Resumo:
Objectives: To analyze the expression of tenascin, fibronectin, collagens I and III, osteonectin, and bone morphogenetic protein 4 (BMP4) in the extracellular matrix of pulp tissue in primary teeth during physiologic root resorption. Method and Materials: Eighteen teeth were decalcified and equally distributed into 3 groups (group I, teeth with two-thirds root length; group II, teeth with one-third root length; and group III, teeth lacking the root). Results: Immunohistochemical analysis showed that all the proteins were expressed. Tenascin, collagen I, and osteonectin showed strong and broad reactivity in group I, with weaker and rare reactivity in groups II and III. The expression of fibronectin, collagen III, and BMP4 did not vary with root resorption phase. Conclusion: The expression of tenascin, collagen I, and osteonectin was reduced in the extracellular matrix and odontoblasts during root resorption. This fact may be related to the decreasing pulp response to damage and treatment during the progression of root resorption. (Quintessence Int 2009; 40: 553-558)
Resumo:
Objective. To determine the slow crack growth (SCG) and Weibull parameters of five dental ceramics: a vitreous porcelain (V), a leucite-based porcelain (D), a leucite-based glass-ceramic (E1), a lithium disilicate glass-ceramic (E2) and a glass-infiltrated alumina composite (IC). Methods. Eighty disks (empty set 12mm x 1.1mm thick) of each material were constructed according to manufacturers` recommendations and polished. The stress corrosion susceptibility coefficient (n) was obtained by dynamic fatigue test, and specimens were tested in biaxial flexure at five stress rates immersed in artificial saliva at 37 degrees C. Weibull parameters were calculated for the 30 specimens tested at 1MPa/s in artificial saliva at 37 degrees C. The 80 specimens were distributed as follows: 10 for each stress rate (10(-2), 10(-1), 10(1), 10(2) MPa/s), 10 for inert strength (10(2) MPa/s, silicon oil) and 30 for 10(0) MPa/s. Fractographic analysis was also performed to investigate the fracture origin. Results. E2 showed the lowest slow crack growth susceptibility coefficient (17.2), followed by D (20.4) and V (26.3). E1 and IC presented the highest n values (30.1 and 31.1, respectively). Porcelain V presented the lowest Weibull modulus (5.2). All other materials showed similar Weibull modulus values, ranging from 9.4 to 11.7. Fractographic analysis indicated that for porcelain D, glass-ceramics E1 and E2, and composite IC crack deflection was the main toughening mechanism. Significance. This study provides a detailed microstructural and slow crack growth characterization of widely used dental ceramics. This is important from a clinical standpoint to assist the clinician in choosing the best ceramic material for each situation as well as predicting its clinical longevity. It also can be helpful in developing new materials for dental prostheses. (c) 2010 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
The objective was to compare fracture toughness (K(Ic)), stress corrosion susceptibility coefficient (n), and stress intensity factor threshold for crack propagation (K(I0)) of two porcelains [VM7/Vita (V) and d.Sign/Ivoclar (D)], two glass-ceramics [Empress/Ivolcar (E1) and Empress2/Ivlocar (E2)] and a glass-infiltrated alumina composite [In-Ceram Alumina/Vita (IC)]. Disks were constructed according to each manufacturer`s processing method, and polished before induction of cracks by a Vickers indenter. Crack lengths were measured under optical microscopy at times between 0.1 and 100 h. Specimens were stored in artificial saliva at 37A degrees C during the whole experiment. K(Ic) and n were determined using indentation fracture method. K(I0) was determined by plotting log crack velocity versus log K(I). Microstructure characterization was carried out under SEM, EDS, X-ray diffraction and X-ray fluorescence. IC and E2 presented higher K(Ic) and K(I0) compared to E1, V, and D. IC presented the highest n value, followed by E2, D, E1, and V in a decreasing order. V and D presented similar K(Ic), but porcelain V showed higher K(I0) and lower n compared to D. Microstructure features (volume fraction, size, aspect ratio of crystalline phases and chemical composition of glassy matrix) determined K(Ic). The increase of K(Ic) value favored the increases of n and K(I0).
Resumo:
The objective of the current study was to characterize the internal nasal dimensions of children with repaired cleft lip and palate and transverse maxillary deficiency, using acoustic rhinometry and analyze the changes caused by rapid maxillary expansion (RME). A convenience sampling of 19 cleft lip and palate individuals, aged 14 to 18 years, of both sexes, previously submitted to primary surgeries and referred for RME were analyzed prospectively at the Hospital for Rehabilitation of Craniofacial Anomalies, University of Sao Paulo, Bauru, Sao Paulo, Brazil. All patients underwent acoustic rhinometry before installation of the expansor and at 30 and 180 days after the active expansion phase. Nasal cross-sectional areas and volumes corresponding to the nasal valve (CSA(1) and V(1)) and the turbinates (CSA(2), CSA(3), and V(2)) regions were determined before and after nasal decongestion. Rapid maxillary expansion led to a statistically significant increase (P < 0.05) in mean CSA(1), CSA(2), V(1), and V(2) (without nasal decongestion) and in CSA(1) and V(1) (with decongestion) in the group as a whole. Individual data analysis showed that 58% of the patients responded positively to RME, with an average increase in CSA(1) of 26% (with decongestion), whereas 37% of the patients had no significant change. Only 1 patient (5%) showed a decrease. The findings contribute toward the characterization of nasal deformities determined by the cleft and demonstrate the positive effect RME had on nasal morphophysiology in a significant number of the patients who underwent this procedure.
Resumo:
P>Aim To assess the push-out strength of Epiphany SE, Epiphany and Hybrid Root SEAL to the dentine walls of root canals. Methodology Sixty roots of canines were prepared and distributed to six groups (n = 10) according to the filling material: GI - Epiphany SE, GII - Epiphany primer and sealer, GIII - Epiphany primer, sealer and resinous solvent, GIV - Clearfil DC Bond and Epiphany sealer, GV - Clearfil, Epiphany sealer and solvent and GVI - Hybrid Root SEAL. Resilon cones were used in all groups. Roots were sectioned transversally to obtain three slices from each third. One slice was subjected to the push-out test (MPa), and results were analysed by anova and Tukey`s test (P < 0.05). The other two slices were prepared for scanning electron microscopy (SEM). Failure mode was also analysed. Results A statistically significant difference (P < 0.05) occurred between Hybrid Root SEAL (5.27 +/- 2.07) and the other materials, GI (0.40 +/- 0.23), GII (0.78 +/- 0.45), GIII (0.57 +/- 0.28), GIV (0.40 +/- 0.24) and GV (0.50 +/- 0.41), which did not differ significantly from each other (P > 0.05). Adhesive failures predominated in groups I, II, IV and V, whilst mixed and cohesive failures were the most frequent in groups III and VI, respectively. There were gaps in the adhesive interface of GI and GII, continuity areas of the filling material with dentine in GIV and GV and good adaptation of the interface of GVI. Conclusion Hybrid Root SEAL had greater push-out strength to root canal dentine than Epiphany SE and Epiphany. The use of primer, solvent and adhesive system did not influence the adhesion of Epiphany.
Resumo:
Objectives: The aim of this study was to assess the fracture resistance of endodontically treated teeth submitted to bleaching with 38% hydrogen peroxide activated by light-emitting diode (LED)-laser system. Methods: Fifty maxillary incisors were endodontically treated, received a zinc phosphate barrier and were embedded in acrylic resin until cemento-enamel junction. The specimens were distributed into five groups (n = 10) according to the number of bleaching sessions: GI, no treatment (control); GII, one session; GIII, two sessions; GIV, three sessions and GV, four sessions. The whitening gel was applied to the buccal surface of the tooth and inside the pulp chamber for three times in each session, followed by LED-laser activation. Specimens were submitted to the fracture resistance test (kN) and data were submitted to the Tukey-Kramer multiple comparisons test. Results: No significant difference (p > 0.05) was found between GI (0.71 +/- 0.30) and GII (0.65 +/- 0.13), which presented the highest strength values to fracture. Groups III (0.35 +/- 0.17), IV (0.23 +/- 0.13) and V (0.38 +/- 0.15) showed lower resistance to fracture (p < 0.01) when compared to GI and GII. Conclusions: The fracture resistance of endodontically treated teeth decreased after two sessions of bleaching with 38% hydrogen peroxide activated by LED-laser system. (c) 2008 Elsevier Ltd. All rights reserved.
Resumo:
Objective. The aim of this study was to evaluate the biocompatibility of the root canal sealer Epiphany in rat subcutaneous tissues. Study design. Polyethylene tubes were filled with the sealer (I: Epiphany; II: photoactivated Epiphany; III: Epiphany associated with self-etch primer; IV: photoactivated Epiphany associated with primer; and V: control group) and later implanted into 4 different regions of the dorsum of 15 adult male rats (Rattus novergicus, Albinus Wistar). After 7, 21, and 42 days, 5 animals were killed, obtaining 4 samples per group, in addition to the control group, at each analyzed time. Results. In all periods, Epiphany induced a mild inflammatory reaction. However, in group II, in which the primer was not used, extensive necrosis and a moderate to intense inflammatory reaction were observed, mainly after 7 and 21 days. Conclusion. Epiphany sealer appears biocompatible when tested on rat subcutaneous tissues.