ZrO(2), gamma-Al(2)O(3) and ZrO(2)/gamma-Al(2)O(3)-supported copper catalysts have been prepared, each with three different copper loads (1, 2 and 5 wt%), by the impregnation method. The catalysts were characterized by nitrogen adsorption (BET), X-ray diffraction (XRD), temperature programmed reduction (TPR) with H(2), Raman spectroscopy and electronic paramagnetic resonance (EPR). The reduction of NO by CO was studied in a fixed-bed reactor packed with these catalysts and fed with a mixture of 1% CO and 1% NO in helium. The catalyst with 5 wt% copper supported on the ZrO(2)/gamma-Al(2)O(3) matrix achieved 80% reduction of NO. Approximately the same rate of conversion was obtained on the catalyst with 2 wt% copper on ZrO(2). Characterization of these catalysts indicated that the active copper species for the reduction of NO are those in direct contact with the oxygen vacancies found in ZrO(2). (C) 2009 Published by Elsevier Ltd.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Co/Al(2)O(3) Fischer-Tropsch synthesis catalysts promoted with different quantities of Group 11 metals (Cu, Ag, Au) were characterized and tested. The presence of relatively small quantities of such metals enhanced Co reducibility and, in the cases of Ag and Au, improved the surface Co metal active site densities. EXAFS experiments with the most loaded catalyst samples show that only Co-Co and Me-Me (Me = Cu, Ag and Au) coordination could be observed. This suggests that the greater fraction of the metals form different phases. However, the reduction promoting effect of the Group 11 metal is severely hampered once the catalyst receives a mild passivation treatment following primary reduction. An explanation in terms of promoter segregation during primary reduction is proposed. At lower promoter levels (0.83%Ag and 1.51%Au) and higher Ag levels (2.76%), significant gains in Co active site densities were achieved resulting in improved CO conversion levels relative to the unpromoted catalyst. Moreover, slight decreases in light product (e.g., CH(4)) selectivity and slight increases in C(5)+ selectivity were achieved. At high Au loading (5.05%), however, too much Au was loaded which, although significantly increasing the fraction of Co reduced, blocked Co surface sites and resulted in decreased Co conversion rates. While Cu facilitated Co reduction, the increased fraction of reduced Co did not translate to improved active site densities. It appears that a fraction of Cu tended to cover the rim of Co clusters, resulting in decreases in CO conversion rates and detrimental increases in light product selectivity. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Catalysts with various nickel loads were prepared on supports of ZrO2, ZrO2-Y2O3 and ZrO2-CaO, characterized by XRD and TPR and tested for activity in ethanol steam reforming. XRD of the supports identified the monoclinic crystalline phase in the ZrO2 and cubic phases in the ZrO2-Y2O3 and ZrO2-CaO supports. In the catalysts, the nickel impregnated on the supports was identified as the NiO phase. In the TPR analysis, peaks were observed showing the NiO phase having different interactions with the supports. In the catalytic tests, practically all the catalysts achieved 100% ethanol conversion, H-2 yield was near 70% and the gaseous concentrations of the other co-products varied in accordance with the equilibrium among them, affected principally by the supports. It was observed that when the ZrO2 was modified with Y2O3 and CaO, there were big changes in the CO and CO2 concentrations, which were attributed to the rise in the number of oxygen vacancies, permitting high-oxygen mobility and affecting the gaseous equilibrium. The liquid products analysis showed a low selectivity to liquid co-products during the reforming reactions. (c) 2007 Published by Elsevier B.V.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Catalysts containing NiO/MgO/ZrO(2) mixtures were synthesized by the polymerization method in a single step. They were characterized by X-ray diffraction (XRD), temperature programmed reduction (TPR) and physisorption of N(2) (BET) and then tested in the reforming of a model biogas (1.5CH4:1CO(2)) in the presence of air (1.5CH(4) + 1CO(2) + 0.25O(2)) at 750 degrees C for 6h. It was observed that the catalyst Ni20MZ performed better in catalytic processes than the well known catalysts, Ni/ZrO(2) and Ni/MgO, synthesized under the same conditions. The formation of solid solutions, MgO-ZrO(2) and NiO-MgO, increased the rate of conversion of reactants (CH(4) and CO(2)) into synthesis gas (H(2) + CO). The formation of oxygen vacancies (in samples containing ZrO(2) and MgO) seems to promote removal of the coke deposited on the nickel surface. The values of the H(2)/CO ratio were generally found to be slightly lower than stoichiometric, owing to the reverse water gas shift reaction occurring in parallel. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper describes an investigation on CuO and CuO-ZnO catalysts supported on CeO(2) and CeO(2)-La(2)O(3) oxides, which were designed for the low temperature water-gas shift reaction (WGSR). Bulk catalysts were prepared by co-precipitation of metal nitrates and characterized by energy-dispersive spectroscopy (EDS), X-ray diffraction (XRD), surface area (by the BET method), X-ray photoelectron spectroscopy (XPS), and in situ X-ray absorption near edge structure (XANES). The catalysts` activities were tested in the forward WGSR, and the CuO/CeO(2) catalyst presented the best catalytic performance. The reasons for this are twofold: (1) the presence of Zn inhibits the interaction between Cu and Ce ions, and (2) lanthanum oxide forms a solid solution with cerium oxide, which will cause a decrease in the surface area of the catalysts. Also the CuO/CeO(2) catalyst presented the highest Cu content on the surface, which could influence its catalytic behavior. Additionally, the Cu and Cu(1+) species could influence the catalytic activity via a reduction-oxidation mechanism, corroborating to the best catalytic performance of the Cu/Ce catalyst. (c) 2010 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Supported nickel catalysts of composition Ni/Y(2)O(3)-ZrO(2) were synthesized in one step by the polymerization method and compared with a nickel catalyst prepared by wet impregnation. Stronger interactions were observed in the formed catalysts between NiO species and the oxygen vacancies of the Y(2)O(3)-ZrO(2) in the catalysts made by polymerization, and these were attributed to less agglomeration of the NiO during the synthesis of the catalysts in one step. The dry reforming of ethanol was catalyzed with a maximum CO(2) conversion of 61% on the 5NiYZ catalyst at 800 degrees C, representing a better response than for the catalyst of the same composition prepared by wet impregnation. (C) 2009 Published by Elsevier B.V.