Resumo:
Two series of lanthanide oxides with different morphologies were synthesized through calcinations of two types of citrate polymeric precursors. These oxides were characterized by XRD patterns, SEM electronic microscopy, and N(2) adsorption isotherms. SEM microscopy analysis showed that the calcination of crystalline fibrous precursors [Ln(2)(LH)(3)center dot 2H(2)O] (L = citrate) originated fibrous shaped particles. On the other hand, the calcination of irregular shaped particles of precursors [LnL center dot xH(2)O] originated irregular shaped particles of oxide, pointing out a morphological template effect of precursors on the formation of the respective oxides.
Resumo:
Stability and interface properties of cellulose acetate propionate (CAP) and cellulose acetate butyrate (CAB) films adsorbed from acetone or ethyl acetate onto Si wafers have been investigated by means of contact angle measurements and atomic force microscopy (AFM). Surface energy (gamma(total)(S)) values determined for CAP adsorbed from acetone are larger than those from ethyl acetate. In the case of CAB films adsorbed from ethyl acetate and acetone were similar. Dewetting was observed by AFM only for CAP films prepared from ethyl acetate. Positive values of effective Hamaker constant (A(eff)) were found only for CAP prepared from ethyl acetate, corroborating with dewetting phenomena observed by AFM. Oil the contrary, negative values of A(eff) were determined for CAP and CAB prepared from acetone and for CAB prepared from ethyl acetate, Corroborating with experimental observations. Sum frequency generation (SFG) vibrational spectra indicated that CAP and CAB films prepared from ethyl acetate present more alkyl groups oriented perpendicularly to the polymer-air interface than those films prepared from acetone. Such preferential orientation corroborates with macroscopic contact angle measurements. Moreover, SFG spectra showed that acetone hinds strongly to Si wafers, creating a new surface for CAP and CAB films. (C) 2008 Elsevier Inc. All rights reserved.
Resumo:
Evidence of the sorption of the whitening agent sodium 4,4`-distyrylbiphenyl sulfonate in the presence of the anionic surfactant sodium dodecylsulfate or the cationic surfactant dodecyl trimethyl ammonium chloride on regenerated cellulose fibers is given by several microscopy techniques. Scanning electron microscopy provided images of the cylindrical fibers with dimensions of 3.5 cm (length) and 13.3 mu m (thickness), with empty cores of 1 mu m diameter and a smooth surface. Atomic force microscopy showed a fiber surface with disoriented nanometric domains using both tapping-mode height and phase image modes. Atomic force microscopy also showed that the whitening agent and surfactant molecules were sorbed onto the fiber surface, in agreement with the adsolubilization sorption model. Transmission electron microscopy showed fibers with nanometric parallel cylinders, surrounded by holes where the fluorescent whitening molecules accumulated. On the basis of these techniques, we conclude that the sorption process occurs preferentially on the fiber surface in contact with the water solution, and under saturated conditions, the whitening agent penetrates into the pores and are simultaneously sorbed on the pore walls bulk, forming molecular aggregates. (C) 2010 Wiley Periodicals, Inc. J Appl Polym Sci 2321-2327, 2010
Resumo:
The need for biodegradable polymers for packaging has fostered the development of novel, biodegradable polymeric materials from natural sources, as an alternative to reduce amount of waste and environmental impacts. The present investigation involves the synthesis of chitosan nanoparticles-carboxymethylcellulose films, in view of their increasing areas of application in packaging industry. The entire process consists of 2-steps including chitosan nanoparticles preparation and their incorporation in carboxymethylcellulose films. Uniform and stable particles were obtained with 3 different chitosan concentrations. The morphology of chitosan nanoparticles was tested by transmission electron microscopy, revealing the nanoparticles size in the range of 80 to 110 nm. The developed film chitosan nanoparticles-carboxymethylcellulose films were characterized by Fourier transform infrared spectroscopy (FT-IR), thermogravimetric analysis, solubility tests, and mechanical analysis. Improvement of thermal and mechanical properties were observed in films containing nanoparticles, with the best results occurring upon addition of nanoparticles with 110 nm size in carboxymethylcellulose films. Practical Application Carboxymethylcellulose films containing chitosan nanoparticles synthesized and characterized in this article could be a potential material for food and beverage packaging applications products due to the increase mechanical properties and high stability. The potential application of the nanocomposites prepared would be in packaging industry to extend the shelf life of products.
Resumo:
A very unusual triple structural transition pattern below room temperature was observed for the antifilarial drug diethylcarbamazine citrate. Besides the first thermal, crystallographic, and vibrational investigations of this first-line drug used in clinical treatment for lymphatic filariasis, a noteworthy behavior with three structural transformations as a function of temperature was demonstrated by differential scanning calorimetry, Raman spectroscopy, and single-crystal X-ray diffractometry. Our X-ray data on single crystals allow for a complete featuring and understanding of all transitions, since the four structures associated with the three solid-solid phase transformations were accurately determined. Two of three structural transitions show an order-disorder mechanism and temperature hysteresis with exothermic peaks at 224 K (T(1)`) and 213 K (T(2)`) upon cooling and endothermic ones at 248 K (T(1)) and 226 K (T(2)) upon heating. The other transition occurs at 108 K (T(3)) and it is temperature-rate sensitive. Molecular displacements onto the (010) plane and conformational changes of the diethylcarbamazine backbone as a consequence of the C-H center dot center dot center dot N hydrogen bonding formation/cleavage between drug molecules explain the mechanism of the transitions at T(1)`/T(2). However, such changes are observed only on alternate columns of the drug intercalated by citrate chains, which leads to a doubling of the lattice period along the a axis of the 235 K structure with respect to the 150 and 293 K structures. At T(2)`/T(1), these structural alterations occur in all columns of the drug. At T(3), there is a rotation on the axis of the N-C bond between the carbamoyl moiety and an ethyl group of one crystallographically independent diethylcarbamazine molecule besides molecular shifts and other conformational alterations. The impact of this study is based on the fascinating finding in which the versatile capability of structural adaptation dependent on the thermal history was observed for a relatively simple organic salt, diethylcarbamazine citrate.
Resumo:
MgAl(2)O(4):Eu, Dy nanoparticles were prepared by citrate sol-gel method and thermally treated at 600, 700, 800 and 900 degrees C. The trivalent europium ion is partially reduced to the divalent state at 700 and 800 degrees C. Infrared spectra of the phosphors showed bands around 700 and 520 cm(-1) corresponding to the AlO(6) groups. X-ray diffraction patterns present sharp reflections of samples heated from 700 to 900 degrees C indicating the MgAl(2)O(4) spinel phase. Grain size in the range 20-30 nm were observed by measurement of transmission electron microscopy (TEM). The emission spectra of the phosphors show a broadened band at 480 nm assigned to the 4f(G)5d -> 4f(7) ((8)S(7/2)) transition of Eu(2+) ion overlapped to the (4)F(9/2) -> (6)H(15/2) transition of the Dy(3+) ion. Besides, the (4)F(9/2) -> (6)H(13/2) transition (579 nm) of Dy(3+) ion is overlapped with the (5)D(0) -> (7)F(0) (578 nm) and (5)D(0) -> (7)F(1) (595 nm) transitions from the Eu(3+) ion. Excitation spectra of the sample heated at 900 degrees C monitoring the excitation at 615 nm of (5)D(0) -> (7)F(2) transition of Eu(3+) ion exhibit a broad band assigned to the O -> Eu(3+) ligand-to-metal charge-transfer states (LMCT) around 280 nm. The samples present green persistent luminescence after exposure to UV radiation. The chromaticity coordinates were obtained from the luminescence emission spectrum. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Spin-coated films of cellulose acetate (CA), cellulose acetate propionate (CAP), cellulose acetate butyrate (CAB) and carboxymethylcellulose acetate butyrate (CMCAB) have been characterized by ellipsometry, atomic force microscopy (AFM) and contact angle measurements. The films were spin-coated onto silicon wafers, a polar surface. Mean thickness values were determined by means of ellipsometry and AFM as a function of polymer concentration in solutions prepared either in acetone or in ethyl acetate (EA), both are good solvents for the cellulose esters. The results were discussed in the light of solvent evaporation rate and interaction energy between substrate and solvent. The effects of annealing and type of cellulose ester on film thickness, film morphology, surface roughness and surface wettability were also investigated.
Resumo:
Asystematic study on the surface-enhanced Raman scattering (SERS) for 3,6-bi-2-pyridyl-1,2,4,5-tetrazine (bptz) adsorbed onto citrate-modified gold nanoparticles (cit-AuNps) was carried out based on electronic and vibrational spectroscopy and density functional methods. The citrate/bptz exchange was carefully controlled by the stepwise addition of bptz to the cit-AuNps, inducing flocculation and leading to the rise of a characteristic plasmon coupling band in the visible region. Such stepwise procedure led to a uniform decrease of the citrate SERS signals and to the rise of characteristic peaks of bptz, consistent with surface binding via the N heterocyclic atoms. In contrast, single addition of a large amount of bptz promoted complete aggregation of the nanoparticles, leading to a strong enhancement of the SERS signals. In this case, from the distinct Raman profiles involved, the formation of a new SERS environment became apparent, conjugating the influence of the local hot spots and charge-transfer (CT) effects. The most strongly enhanced vibrations belong to a(1) and b(2) representations, and were interpreted in terms of the electromagnetic and the CT mechanisms: the latter involving significant contribution of vibronic coupling in the system. Copyright (C) 2010 John Wiley & Sons, Ltd.
Resumo:
Microwave (MW)-assisted cellulose dissolution in ionic liquids (ILs) has routinely led either to incomplete biopolymer solubilization, or its degradation. We show that these problems can be avoided by use of low-energy MW heating, coupled with efficient stirring. Dissolution of microcrystalline cellulose in the IL 1-allyl-3-methylimidazolium chloride has been achieved without changing its degree of polymerization; regenerated cellulose showed pronounced changes in its index of crystallinity, surface area, and morphology. MW-assisted functionalization of MCC by ethanoic, propanoic, butanoic, pentanoic, and hexanoic anhydrides has been studied. Compared with conventional heating, MW irradiation has resulted in considerable decrease in dissolution and reaction times. The value of the degree of substitution (DS) was found to be DS(ethanoate) > DS(propanoate) > DS(butanoate). The values of DS(pentanoate) and DS(hexanoate) were found to be slightly higher than DS(ethanoate). This surprising dependence on the chain length of the acylating agent has been reported before, but not rationalized. On the basis of the rate constants and activation parameters of the hydrolysis of ethanoic, butanoic, and hexanoic anhydrides in aqueous acetonitrile (a model acyl transfer reaction), we suggest that this result may be attributed to the balance between two opposing effects, namely, steric crowding and (cooperative) hydrophobic interactions between the anhydride and the cellulosic surface, whose lipophilicity has increased, due to its partial acylation. Four ethanoate-based mixed esters were synthesized by the reaction with a mixture of the two anhydrides; the ethanoate moiety predominated in all products. The DS is reproducible and the IL is easily recycled. (C) 2009 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem 48: 134-143, 2010
Resumo:
The ionic liquid (IL), 1-allyl-3-(1-butyl)imidazolium chloride (AlBuImCl), has been synthesized and its properties determined. Increase in the temperature increased its conductivity and decreased its density, polarity, and viscosity. Microcrystalline cellulose (MCC), dissolves in thisIL by heating at 80 degrees C; this did not affect its degree of polymerization, decreased its index of crystallinity (Ic), and changed in morphology after regeneration. Convenient acylation of MCC was achieved by using 50% excess anhydride at 80 degrees C, for 24 or 48 h for acetic and butyric anhydride, respectively. The composition of the mixed esters depended on the initial ratio of the anhydrides, and their order of addition.
Resumo:
The swelling of microcrystalline, native and mercerized cotton and eucalyptus celluloses by 16 aprotic solvents was investigated. The number of moles of solvent/anhydroglucose unit, nSw, correlates well with solvent molar volume, basicity and dipolarity/polarizability. Swelling is sensitive to cellulose crystallite size, surface area and the presence of its chains in parallel or anti-parallel arrangements. Use of solvatochromic parameters is a superior alternative to the use of other descriptors, such as Hildebrand`s solubility parameters and Gutmann`s donor numbers. The calculated nSw for 28 protic and aprotic solvents correlated well with their experimental counterparts, although hydrogen bond donation by the solvent was not included.
Resumo:
The question posed in the title has been addressed by studying the swelling of celluloses at 20 C by twenty protic solvents, including water; linear- and branched-chain aliphatic alcohols; unsaturated aliphatic alcohols, and alkoxyalcohols. The biopolymers investigated included microcrystalline cellulose, MC, native and never-dried mercerized cotton cellulose, cotton and M-cotton, and native and never-dried mercerized eucalyptus cellulose, eucalyptus and M-eucalyptus, respectively. In most cases, better correlations with the physico-chemical properties of the solvents were obtained when the swelling was expressed as number of moles of solvent/anhydroglucose unit, nSw, rather than as % increase in sample weight. The descriptors employed in these correlations included, where available, Hildebrand`s solubility parameters, Gutmann`s acceptor and donor numbers, solvent molar volume, V(S), as well as solvatochromic parameters. The latter, employed for the first time for correlating the swelling of biopolymers, included empirical solvent polarity, E(T)(30), solvent ""acidity"", alpha(S), ""basicity"", beta(S), and dipolarity/polarizability, pi(S)*, respectively. Small regression coefficients and large sums of the squares of the residues were obtained when values of nSw were correlated with two solvent parameters. Much better correlations were obtained with three solvent parameters. The most statistically significant descriptor in the correlation equation depends on the cellulose, being pi(S)* for MC, cotton, and eucalyptus, and V(S) for M-cotton and M-eucalyptus. The best correlations were obtained with the same set of four parameters for all celluloses, namely, solvent pKa (or alpha(S)) beta(S), pi(S)*, and V(S), respectively. These results indicate that the supra-molecular structure of the biopolymer, in particular the average sizes of crystallites and micro-pores, and the presence of its chains in parallel (cellulose I) or anti-parallel (cellulose II) arrangements control its swelling. At least for the present biopolymer/solvent systems, use of solvatochromic parameters is a superior alternative to Hildebrand`s solubility parameters and/or Gutmann`s acceptor and donor numbers. The relevance of these results to the accessibility of the hydroxyl groups of cellulose, hence to its reactivity, is briefly discussed.
Resumo:
Co-solvents can minimize two of the major problems associated with the use of ionic liquids (ILs) as solvents for homogeneous derivatization of cellulose: high viscosity and limited miscibility with non-polar reagents or reaction products. Thus, the effects of 18 solvents and 3 binary solvent mixtures on cellulose solutions in three ILs were systematically studied with respect to the solution phase behavior. The applicable limits of these mixtures were evaluated and general guidelines for the use of co-solvents in cellulose chemistry could be advanced: Appropriate co-solvents should have EN T values (normalized empirical polarity) > 0.3, very low ``acidity`` (alpha < 0.5), and relatively high ""basicity`` (beta >= 0.4). Moreover, novel promising co-solvents and binary co-solvent mixtures were identified.
Resumo:
The acylation of three cellulose samples by acetic anhydride, Ac(2)O, in the solvent system LiCl/N,N-dimethylacetamide, DMAc (4 h, 110 A degrees C), has been revisited in order to investigate the dependence of the reaction efficiency on the structural characteristics of cellulose, and its aggregation in solution. The cellulose samples employed included microcrystalline, MCC; mercerized cotton linters, M-cotton, and mercerized sisal, M-sisal. The reaction efficiency expresses the relationship between the degree of substitution, DS, of the ester obtained, and the molar ratio Ac(2)O/AGU (anhydroglucose unit of the biopolymer); 100% efficiency means obtaining DS = 3 at Ac(2)O/AGU = 3. For all celluloses, the dependence of DS on Ac(2)O/AGU is described by an exponential decay equation: DS = DS(o) - Ae(-[(Ac2O/AGU)/B]); (A) and (B) are regression coefficients, and DS(o) is the calculated maximum degree of substitution, achieved under the conditions of each experiment. Values of (B) are clearly dependent on the cellulose employed: B((M-cotton)) > B((M-sisal)) > B((MCC)); they correlate qualitatively with the degree of polymerization of cellulose, and linearly with the aggregation number, N(agg), of the dissolved biopolymer, as calculated from static light scattering measurements: (B) = 1.709 + 0.034 N(agg). To our knowledge, this is the first report on the latter correlation; it shows the importance of the physical state of dissolved cellulose, and serves to explain, in part, the need to use distinct reaction conditions for MCC and fibrous celluloses, in particular Ac(2)O/AGU, time, temperature.
Resumo:
Two techniques, namely UV-vis- and FTIR spectroscopy, have been employed in order to calculate the degree of substitution (DS) of cellulose carboxylic esters, including acetates, CAs, butyrates, CBs, and hexanoates, CHs. Regarding UV-vis spectroscopy, we have employed a novel approach, based on measuring the dependence of lambda(max) of the intra-molecular charge-transfer bands of polarity probes adsorbed on DS of the ester films (solvatochromism). Additionally, we have revisited the use of FTIR for DS determination. Several methods have been used in order to plot Beer`s law graph, namely: Absorption of KBr pellets, pre-coated with CA: reflectance (DRIFTS) of CAs-KBr solid-solid mixtures with, or without the use of 1.4-dicyanobenzene as an internal reference; reflectance of KBr powder pre-coated with CA. The methods indicated are simple, fast, and accurate, requiring much less ester than the titration method. The probe method is independent of the experimental variables examined. (c) 2010 Published by Elsevier Ltd.