The aim of the present work is to provide insight into the mechanism of laccase reactions using syringyl-type mediators. We studied the pH dependence and the kinetics of oxidation of syringyl-type phenolics using the low CotA and the high redox potential TvL laccases. Additionally, the efficiency of these compounds as redox mediators for the oxidation of non-phenolic lignin units was tested at different pH values and increasing mediator/non-phenolic ratios. Finally, the intermediates and products of reactions were identified by LC-MS and H-1 NMR. These approaches allow concluding on the (1) mechanism involved in the oxidation of phenolics by bacterial laccases, (2) importance of the chemical nature and properties of phenolic mediators, (3) apparent independence of the enzyme's properties on the yields of non-phenolics conversion, (4) competitive routes involved in the catalytic cycle of the laccase-mediator system with several new C-O coupling type structures being proposed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Eucalyptus globulus sapwood and heartwood showed no differences in lignin content (23.0% vs. 23.7%) and composition: syringyl-lignin (17.9% vs. 18.0%) and guaiacyl-lignin (4.8% vs. 5.2%). Delignification kinetics of S- and G-units in heartwood and sapwood was investigated by Py-GC–MS/FID at 130, 150 and 170 °C and modeled as double first-order reactions. Reactivity differences between S and G-units were small during the main pulping phase and the higher reactivity of S over G units was better expressed in the later pulping stage. The residual lignin composition in pulps was different from wood or from samples in the initial delignification stages, with more G and H-units. S/G ratio ranged from 3 to 4.5 when pulp residual lignin was higher than 10%, decreasing rapidly to less than 1. The S/H was initially around 20 (until 15% residual lignin), decreasing to 4 when residual lignin was about 3%.