6 resultados para Processus de substitution
em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo (BDPI/USP)
Resumo:
In this work we report results on the influence of heavy rare earth ions substitution on microstructure and magnetism of nanocrystalline magnetite. A series of Fe(2.85)RE(0.15)O(4) (RE = Gd, Dy, Ho, Tm and Yb) samples have been prepared by high energy ball milling. Structure/microstructure investigations of two selected samples Fe(2.85)Gd(0.15)O(4) and Fe(2.85)Tm(0.15)O(4), represent an extension of the previously published results on Fe(3)O(4)/gamma-Fe(2)O(3), Fe(2.85)Y(0.15)O(4) and Fe(2.55)In(0.45)O(4) [Z. Cvejic, S. Rakic, A. Kremenovic, B. Antic, C. Jovalekic. Ph. Colomban, Sol. State Sciences 8 (2006) 908], while magnetic characterization has been done for all the samples. Crystallite/particle size and strain determined by X-ray diffractometry and Transmission electron microscopy (TEM) confirmed the nanostructured nature of the mechanosynthesized materials. X-ray powder diffraction was used to analyze anisotropic line broadening effects through the Rietveld method. The size anisotropy was found to be small while strain anisotropy was large, indicating nonuniform distribution of deffects in the presence of Gd and Tm in the crystal structure. Superparamagnetic(SPM) behavior at room temperature was observed for all samples studied. The Y-substituted Fe(3)O(4) had the largest He and the lowest M(S). We discuss the changes in magnetic properties in relation to their magnetic anisotropy and microstructure. High field irreversibility (H>20kOe) in ZFC/FC magnetization versus temperature indicates the existence of high magnetocrystalline and/or strain induced anisotropy. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
The reaction of cis-[RuCl(2)(P-P)(N-N)] type complexes (P-P = 1,4-bis(diphenylphosphino)butane or (1,1`-diphenylphosphino)ferrocene; N-N = 2,2`-bipyridine or 1,10-phenantroline) with monodentate ligands (L), such as 4-methylpyridine, 4-phenylpyridine and benzonitrile forms [RuCl(L)(P-P)(N-N)](+) species Upon characterization of the isolated compounds by elemental analysis, (31)P{(1)H} NMR and X-ray crystallography it was found out that the type of the L ligand determines its position in relation to the phosphorus atom. While pyridine derivatives like 4-methylpyridine and 4-phenylpyridine coordinate trans to the phosphorus atom, the benzonitrile ligand (bzCN), a good pi acceptor, coordinates trans to the nitrogen atom. A (31)P{(1)H} NMR experiment following the reaction of the precursor cis-[RuCl(2)(dppb)(phen)] with the benzonitrile ligand shows that the final position of the entering ligand in the complex is better defined as a consequence of the competitive effect between the phosphorus atom and the cyano-group from the benzonitrile moiety and not by the trans effect. In this case, the benzonitrile group is stabilized trans to one of the nitrogen atoms of the N-N ligand. A differential pulse voltammetry experiment confirms this statement. In both experiments the [RuCl(bzCN)(dppb)(phen)]PF(6) species with the bzCN ligand positioned trans to a phosphorus atom of the dppb ligand was detected as an intermediate complex. (c) 2009 Elsevier Ltd. All rights reserved.
Resumo:
Two techniques, namely UV-vis- and FTIR spectroscopy, have been employed in order to calculate the degree of substitution (DS) of cellulose carboxylic esters, including acetates, CAs, butyrates, CBs, and hexanoates, CHs. Regarding UV-vis spectroscopy, we have employed a novel approach, based on measuring the dependence of lambda(max) of the intra-molecular charge-transfer bands of polarity probes adsorbed on DS of the ester films (solvatochromism). Additionally, we have revisited the use of FTIR for DS determination. Several methods have been used in order to plot Beer`s law graph, namely: Absorption of KBr pellets, pre-coated with CA: reflectance (DRIFTS) of CAs-KBr solid-solid mixtures with, or without the use of 1.4-dicyanobenzene as an internal reference; reflectance of KBr powder pre-coated with CA. The methods indicated are simple, fast, and accurate, requiring much less ester than the titration method. The probe method is independent of the experimental variables examined. (c) 2010 Published by Elsevier Ltd.
Resumo:
Although cellulose acetates, CAs, are extensively employed there is scant information about the systematic dependence of their properties on their degree of substitution, DS; this is the subject of the present work. Nine CAs samples, DS from 0.83 to 3.0 were synthesized; their films were prepared. The following solvatochromic probes have been employed in order to determine the empirical polarity, E (T)(33); ""acidity, alpha""; ""basicity, beta"", and ""dipolarity/polarizability, pi*"" of the casted films: 2,6-dichloro-4-(2,4,6-triphenyl-pyridinium-1-yl) phenolate, WB; 4-nitroaniline; 4-nitroanisole; 4-nitro-N,N-dimethylaniline; 2,6-diphenyl-4-(2,4,6-triphenyl-pyridinium-1-yl)phenolate, RB. Additionally, two systems, ethanol plus ethyl acetate (EtOH-EtAc), and cellulose plus cellulose triacetate, CTA, were employed as models for CAs of different DS. Regarding the model systems, the following was observed: (i) For EtOH-EtAc, the dependence of all solvatochromic parameters on the ""equivalent-DS"" of the binary mixture was non-linear because of preferential solvation; (ii) The dependence of E (T)(33) on equivalent DS of the cellulose-CTA films is linear, but the slope is smaller than that of the corresponding plot for CAs. This is attributed to the more efficient hydrogen bonding in the model system, a conclusion corroborated by IR measurements. The dependence of solvatochromic parameters of CAs on their DS is described by the simple equations; a consequence of the substitution of the OH by the ester group. The thermal properties of bulk CAs samples were investigated by DSC and TGA; their dependence on DS is described by simple equations. The relevance of these data to the processing and applications of CAs is briefly discussed.
Resumo:
The second-order rate constants of thiolysis by n-heptanethiol on 4-nitro-N-n-butyl-1,8-naphthalimide (4NBN) are strongly affected by the water-methanol binary mixture composition reaching its maximum at around 50% mole fraction. In parallel solvent effects on 4NBN absorption molar extinction coefficient also shows a maximum at this composition region. From the spectroscopic study of reactant and product and the known H-bond capacity of the mixture a rationalization that involves specific solvent H-donor interaction with the nitro group is proposed to explain the kinetic data. Present findings also show a convenient methodology to obtain strongly fluorescent imides, valuable for peptide and analogs labeling as well as for thio-naphthalimide derivatives preparations. Copyright (C) 2008 John Wiley & Sons, Ltd.