Resumo:
This paper presents a study concerning the fatigue behaviour of asphalt mixtures with bitumen modified with high content of crumb rubber used in Portugal. For assessing the fatigue behaviour of this type of mixtures, four asphalt mixtures with high content of crumb rubber were used: two field bituminous mixtures – an open-graded and a gap-graded – both with granite aggregates; and two laboratory manufactured bituminous mixtures – an open-graded mixture with granite aggregates and a gap-graded mixture with crushed gravel aggregates. Since this type of mixtures are mainly applied in wearing courses, the effect of ageing in the fatigue behaviour of one of the studied asphalt rubber mixtures was also assessed through laboratory testing. The paper presents the main results achieved so far concerning the fatigue resistance and it could be concluded that all the materials have exhibited a good behaviour, in agreement with others previous studies. In the case of the aged gap-graded material, it was observed a slight reduction on the fatigue life comparatively to the un-aged one.
Resumo:
Reuse of tire crumb in sport facilities is currently a very cost-effective waste management measure. Considering that incorporation of the waste materials in artificial turf would be facilitated if the rubber materials were already colored green, coatings were specifically developed for this purpose. This paper presents an experimental toxicological and environmental assessment aimed at comparing the obtained emissions to the environment in terms of polycyclic aromatic hydrocarbons (PAHs), heavy metals, and ecotoxicity for coated and noncoated rubber granulates. This study is a comprehensive evaluation of the major potential critical factors related with the release of all of these classes of pollutants because previous studies were not systematically performed. It was concluded that between the two types of coatings tested, one is particularly effective in reducing emissions to the environment, simultaneously meeting the requirements of adherence and color stability.
Resumo:
One Plus Sequential Air Sampler—Partisol was placed in a small village (Foros de Arrão) in central Portugal to collect PM10 (particles with an aerodynamic diameter below 10 μm), during the winter period for 3 months (December 2009–March 2010). Particles masses were gravimetrically determined and the filters were analyzed by instrumental neutron activation analysis to assess their chemical composition. The water-soluble ion compositions of the collected particles were determined by Ion-exchange Chromatography. Principal component analysis was applied to the data set of chemical elements and soluble ions to assess the main sources of the air pollutants. The use of both analytical techniques provided information about elemental solubility, such as for potassium, which was important to differentiate sources.
Resumo:
This paper concerns the study of biocides application in old timber structures of maritime pine (Pinus pinaster Ail.), previously impregnated with other products. A method was developed in laboratory to determine in situ the penetration depth of a product applied superficially. As initial treatment, three traditional products for sawn timber for buildings were used and, for new treatments, two newer, more environmentally benign products were used. Their ability to penetrate the pre-treated surfaces was evaluated after 1, 2 and 3 applications at 24 hours intervals and the results obtained are presented. Finally, the applicability of the developed test to the in-situ evaluation of timber structures is also discussed.
Resumo:
A test chamber was projected and built (according to ISO 16000-9 Standard) to simulate atmospheric conditions experienced by rubber infill (when applied in synthetic turf pitches) and measure accurately the airborne emissions of pollutants such as dusts and volatile organic compounds (VOC), as well as pollutants present in leachates. It should be pointed out that standard ISO 16000-9 is only concerned with the determination of the emission of VOC from building products and furnishing (not specific of synthetic turf materials), whereas other standards are concerned with the emission of leachates only. This procedure is to be considered as a technical option to the lysimeter "global turf system evaluation" when the rubber infill alone is to be evaluated. The advantage of the proposed option considering this "test chamber" is its simplicity and economy. This test chamber is actually installed and being used for tests in LAIST.
Resumo:
The kraft pulps produced from heartwood and sapwood of Eucalyptus globulus at 130 degrees C, 150 degrees C, and 170 degrees C were characterized by wet chemistry (total lignin as sum of Klason and soluble lignin fractions) and pyrolysis (total lignin denoted as py-lignin). The total lignin content obtained with both methods was similar. In the course of delignification, the py-lignin values were higher (by 2 to 5%) compared to Klason values, which is in line with the importance of soluble lignin for total lignin determination. Pyrolysis analysis presents advantages over wet chemical procedures, and it can be applied to wood and pulps to determine lignin contents at different stages of the delignification process. The py-lignin values were used for kinetic modelling of delignification, with very high predictive value and results similar to those of modelling using wet chemical determinations.
Resumo:
Reuse of tire crumb in sport facilities is currently a very cost-effective waste management measure. Considering that incorporation of the waste materials in artificial turf would be facilitated if the rubber materials were already colored green, coatings were specifically developed for this purpose. This paper presents an experimental toxicological and environmental assessment aimed at comparing the obtained emissions to the environment in terms of polycyclic aromatic hydrocarbons (PAHs), heavy metals, and ecotoxicity for coated and noncoated rubber granulates. This study is a comprehensive evaluation of the major potential critical factors related with the release of all of these classes of pollutants because previous studies were not systematically performed. It was concluded that between the two types of coatings tested, one is particularly effective in reducing emissions to the environment, simultaneously meeting the requirements of adherence and color stability.
Resumo:
When timber elements in heritage buildings are moderately degraded by fungi and assuming underlying moisture problems have been solved, two actions can be taken: i) use a biocide to stop fungal activity; ii) consolidate the degraded elements so that the timber keeps on fulfilling its structural and decorative functions. The aim of this work is to investigate the mechanical performance of maritime pine wood degraded by fungi after being treated with a biocide followed by impregnation with a polymer product. Three commercially available products were used: a boron water-based biocide, an acrylic consolidant and an epoxy-based consolidant. Treated and consolidated specimens were subjected to mechanical tests: axial compression test (NP 618), static surface hardness (ISO 3350) and bending test (NP 619). Sets of replicates were subjected to an evaporation ageing test (EN 73) after application of the products and also tested for mechanical behaviour. An increase in mechanical strength was observed for both consolidants with no significant influence from the previous use of biocide product. The specimens subjected to ageing showed a slightly better general mechanical performance.
Resumo:
Eucalyptus globulus sapwood and heartwood showed no differences in lignin content (23.0% vs. 23.7%) and composition: syringyl-lignin (17.9% vs. 18.0%) and guaiacyl-lignin (4.8% vs. 5.2%). Delignification kinetics of S- and G-units in heartwood and sapwood was investigated by Py-GC–MS/FID at 130, 150 and 170 °C and modeled as double first-order reactions. Reactivity differences between S and G-units were small during the main pulping phase and the higher reactivity of S over G units was better expressed in the later pulping stage. The residual lignin composition in pulps was different from wood or from samples in the initial delignification stages, with more G and H-units. S/G ratio ranged from 3 to 4.5 when pulp residual lignin was higher than 10%, decreasing rapidly to less than 1. The S/H was initially around 20 (until 15% residual lignin), decreasing to 4 when residual lignin was about 3%.