Resumo:

Eucalyptus globulus heartwood, sapwood and their delignified samples by kraft pulping at 130, 150 and 170 degrees C along time were characterized in respect to total carbohydrates by Py-GC/MS(FID). No significant differences between heartwood and sapwood were found in relation to pyrolysis products and composition. The main wood carbohydrate derived pyrolysis compounds were levoglucosan (25.1%), hydroxyacetaldehyde (12.5%), 2-oxo-propanal (10.3%) and acetic acid (8.7%). Levoglucosan decreased during the early stages of delignification and increased during the bulk and residual phases. Acetic acid decreased hydroxyacetaldehyde and 2-oxo-propanal increased, and 2-furaldehyde and hydroxypropanone remained almost constant during delignification. The C/L ratio was 3.2 in wood and remained rather constant in the first pulping periods until a loss of 15-25% in carbohydrate and 60% in lignin. Afterwards it increased sharply until 44 that correspond to the removal of 25-35% of carbohydrates and 95% of lignin. The pulping reactive selectivity to lignin vs. polysaccharides was the same for sapwood and heartwood. (C) 2013 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The kraft pulps produced from heartwood and sapwood of Eucalyptus globulus at 130 degrees C, 150 degrees C, and 170 degrees C were characterized by wet chemistry (total lignin as sum of Klason and soluble lignin fractions) and pyrolysis (total lignin denoted as py-lignin). The total lignin content obtained with both methods was similar. In the course of delignification, the py-lignin values were higher (by 2 to 5%) compared to Klason values, which is in line with the importance of soluble lignin for total lignin determination. Pyrolysis analysis presents advantages over wet chemical procedures, and it can be applied to wood and pulps to determine lignin contents at different stages of the delignification process. The py-lignin values were used for kinetic modelling of delignification, with very high predictive value and results similar to those of modelling using wet chemical determinations.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Cork samples from Betula pendula, Quercus suber and Quercus cerris were submitted to Py-GC-MS/FID at temperatures between 550 degrees C and 900 degrees C and the pyrolysis-derived compounds (py-products) were identified and quantified. Corks were compared with wood samples. Py-products include suberin, lignin and carbohydrates derivatives. Suberin py-products are dominated by unsaturated aliphatics. Corks pyrolysis yield and composition were dramatically influenced by temperature in contrast to wood that showed stable results across temperatures. At 850-900 degrees C the peaks area of cork pyrograms were approximately two times higher than at 550 degrees C, for which yield was about half of the woods, and cork py-products were dominated by suberin-derived short chain aliphatics, namely 1-alkenes, while at 550 degrees C composition was dominated by lignin derivatives. Lignin and carbohydrate derived products decreased dramatically over 750 degrees C while the opposite was observed for unsaturated aliphatics. Cork materials show a high potential as feedstock for production of aliphatic-rich pyrolytic biofuels or as a source of olefins. (C) 2014 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Eucalyptus globulus sapwood and heartwood showed no differences in lignin content (23.0% vs. 23.7%) and composition: syringyl-lignin (17.9% vs. 18.0%) and guaiacyl-lignin (4.8% vs. 5.2%). Delignification kinetics of S- and G-units in heartwood and sapwood was investigated by Py-GC–MS/FID at 130, 150 and 170 °C and modeled as double first-order reactions. Reactivity differences between S and G-units were small during the main pulping phase and the higher reactivity of S over G units was better expressed in the later pulping stage. The residual lignin composition in pulps was different from wood or from samples in the initial delignification stages, with more G and H-units. S/G ratio ranged from 3 to 4.5 when pulp residual lignin was higher than 10%, decreasing rapidly to less than 1. The S/H was initially around 20 (until 15% residual lignin), decreasing to 4 when residual lignin was about 3%.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Four Cynara cardunculus clones, two from Portugal and two from Spain were studied for biomass production and their lignin was characterized. The clones differed in biomass partitioning: Spanish clones produced more capitula (54.5% vs. 43.9%), and Portuguese clones more stalks (37.2% vs. 25.6%). The heating values (HHV0) of the stalks were similar, ranging from 17.1 to 18.4 MJ/kg. Lignin was studied by analytical pyrolysis (Py-GC/MS(FID)), separately in depithed stalks (stalksDP) and pith. StalksDP had in average higher relative proportions of lignin derived compounds than pith (23.9% vs. 21.8%) with slightly different lignin monomeric composition: pith samples were richer in syringyl units as compared to stalksDP (64% vs. 53%), with S/G ratios of 2.1 and 1.3, respectively. The H:G:S composition was 7:40:53 in stalksDP and 7:29:64 in pith. The lignin content ranged from 18.8% to 25.5%, enabling a differentiation between clones and provenances. © 2015 Elsevier Ltd. All rights reserved.