The cleaning procedure consists of two-step-flashing: (i) cycles of low power flashes T similar to 1200 K) at an oxygen partial pressure of P(o2) = 6 x 10(-8) mbar, to remove the carbon from the surface, and (ii) a single high power flash (T similar to 2200 K), to remove the oxide layer. The removal of carbon from the surface through the chemical reaction with oxygen during low power flash cycles is monitored by thermal desorption spectroscopy. The exposure to O(2) leads to the oxidation of the W surface. Using a high power flash, the volatile W-oxides and the atomic oxygen are desorbed, leaving a clean crystal surface at the end of procedure. The method may also be used for cleaning other refractory metals like Mo, Re and It. (C) 2009 Elsevier B.V. All rights reserved.