4 resultados para FTIR analysis

em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo (BDPI/USP)


Relevância:

30.00% 30.00%

Publicador:

Resumo:

Irradiation with heavy ions can produce several modifications in the chain structure of polymers. These modifications can be related to scissioning and cross-linking of chemical bonds. which depend on the ion fluence and the density of energy deposited in the material. Stacked thin film Makrofol-KG (R) samples were irradiated with 350 MeV Au(26+) ions and FTIR absorption spectroscopy was used to determine the bond changes in the samples. Data on the absorption bands as a function of the fluence indicated a higher probability for simple-bonds scissioning than for double-bonds scissioning and no dependence on the number of double bonds breaking with ion fluence. Since sample irradiation was done in a non-track-overlapping regime, a novel process for double bonds formation is suggested: the excitation of a site in the material by only one incident ion followed by a double bond formation during the de-excitation process. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Raman and IR experiments have been carried out on formamide (FA) and pyridine (Py) mixtures at different compositions. The appearance of a new Raman band at 996 cm(-1) (nu(1) region of Py), whose intensity depends on the FA concentration, is assigned to an FA: Py adduct and this result is in excellent agreement with those of other authors who employed noisy light-based coherent Raman scattering spectroscopy (I((2)) CARS). Another band at 1587 cm(-1) (nu(8) region of Py) has been observed for the first time by using Raman and IR spectroscopies. Its intensity shows the same dependence on the FA concentration and this fact allows us to also attribute it to an FA: Py adduct. The good relationship between the Raman and IR data demonstrates the potential of the vibrational spectroscopy for this kind of study. Owing to higher absolute Raman scattering cross section, the nu(1) region of Py has been chosen for the quantitative analysis and a stoichiometry of 1 : 1 FA: Py is reported. The experimental data are very well supported by the density functional theory (OFT) calculation, which was employed for the first time to the present system. Furthermore, the actual investigation shows an excellent agreement with those reported from computational calculations for similar systems. A comparison with our previous studies confirms that: the solvent dielectric constant determines the stoichiometry of a given Lewis acid-base adduct in the infinite dilution limit. Copyright (C) 2009 John Wiley & Sons, Ltd.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fourier Transformed Infrared Spectroscopy, Thermogravimetric Analysis, and X-ray Diffractometry have been used to investigate the rigid, semi rigid, and soft polyurethane (PU) forms, which were developed by the Group of Analytic Chemistry and Technology of Polymers - USF - Sao Carlos. The -NCO/-OH ratios were 0.6, 0.5, and 0.3% for rigid, semi rigid, and soft PUs, respectively, showing that different ratios cause differences in thermal behaviors and crystalline structures of the synthesized PU resins. (C) 2009 Wiley Periodicals, Inc. J Appl Polym Sci 115: 263-268, 2010

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The aim of this work was to evaluate the effect of the storage time on the thermal properties of triethylene glycol dimethacrylate/2,2-bis[4-(2-hydroxy-3-methacryloxy-prop-1-oxy)-phenyl]propane bisphenyl-alpha-glycidyl ether dimethacrylate (TB) copolymers used in formulations of dental resins after photopolymerization. The TB copolymers were prepared by photopolymerization with an Ultrablue IS light-emitting diode, stored in the dark for 160 days at 37 degrees C, and characterized with differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA), and Fourier transform infrared spectroscopy with attenuated total reflection. DSC curves indicated the presence of an exothermic peak, confirming that the reaction was not completed during the photopolymerization process. This exothermic peak became smaller as a function of the storage time and was shifted at higher temperatures. In DMA studies, a plot of the loss tangent versus the temperature initially showed the presence of two well-defined peaks. The presence of both peaks confirmed the presence of residual monomers that were not converted during the photopolymerization process. (C) 2009 Wiley Periodicals, Inc. J Appl Polym Sci 112: 679-684, 2009