4 resultados para time preparation
em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo (BDPI/USP)
Resumo:
Statement of the problem: The performance of self-etch systems on enamel is controversial and seems to be dependent on the application technique and the enamel preparation. Purpose of the Study: To examine the effects of conditioning time and enamel surface preparation on bond strength and etching pattern of adhesive systems to enamel. Materials and Methods: Ninety-six teeth were divided into 16 conditions (N = 6) in function of enamel preparation and conditioning time for bond strength test. The adhesive systems OptiBond FL (Kerr, Orange, CA, USA), OptiBond SOLO Plus (Kerr), Clearfil SE Bond (Kuraray, Osaka, Japan), and Adper Prompt L-Pop (3M ESPE, St. Paul, MN, USA) were applied on unground or ground enamel following the manufacturers` directions or doubling the conditioning time. Cylinders of Filtek Flow (0.5-mm height) were applied to each bonded enamel surface using a Tygon tube (0.7 mm in diameter; Saint-Gobain Corp., Aurora, OH, USA). After storage (24 h/37 degrees C), the specimens were subjected to shear force (0.5 mm/min). The data were treated by a three-way analysis of variance and Tukey`s test (alpha = 0.05). The failure modes of the debonded interfaces and the etching pattern of adhesives were observed using scanning electron microscopy. Results: Only the main factor ""adhesive"" was statistically significant (p < 0.001). The lowest bond strength value was observed for OptiBond FL. The most defined etching pattern was observed for 35% phosphoric acid and for Adper Prompt L-Pop. Mixed failures were observed for all adhesives, but OptiBond FL showed cohesive failures in resin predominantly. Conclusions: The increase in the conditioning time as well as the enamel pretreatment did not provide an increase in the resin-enamel bond strength values for the studied adhesives. CLINICAL SIGNIFICANCE The surface enamel preparation and the conditioning time do not affect the performance of self-etch systems to enamel. (J Esthet Restor Dent 20:322-336, 2008)
Resumo:
For the first time, crystals of suitable size for X-ray diffractometry structure determination (Dian important anti-HI V drug were prepared under solvothermal conditions. In this study, the crystal structure of didanosine (2`,3`-dideoxyinosine, ddI) in the form of a hydrate was determined using single-crystal X-ray diffractometry. Powder X-ray diffraction analysis revealed that the solid-state phase of the drug incorporated into pharmaceutical solid dosage forms is isostructural to the solvothermally prepared ddI material, even though they do not exhibit an identical chemical composition due to different water fractions occupying hydrophobic channels formed within the crystal lattice. Two ddI conformers are present in the structure, in agreement with a previous structure elucidation attempt. Concerning the keto enol equilibrium of ddI, our crystal data and vibrational characterizations by Fourier transform infrared (FTIR) and FT-Raman spectroscopy techniques were conclusive to state that both conformers exist in the keto form, contrary to solid-state NMR spectroscopic assignments that suggested ddI molecules occur as enol tautomers. In addition, characterizations by thermal (differential scanning calorimetry) and spectroscopic techniques allowed us to understand the structural similarities and the differences related to the hydration pattern of the nonstoichiometric hydrates.
Resumo:
A magnetically recoverable Pt(0) catalyst was prepared by in situ H(2) reduction of Pt(2+) species bound to an amino modified silica-coated magnetic nanoparticles. Compared to ordinary silica (maximum uptake Pt 0.03 wt%), the amino-functionalized silica surfaces were loaded with 1.95 wt% of metal. The supported Pt(0) nanoparticles exhibit high catalytic activity in the hydrogenation of alkenes and ketones under solventless mild reaction conditions. Partially hydrogenated products could also be isolated. The magnetic property of the catalyst grants a fast and efficient product isolation compared to traditional methods used in heterogeneous systems that generally make use of time- and solvent-consuming procedures. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Composite electrodes were prepared using graphite powder and silicone rubber in different compositions. The use of such hydrophopic materials interned to diminish the swallowing observed in other cases when the electrodes are used in aqueous solutions for a long time. The composite was characterized for the response reproducibility, ohmic resistance, thermal behavior and active area. The voltammetric response in relation to analytes with known voltammetric behavior was also evaluated, always in comparison with the glassy carbon. The 70% (graphite, w/w) composite electrode was used in the quantitative determination of hydroquinone (HQ) in a DPV procedure in which a detection limit of 5.1 x 10(-8) mol L-1 was observed. HQ was determined in a photographic developer sample with errors lower then 1% in relation to the label value. (c) 2007 Elsevier B.V. All rights reserved.