmetric case, the ordering process slows down dramatically. Concerning the asymptotic behavior it is algebraic and characterized by the Allen-Cahn growth exponent x51/2. The late stages of the evolution are preceded by a transient regime strongly affected by both the temperature and the degree of asymmetry of the alloy. The results are discussed and compared to those obtained for the symmetric case.