Resumo:
The goal of this study is to evaluate the influence of the urea and glycine fuels on the synthesis of Mn-Zn ferrite by combustion reaction The morphology and magnetic properties of the resulting powders were investigated. The powders were characterized by X-ray diffraction (XRD), nitrogen adsorption (BET), scanning and transmission electron microscopy (SEM and TEM), and magnetic measurement of M x H curves. The X-lay diffraction patterns indicated that the samples containing urea resulted in the formation of crystalline powders and the presence of hematite as a secondary phase The samples containing glycine presented only the formation of crystalline and monophases (Mn,Zn)Fe(2)O(4). The average crystallite size was 18 and 35 nm and saturation magnetization was 3.6 and 75 emu/g, respectively, for the samples containing urea and glycine. The samples synthesized with glycine fuel showed better magnetic properties for application as soft magnetic devices. (C) 2009 Elsevier B.V All rights reserved
Resumo:
The (16)O+(27)Al elastic and inelastic angular distributions have been measured in a broad angular range (13 degrees < theta(lab) < 52 degrees) at about 100 MeV incident energy. The use of the MAGNEX large acceptance magnetic spectrometer and of the ray-reconstruction analysis technique has been crucial in order to provide, in the same experiment, high-resolution energy spectra and cross-section measurements distributed over more than seven orders of magnitude down to hundreds of nb/sr. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
The magnetic linear dichroism (MLD) at band-edge photon energies in the Voigt geometry was calculated for EuTe. At the spin-flop transition, MLD shows a step-like increase. Above the spin-flop transition MLD slowly decreases and becomes zero when the averaged electronic charge becomes symmetric relative to the axis of light propagation. Further increase of the magnetic field causes ferromagnetic alignment of the spins along the magnetic field direction, and MLD is recovered but with an opposite sign, and reaches maximum absolute values. These results are explained by the rearrangement of the Eu(2+) spin distribution in the crystal lattice as a function of magnetic field, due to the Zeeman interaction, demonstrating that MLD can be a sensitive probe of the spin order in EuTe, and provides information that is not accessible from other magneto-optical techniques, such as magnetic circular dichroism measurement studies.