55 resultados para Glass-fibre Reinforced Cement


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polyolefins are especially difficult to bond due to their non-polar, non-porous and chemically inert surfaces. Acrylic adhesives used in industry are particularly suited to bond these materials, including many grades of polypropylene (PP) and polyethylene (PE), without special surface preparation. In this work, the tensile strength of single-lap PE and mixed joints bonded with an acrylic adhesive was investigated. The mixed joints included PE with aluminium (AL) or carbon fibre reinforced plastic (CFRP) substrates. The PE substrates were only cleaned with isopropanol, which assured cohesive failures. For the PE CFRP joints, three different surfaces preparations were employed for the CFRP substrates: cleaning with acetone, abrasion with 100 grit sand paper and peel-ply finishing. In the PE AL joints, the AL bonding surfaces were prepared by the following methods: cleaning with acetone, abrasion with 180 and 320 grit sand papers, grit blasting and chemical etching with chromic acid. After abrasion of the CFRP and AL substrates, the surfaces were always cleaned with acetone. The tensile strengths were compared with numerical results from ABAQUS® and a mixed mode (I+II) cohesive damage model. A good agreement was found between the experimental and numerical results, except for the PE AL joints, since the AL surface treatments were not found to be effective.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The interlaminar fracture toughness in pure mode II (GIIc) of a Carbon-Fibre Reinforced Plastic (CFRP) composite is characterized experimentally and numerically in this work, using the End-Notched Flexure (ENF) fracture characterization test. The value of GIIc was extracted by a new data reduction scheme avoiding the crack length measurement, named Compliance-Based Beam Method (CBBM). This method eliminates the crack measurement errors, which can be non-negligible, and reflect on the accuracy of the fracture energy calculations. Moreover, it accounts for the Fracture Process Zone (FPZ) effects. A numerical study using the Finite Element Method (FEM) and a triangular cohesive damage model, implemented within interface finite elements and based on the indirect use of Fracture Mechanics, was performed to evaluate the suitability of the CBBM to obtain GIIc. This was performed comparing the input values of GIIc in the numerical models with the ones resulting from the application of the CBBM to the numerical load-displacement (P-) curve. In this numerical study, the Compliance Calibration Method (CCM) was also used to extract GIIc, for comparison purposes.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Hole drilling operations are common in fibre reinforced plastics - FRP’s - to facilitate fastener assembly to other parts in more complex structures. As these materials are non-homogeneous, drilling causes some damages, like delamination, for example. Delamination can be reduced by a careful selection of drilling parameters, drill material and drill bit geometry. In this work two types of laminates are drilled using different machining parameters and comparing drill geometries. Results show the importance of a cautious selection of these variables when composites’ drilling is involved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

“Drilling of polymeric matrix composites structures”

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The increasing use of Carbon-Fibre Reinforced Plastic (CFRP) laminates in high responsibility applications introduces an issue regarding their handling after damage. The availability of efficient repair methods is essential to restore the strength of the structure. The availability of accurate predictive tools for the repairs behaviour is also essential for the reduction of costs and time associated to extensive tests. This work reports on a numerical study of the tensile behaviour of three-dimensional (3D) adhesively-bonded scarf repairs in CFRP structures, using a ductile adhesive. The Finite Element (FE) analysis was performed in ABAQUS® and Cohesive Zone Models (CZM’s) was used for the simulation of damage in the adhesive layer. A parametric study was performed on two geometric parameters. The use of overlaminating plies covering the repaired region at the outer or both repair surfaces was also tested as an attempt to increase the repairs efficiency. The results allowed the proposal of design principles for repairing CFRP structures.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In the injection moulding of polypropylene reinforced with hard glass fibres, die materials are commonly subjected to severe abrasive wear. In order to improve its wear resistance, an unbalanced magnetron sputtering PVD compositional monolayered coating has been produced. The film was composed by a nanostructured TiB2 monolayer. Microstructure characterization and thickness evaluation were conducted by scanning electron microscopy (SEM). Film topography and roughness were accessed by SEM and Atomic Force Microscopy (AFM). The phase analyse was investigated by X-ray diffraction (XRD), using Cu Kalpha radiation. Scratch tests were conducted in order to study the film adhesion to the substrate. Load-Displacement curves (nanoindentation analysis) allowed measuring the film hardness and Young's modulus. A ball-cratering tribometer was used to determine the micro-abrasion laboratorial wear resistance, under different tests conditions, using SiC particles in distilled water slurry. At the end of these tests, the worn surfaces were analyzed by SEM and Energy Dispersive X-ray Spectroscopy (EDS) in order to compare these results with some other coatings already tested in the same conditions. To test the practical wear resistance, 135000 injection cycles were done in a plastic injection industrial mould. Coated samples were put on the plastic feed canal, after a turbulent zone. In these tests, a 30% (wt) glass fibres reinforced polypropylene was used. Worn sample surfaces were analyzed by SEM after 45.000 and 90.000 cycles. Image analyses were made in order to evaluate the damage increases and to observe the wear mechanisms involved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The injection process of glass fibres reinforced plastics promotes the moulds surface degradation by erosion. In order to improve its wear resistance, several kinds of PVD thin hard coatings were used. It is well-known that nanostructures present a better compromise between hardness and toughness. Indeed, when the coating is constituted by a large number of ultra-thin different layers, cracks and interface troubles tend to decrease. However, it is not clear that these nanostructures present a better wear behaviour in erosion processes. In order to study its wear behaviour, a sputtered PVD nanostructured TiAlCrSiN coating was used. The substrate and film surfaces topography were analyzed by profilometry and atomic force microscopy techniques. Film adhesion to the substrate was evaluated by scratch tests. The surface hardness was measured with a Vickers micro-hardness tester. The wear resistance was evaluated by micro-abrasion with a rotating ball tribometer tests. Slurry of SiC particles in distilled water was used in order to provoke the surface abrasion. Different duration tests were performed in order to analyze the wear evolution. After these tests, the wear mechanisms developed were analyzed by scanning electron microscopy. Wear craters were measured and the wear rate was calculated and discussed. With the same purpose, coated inserts were mounted in an injection mould working with a 30% glass fibres reinforced polypropylene. After 45 000 cycles no relevant wear was registered.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The characteristics of carbon fibre reinforced laminates have widened their use from aerospace to domestic appliances, and new possibilities for their usage emerge almost daily. In many of the possible applications, the laminates need to be drilled for assembly purposes. It is known that a drilling process that reduces the drill thrust force can decrease the risk of delamination. In this work, damage assessment methods based on data extracted from radiographic images are compared and correlated with mechanical test results—bearing test and delamination onset test—and analytical models. The results demonstrate the importance of an adequate selection of drilling tools and machining parameters to extend the life cycle of these laminates as a consequence of enhanced reliability.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The aim of this study is to optimize the heat flow through the pultrusion die assembly system on the manufacturing process of a specific glass-fiber reinforced polymer (GFRP) pultrusion profile. The control of heat flow and its distribution through whole die assembly system is of vital importance in optimizing the actual GFRP pultrusion process. Through mathematical modeling of heating-die process, by means of Finite Element Analysis (FEA) program, an optimum heater selection, die position and temperature control was achieved. The thermal environment within the die was critically modeled relative not only to the applied heat sources, but also to the conductive and convective losses, as well as the thermal contribution arising from the exothermic reaction of resin matrix as it cures or polymerizes from the liquid to solid condition. Numerical simulation was validated with basis on thermographic measurements carried out on key points along the die during pultrusion process.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Pultrusion is an industrial process used to produce glass fibers reinforced polymers profiles. These materials are worldwide used when performing characteristics, such as great electrical and magnetic insulation, high strength to weight ratio, corrosion and weather resistance, long service life and minimal maintenance are required. In this study, we present the results of the modelling and simulation of heat flow through a pultrusion die by means of Finite Element Analysis (FEA). The numerical simulation was calibrated based on temperature profiles computed from thermographic measurements carried out during pultrusion manufacturing process. Obtained results have shown a maximum deviation of 7%, which is considered to be acceptable for this type of analysis, and is below to the 10% value, previously specified as maximum deviation. © 2011, Advanced Engineering Solutions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

As ligações adesivas são frequentemente utilizadas na fabricação de estruturas complexas que não poderiam ou não seriam tão fáceis de ser fabricadas numa só peça, a fim de proporcionar uma união estrutural que, teoricamente, deve ser pelo menos tão resistente como o material de base. As juntas adesivas têm vindo a substituir métodos como a soldadura, e ligações parafusadas e rebitadas, devido à facilidade de fabricação, menor custo, facilidade em unir materiais diferentes, melhor resistência, entre outras características. Os materiais compósitos reforçados com fibra de carbono são amplamente utilizados em muitas indústrias, tais como de construção de barcos, automóvel e aeronáutica, sendo usados em estruturas que requerem elevada resistência e rigidez específicas, o que reduz o peso dos componentes, mantendo a resistência e rigidez necessárias para suportar as diversas cargas aplicadas. Embora estes métodos de fabricação reduzam ao máximo as ligações através de técnicas de fabrico avançadas, estas ainda são necessárias devido ao tamanho dos componentes, limitações de projecto tecnológicas e logísticas. Em muitas estruturas, a combinação de compósitos com metais tais como alumínio ou titânio traz vantagens de projecto. Este trabalho tem como objectivo estudar, experimentalmente e por modelos de dano coesivo (MDC), juntas adesivas em L entre componentes de alumínio e compósito de carbono epóxido quando solicitados a forças de arrancamento, considerando diferentes configurações de junta e adesivos de ductilidade distinta. Os parâmetros geométricos abordados são a espessura do aderente de alumínio (tP2) e comprimento de sobreposição (LO). A análise numérica permitiu o estudo da distribuição das tensões, evolução do dano, resistência e modos de rotura. Os testes experimentais validam os resultados numéricos e fornecem mecanismos de projecto para juntas em L. Foi mostrado que a geometria do aderente em L (alumínio) e o tipo de adesivo têm uma influência directa na resistência de junta.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

With the need to find an alternative way to mechanical and welding joints, and at the same time to overcome some limitations linked to these traditional techniques, adhesive bonds can be used. Adhesive bonding is a permanent joining process that uses an adhesive to bond the components of a structure. Composite materials reinforced with fibres are becoming increasingly popular in many applications as a result of a number of competitive advantages. In the manufacture of composite structures, although the fabrication techniques reduce to the minimum by means of advanced manufacturing techniques, the use of connections is still required due to the typical size limitations and design, technological and logistical aspects. Moreover, it is known that in many high performance structures, unions between composite materials with other light metals such as aluminium are required, for purposes of structural optimization. This work deals with the experimental and numerical study of single lap joints (SLJ), bonded with a brittle (Nagase Chemtex Denatite XNRH6823) and a ductile adhesive (Nagase Chemtex Denatite XNR6852). These are applied to hybrid joints between aluminium (AL6082-T651) and carbon fibre reinforced plastic (CFRP; Texipreg HS 160 RM) adherends in joints with different overlap lengths (LO) under a tensile loading. The Finite Element (FE) Method is used to perform detailed stress and damage analyses allowing to explain the joints’ behaviour and the use of cohesive zone models (CZM) enables predicting the joint strength and creating a simple and rapid design methodology. The use of numerical methods to simulate the behaviour of the joints can lead to savings of time and resources by optimizing the geometry and material parameters of the joints. The joints’ strength and failure modes were highly dependent on the adhesive, and this behaviour was successfully modelled numerically. Using a brittle adhesive resulted in a negligible maximum load (Pm) improvement with LO. The joints bonded with the ductile adhesive showed a nearly linear improvement of Pm with LO.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Adhesive bonding has become more efficient in the last few decades due to the adhesives developments, granting higher strength and ductility. On the other hand, natural fibre composites have recently gained interest due to the low cost and density. It is therefore essential to predict the fracture behavior of joints between these materials, to assess the feasibility of joining or repairing with adhesives. In this work, the tensile fracture toughness (Gc n) of adhesive joints between natural fibre composites is studied, by bonding with a ductile adhesive and co-curing. Conventional methods to obtain Gc n are used for the co-cured specimens, while for the adhesive within the bonded joint, the J-integral is considered. For the J-integral calculation, an optical measurement method is developed for the evaluation of the crack tip opening and adherends rotation at the crack tip during the test, supported by a Matlab sub-routine for the automated extraction of these quantities. As output of this work, an optical method that allows an easier and quicker extraction of the parameters to obtain Gc n than the available methods is proposed (by the J-integral technique), and the fracture behaviour in tension of bonded and co-cured joints in jute-reinforced natural fibre composites is also provided for the subsequent strength prediction. Additionally, for the adhesively- bonded joints, the tensile cohesive law of the adhesive is derived by the direct method.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

n the last decades the biocomposites have been widely used in the construction, automobile and aerospace industries. Not only the interface transition zone (ITZ) but also the heterogeneity of natural fibres affects the mechanical behaviour of these composites. This work focuses on the numerical and experimental analyses of a polymeric composite fabricated with epoxy resin and unidirectional sisal and banana fibres. A three-dimensional model was set to analyze the composites using the elastic properties of the individual phases. In addition, a two-dimensional model was set taking into account the effective composite properties obtained by micromechanical models. A tensile testing was performed to validate the numerical analyses and evaluating the interface condition of the constitutive phases.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper describes the design and manufacture of a low-cost full scale pultrusion prototype equipment and discusses the production and obtained mechanical properties of polypropylene/glass (GF/PP) reinforced composite ba rs fabricated by using the prototype equipment. Three different GF/PP pre-impregnated ra w-materials, a commercial GF/PP comingled system from Vetrotex, a GF/PP powder coat ed towpreg [1-3] and, a GF/PP pre- consolidated tape (PCT) produced in our laboratorie s, were used in the production of composite bars that were subsequently submitted to mechanical testing in order to determine the relevant mechanical properties and quantify the consolidation quality. Samples of the different composite profiles were also observed und er SEM microscopy.