13 resultados para Magnetic exchange
em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo (BDPI/USP)
Resumo:
Measurements of X-ray diffraction, electrical resistivity, and magnetization are reported across the Jahn-Teller phase transition in LaMnO(3). Using a thermodynamic equation, we obtained the pressure derivative of the critical temperature (T(JT)), dT(JT)/dP = -28.3 K GPa(-1). This approach also reveals that 5.7(3)J(mol K)(-1) comes from the volume change and 0.8(2)J(mol K)(-1) from the magnetic exchange interaction change across the phase transition. Around T(JT), a robust increase in the electrical conductivity takes place and the electronic entropy change, which is assumed to be negligible for the majority of electronic systems, was found to be 1.8(3)J(mol K)(-1).
Resumo:
The distributions of coercivities and magnetic interactions in a set of polycrystalline Ni(0.8)Fe(0.2)/FeMn bilayers have been determined using the first-order reversal curve (FORC) formalism. The thickness of the permalloy (Py) film was fixed at 10 nm (nominal), while that of the FeMn film varied within the range 0-20 nm. The FORC diagrams of each bilayer displayed two clearly distinguishable regions. The main region was generated by Py particles whose coercivities were enhanced in comparison with those in which the FeMn film was absent (sample O). The minor region was produced by Py particles with coercivities similar to or slightly higher than those of particles in the Py film of sample O. Each sample presented two distributions of interaction fields, one for each region, and both were centred slightly below the exchange-bias field, thus indicating a prevalence of magnetizing interactions. These results are consistent with a grain size distribution in the Py layer and the presence of uncompensated antiferromagnetic moments.
Resumo:
The exchange energy of an arbitrary collinear-spin many-body system in an external magnetic field is a functional of the spin-resolved charge and current densities, E(x)[n(up arrow), n(down arrow), j(up arrow), j(down arrow)]. Within the framework of density-functional theory (DFT), we show that the dependence of this functional on the four densities can be fully reconstructed from either of two extreme limits: a fully polarized system or a completely unpolarized system. Reconstruction from the limit of an unpolarized system yields a generalization of the Oliver-Perdew spin scaling relations from spin-DFT to current-DFT. Reconstruction from the limit of a fully polarized system is used to derive the high-field form of the local-spin-density approximation to current-DFT and to magnetic-field DFT.
Resumo:
The magnetic behavior of polycrystalline yttrium orthoferrite was studied from the experimental and theoretical points of view. Magnetization measurements up to 170 kOe were carried out on a single-phase YFeO3 sample synthesized from heterobimetallic alkoxides. The complex interplay between weak-ferromagnetic and antiferromagnetic interactions, observed in the experimental M(H) curves, was successfully simulated by locally minimizing the magnetic energy of two interacting Fe sublattices. The resulting values of exchange field (H-E = 5590 kOe), anisotropy field (H-A = 0.5 kOe) and Dzyaloshinsky-Moriya antisymmetric field (H-D = 149 kOe) are in good agreement with previous reports on this system. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Measurements of the magnetic susceptibility of the frustrated pyrochlore magnet Gd(2)Sn(2)O(7) have been performed at temperatures below T = 5 K and in magnetic fields up to H = 12 T. The phase boundaries determined from these measurements are mapped out in an H-T phase diagram. In this gadolinium compound, where the crystal-field splitting is small and the exchange and dipolar energy are comparable, the Zeeman energy overcomes these competing energies, resulting in at least four magnetic phase transitions below 1 K. These data are compared against those for Gd(2)Ti(2)O(7) and will, we hope, stimulate further studies.
Resumo:
The perpendicular exchange bias and magnetic anisotropy were investigated in IrMn/Pt/[Co/Pt](3) multilayers through the analysis of in-plane and out-of-plane magnetization hysteresis loops. A phenomenological model was used to simulate the in-plane curves and the effective perpendicular anisotropies were obtained employing the area method. The canted state anisotropy was introduced by taking into account the first and second uniaxial anisotropy terms of the ferromagnet with the corresponding uniaxial anisotropy direction allowed to make a nonzero angle with the film`s normal. This angle, obtained from the fittings, was of approximately 15 degrees for IrMn/[Co/Pt](3) film and decreases with the introduction of Pt in the IrMn/Pt/[Co/Pt](3) system, indicating that the Pt interlayer leads to a predominant perpendicular anisotropy. A maximum of the out-of-plane anisotropy was found between 0.5 and 0.6 nm of Pt, whereas a maximum of the perpendicular exchange bias was found at 0.3 nm. These results are very similar to those obtained for IrMn/Cu/[Co/Pt](3) system; however, the decrease of the exchange bias with the spacer thickness is more abrupt and the enhacement of the perpendicular anisotropy is higher for the case of Cu spacer as compared with that of Pt spacer. The existence of a maximum in the perpendicular exchange bias as a function of the Pt layer thickness was attributed to the predominance of the enhancement of exchange bias due to more perpendicular Co moment orientation over the exponential decrease of the ferromagnetic/antiferromagnetic exchange coupling and, consequently, of the exchange-bias field. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Magnetic properties of nanocrystalline NiFe(2)O(4) spinel mechanically processed for 350 h have been studied using temperature dependent from both zero-field and in-field (57)Fe Mossbauer spectrometry and magnetization measurements. The hyperfine structure allows us to distinguish two main magnetic contributions: one attributed to the crystalline grain core, which has magnetic properties similar to the NiFe(2)O(4) spinel-like structure (n-NiFe(2)O(4)) and the other one due to the disordered grain boundary region, which presents topological and chemical disorder features(d-NiFe(2)O(4)). Mossbauer spectrometry determines a large fraction for the d-NiFe(2)O(4) region(62% of total area) and also suggests a speromagnet-like structure for it. Under applied magnetic field, the n-NiFe(2)O(4) spins are canted with angle dependent on the applied field magnitude. Mossbauer data also show that even under 120 kOe no magnetic saturation is observed for the two magnetic phases. In addition, the hysteresis loops, recorded for scan field of 50 kOe, are shifted in both field and magnetization axes, for temperatures below about 50 K. The hysteresis loop shifts may be due to two main contributions: the exchange bias field at the d-NiFe(2)O(4)/n-NiFe(2)O(4) interfaces and the minor loop effect caused by a high magnetic anisotropy of the d-NiFe(2)O(4) phase. It has also been shown that the spin configuration of the spin-glass like phase is modified by the consecutive field cycles, consequently the n-NiFe(2)O(4)/d-NiFe(2)O(4) magnetic interaction is also affected in this process. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
The growth and magnetic properties of Tin Selenide (SnSe) doped with Eu(2+) Sn(1-x)Eu(x)Se (x=2.5%) were investigated. Q-band (34 GHz) electron paramagnetic resonance measurements show that the site symmetry of Eu(2+) at 4.2 K is orthorhombic and the Lande factor was determined to be g=1.99 +/- 0.01. The exchange coupling between nearest-neighbor (NN) Eu(2+) ions was estimated from magnetization and magnetic-susceptibility measurements using a model that takes into account the magnetic contributions of single ions, pairs and triplets. The exchange interaction between Eu(2+) nearest neighbors was found to be antiferromagnetic with an estimated average value of J(p)/k(B) =-0.18 +/- 0.03 K. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
The magnetic response of the near-band-edge optical properties is studied in EuTe layers. In several magneto-optical experiments, the absorption and emission are described as well as the related Stokes shift. Specifically, we present the first experimental report of the photoluminescence excitation (PLE) spectrum in Faraday configuration. The PLE spectra shows to be related with the absorption spectra through the observation of resonance between the excitation light and the zero-field band-gap. A new emission line appears at 1.6 eV at a moderate magnetic field in the photoluminescence (PL) spectra. Furthermore, we examine the absorption and PL red-shift induced by the magnetic field in the light of the d-f exchange interaction energy involved in these processes. Whereas the absorption red-shift shows a quadratic dependence on the field, the PL red-shift shows a linear dependence which is explained by spin relaxation of the excited state.
Resumo:
Magnetic M( T, H, P) and electrical transport.( T, H, P) measurements in a strong spin-lattice-charge coupled La(0.7)Ca(0.3)MnO(3) system have been conducted. The application of H and P leads to the formation of different magnetic domain structures in the vicinity and below the polaronic-to-ferromagnetic transition temperature. The charge mobility is more sensitive to the variation of the spatial wave function overlap between Mn(3+) eg and O(2-) 2p orbitals due to the applied compacting pressure rather than the relative spin orientation between neighbouring Mn ions when the magnetic field is applied. In spite of the presence of different magnetic domain structures due to the sample history, the effect of magnetic field and pressure is less pronounced at lower temperatures on electrical transport properties.
Resumo:
Polycrystalline La(0.86)Sr(0.14)Mn(1-x)Cu(x)O(3+delta) (x = 0, 0.05, 0.10, 0.15, 0.20) manganites were investigated by means of magnetic measurements and zero-field (139)La and (55)Mn nuclear magnetic resonance (NMR) spectroscopy. Magnetization versus temperature measurements revealed a paramagnetic to ferromagnetic transition in most samples, with lower Curie temperatures and broader transitions for samples with higher Cu contents. The details of the magnetization measurements suggested a phase-separated scenario, with ferromagnetic clusters embedded in an antiferromagnetic matrix, especially for the samples with large Cu contents (x = 0.15 and 0.20). Zero-field (139)La NMR measurements confirmed this finding, since the spectral features remained almost unchanged for all Cu-doped samples, whereas the bulk magnetization was drastically reduced with increasing Cu content. (55)Mn NMR spectra were again typical of ferromagnetic regions, with a broadening of the resonance line caused by the disorder introduced by the Cu doping. The results indicate a coexistence of different magnetic phases in the manganites studied, with the addition of Cu contributing to the weakening of the double-exchange interaction in most parts of the material.
Resumo:
We have employed UV-vis spectroscopy in order to investigate details of the solvation of six solvatochromic indicators, hereafter designated as ""probes"", namely, 2,6-diphenyl-4-(2,4,6-triphenylpyridinium-1-yl) phenolate (RB); 4-[(E)-2-(1-methylpyridinium-4-yl)ethenyl] phenolate, MePM; 1-methylquinolinium-8-olate, QB; 2-bromo-4-[(E)-2-(1-methylpyridinium-4-yl)ethenyl] phenolate, MePMBr, 2,6-dichloro-4-(2,4,6-triphenylpyridinium-1-yl) phenolate (WB); and 2,6-dibromo-4-[(E)-2-(1-methylpyridinium-4-yl)ethenyl] phenolate, MePMBr,, respectively. These can be divided into three pairs, each includes two probes of similar pK(a) in water and different lipophilicity. Solvation has been studied in binary mixtures, BMs, of water, W, with 12 protic organic solvents, S, including mono- and bifunctional alcohols (2-alkoxyethanoles, unsaturated and chlorinated alcohols). Each medium was treated as a mixture of S, W, and a complex solvent, S-W, formed by hydrogen bonding. Values of lambda(max) (of the probe intramolecular charge transfer) were converted into empirical polarity scales, E(T)(probe) in kcal/mol, whose values were correlated with the effective mole fraction of water in the medium, chi w(effective). This correlation furnished three equilibrium constants for the exchange of solvents in the probe solvation shell; phi(W/S) (W substitutes S): phi(S-W/W) (S-W substitutes W), and phi(S-W/S) (S-W substitutes S), respectively. The values of these constants depend on the physicochemical properties of the probe and the medium. We tested, for the first time, the applicability of a new solvation free energy relationship: phi = constant + a alpha(BM) + b beta(BM) + s(pi*(BM) + d delta) + p log P(BM), where a, b, s, and p are regression coefficients alpha(BM), beta(BM), and pi*(BM) are solvatochromic parameters of the BM, delta is a correction term for pi*, and log P is an empirical scale of lipophilicity. Correlations were carried out with two-, three-, and four-medium descriptors. In all cases, three descriptors gave satisfactory correlations; use of four parameters gave only a marginal increase of the goodness of fit. For phi(W/S), the most important descriptor was found to be the lipophilicity of the medium; for phi(S-W/W) and phi(S-W/S), solvent basicity is either statistically relevant or is the most important descriptor. These responses are different from those of E(T)(probe) of many solvatochromic indicators in pure solvents, where the importance of solvent basicity is usually marginal, and can be neglected.
Nuclear magnetic resonance water relaxation time changes in bananas during ripening: a new mechanism
Resumo:
BACKGROUND: Nuclear magnetic resonance studies of banana fragments during ripening show an increase on the water transverse relaxation time (T(2)) and a decrease in water self-diffusion coefficient (D). As T(2) and D are normally directly correlated, we studied these two properties in intact bananas during ripening, in an attempt to rule out the effect of injury on the apparent discrepancies in the behavior of T(2) and D. RESULTS: The results show that injury in bananas causes a decrease in T(2) of the water in vacuoles (T(2vac)). They also show that T(2vac) increased and D decreased during ripening, ruling out the injury effect. To explain the apparent discrepancies, we propose a new hypothesis for the increase in T(2) values, based on the reduction of Fe(3+) ions to Fe(2+) by galacturonic acid, produced by the hydrolysis of pectin and a decrease in internal oxygen concentration during ripening. CONCLUSION: As injury alters T(2) values it is necessary to use intact bananas to study relaxation times during ripening. The novel interpretation for the increase in T(2vac) based on reduction of Fe(+3) and O(2) concentration is an alternative mechanism to that based on the hydrolysis of starch in amyloplasts. (C) 2010 Society of Chemical Industry