Resumo:
Research on the use of Construction and Demolition Waste (CDW) as recycled aggregate (in particular crushed concrete) for the production of new concrete has by now established the feasibility of this environmentally-friendly use of otherwise harmful waste. However, contrary to conventional concrete (CC), no large applications of concrete made with recycled concrete have been made and there is still a lack of knowledge in some areas of production and performance of recycled aggregate concrete (RAC). One issue concerns curing conditions: these greatly affect the performance of concrete made on site and some potential users of RAC wonder how RAC is affected by far-from-ideal curing conditions. This paper shows the main results of experiments to determine the influence of different curing conditions on the mechanical performance of concrete made with coarse recycled aggregate from crushed concrete. The properties analyzed include compressive strength, splitting tensile strength, modulus of elasticity, and abrasion resistance. The general conclusion in terms of mechanical performance is that RAC is affected by curing conditions roughly in the same way as CC. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
To study luminescence, reflectance, and color stability of dental composites and ceramics. Materials and Methods: IPS e.max, IPS Classic, Gradia, and Sinfony materials were tested, both unpolished (as-cast) and polished specimens. Coffee, tea, red wine, and distilled water (control) were used as staining drinks. Disk-shaped specimens were soaked in the staining drinks for up to 5 days. Color was measured by a colorimeter. Fluorescence was recorded using a spectrofluorometer, in the front-face geometry. Time-resolved fluorescence spectra were recorded using a laser nanosecond spectrofluorometer. Results: The exposure of the examined dental materials to staining drinks caused changes in color of the composites and ceramics, with the polished specimens exhibiting significantly lower color changes as compared to unpolished specimens. Composites exhibited lower color stability as compared to ceramic materials. Water also caused perceptible color changes in most materials. The materials tested demonstrated significantly different initial luminescence intensities. Upon exposure to staining drinks, luminescence became weaker by up to 40%, dependent on the drink and the material. Time-resolved luminescence spectra exhibited some red shift of the emission band at longer times, with the lifetimes in the range of tens of nanoseconds. Conclusions: Unpolished specimens with a more developed surface have lower color stability. Specimens stored in water develop some changes in their visual appearance. The presently proposed methods are effective in evaluating the luminescence of dental materials. Luminescence needs to be tested in addition to color, as the two characteristics are uncorrelated. It is important to further improve the color and luminescence stability of dental materials.