Resumo:
The adhesive performance on deproteinized dentin of different self-adhesive resin cements was evaluated through microtensile bond strength (mu TBS) analysis and scanning electron microscopy (SEM). Occlusal dentin of human molars were distributed into different groups, according to the categories: adhesive cementation with two-step bonding systems-control Groups (Adper Single Bond 2 + RelyX ARC/3M ESPE; One Step Plus + Duolink/Bisco; Excite + Variolink I/Ivoclar Vivadent) and self-adhesive cementation-experimental groups (Rely X Unicem/3M ESPE; Biscem/Bisco; MultiLink Sprint/Ivoclar Vivadent). Each group was subdivided according to the dentin approach to: alpha, maintenance of collagen fibers and beta, deproteinization. The mean values were obtained, and submitted to ANOVA and Tukey test. Statistical differences were obtained to the RelyX Unicem groups (alpha = 13.59 MPa; beta = 30.19 MPa). All the BIS Group specimens failed before the mechanical tests. Dentinal deproteinization provided an improved bond performance for the self-adhesive cement Rely X Unicem, and had no negative effect on the other cementing systems studied. (C) 2011 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater 98B: 387-394, 2011.
Resumo:
The aim of this in vitro study was to evaluate qualitatively the surface morphology of enamel bleached with 35% hydrogen peroxide (HP) followed by application of fluoridated agents. Forty intact pre molars were randomly distributed into four groups (n = 10), treated as follows: Group I (control group) remained stored in artificial saliva at 37 degrees C, Group II - 35% HP; Group III - 35% HP + acidulated fluoride (1.23%) and Group IV - 35% HP + neutral fluoride (2%). The experimental groups received three applications of bleaching gel and after the last application all specimens were polished. This procedure was repeated after 7 and 14 days, and during the intervals of applications, the specimens were stored in artificial saliva at 37 degrees C. Scanning electron microscopy (SEM) analysis showed superficial irregularities and porosities to varying degrees in bleached enamel compared to control group. Sample evaluation was made by attributing scores, and data were statistically analyzed using Kruskal-Wallis and Dunn tests (P < 0.05). SEM qualitative investigation demonstrated that 35% hydrogen peroxide affected human dental enamel morphology, producing porosities, depressions, and superficial irregularities at various degrees. These morphological changes were higher after the application of 1.23% acidulated fluoride gel. Microsc. Res. Tech. 74:512-516, 2011. (C) 2010 Wiley-Liss, Inc.
Resumo:
The purpose of this study was to evaluate the characteristics of diseased root surfaces treated by the association of scaling and the application of Carisolv. Twenty-four uniradicular periodontally involved teeth were used in this study The teeth were divided randomly into three groups: eight teeth were scaled and root planed until there was a complete visible removal of calculus (group 1), Carisolv was applied on the root surfaces of eight teeth twice for 30 seconds before scaling with a sharp curette (group 2), and eight teeth received the same treatment as in group 2 but with a blunt curette (group 3). Specimens were examined using scanning electron microscopy The superficial aspect of the roots from group 1 presented scratches that mirrored the curette cutting edge, and the smear layer completely covered the surface. Root surfaces from groups 2 and 3 also presented a smear layer that covered the surface completely but it was somewhat smoother than group 1. The use of Carisolv as an adjunct to scaling and root planing presented no advantage for smear layer removal over scaling alone, suggesting that no benefit is obtained by the use of Carisolv during periodontal mechanical treatment. (Int J Periodontics Restorative Dent 2011;31:91-95.)
Resumo:
The aim of this in vitro study was to investigate the effect of erbium:yttrium-aluminum-garnet (Er:YAG) laser irradiation on dentinal collagen by transmission electron microscopy and to analyze the resin-dentin interface by scanning electron microscopy. A tensile bond strength test was also applied. Specimens from 69 sound human third molars were randomly divided into three groups: control (no laser), and two irradiated groups, laser 250 (250 mJ/2 Hz) and laser 400 (400 mJ/4 Hz). Then, specimens were restored with two adhesive systems, an etch-and-rinse or a self-etch system. Although ultrastructural examination showed a modified surface in the irradiated dentin, there was no statistical difference in bond strength values between the laser groups and controls (P < 0.05). In conclusion, the use of Er:YAG laser for ablating human dentin did not alter the main adhesion parameters when compared with those obtained by conventional methods, thus reinforcing its use in restorative dentistry.
Resumo:
Introduction: This study compared the combined use of sodium hypochlorite (NaOCl) and chlorhexidine (CXH) with citric acid and CXH on dentinal permeability and precipitate formation. Methods: Thirty-four upper anterior teeth were prepared by rotary instrumentation and NaOCl. The root canal surfaces were conditioned for smear layer removal using 15% citric acid solution under ultrasonic activation and a final wash with distilled water. All teeth were dried, and 30 specimens were randomly divided into three equal groups as follows: positive control group (PC), no irrigation; 15% citric acid + 2% CHX group (CA + CHX); and 1% NaOCl + 2% CHX group (NaOCl + CHX). All roots were immersed in a 0.2% Rhodamine B solution for 24 hours. One-millimeter-thick slices from the cementum-enamel junction were scanned at 400 dpi and analyzed using the software ImageLab (LIDO-USP, Sao Paulo, Brazil) for the assessment of leakage in percentage. For scanning electron microscopy analysis, four teeth, irrigated for NaOCl + CHX samples, were split in half, and each third was evaluated at 1,000x and 5,000x (at the precipitate). Results: Using the analysis of variance test followed by the Bonferroni comparison method, no statistical differences between groups were found when analyzed at the cervical and medium thirds. At the apical third, differences between the PC and NaOCl + CHX (p<0.05) and CA + CHX and NaOCl + CHX could be seen (p < 0.05). Conclusion: The combination of 1% NaOCl and 2% CHX solutions results in the formation of a flocculate precipitate that acts as a chemical smear layer reducing the dentinal permeability in the apical third. (J Endod 2010;36:847-850)
Resumo:
This study compared ultrasonic chemical vapor deposition (CVD)-coated tip (CVDentus #8.1117-1; Clorovale Diamantes Ind. e Com. Ltda Epp, Sao Jose dos Campos, SP, Brazil) versus high-speed (#FG700L) and low-speed (#699) carbide burs for apicoectomy, evaluating the time required for resection and analyzing the root-end surfaces by scanning electron microscopy. Thirty extracted human premolars had the canals instrumented and obturated and were randomly assigned to 3 groups (n = 10), according to the instrument used for root-end resection. The time required for resection of the apical 2 mm of each root was recorded. The resected apical segments were dried, sputter coated with gold, and examined with a scanning electron microscope at X 350 magnification. A four-point (0-3) scoring system was used to evaluate the apical surface smoothness. The results were analyzed statistically by the Kruskal-Wallis test and two-by-two comparisons analyses were performed using the Miller test. The significance level was set at 5%. Root-end resection with the high-speed bur was significantly faster (p < 0.05) compared with the low-speed bur and CVD tip. The carbide burs produced significantly smoother root-end surfaces than the CVD tip (p < 0.05). The low-speed bur produced the smoothest root-end surfaces, whereas the roughest and most irregular root ends (p < 0.05) were obtained with the CVD tip. However, no statistically significant difference (p > 0.05) was found between the high- and low-speed burs regarding the surface roughness of the resected root ends (p > 0.05). In conclusion, under the tested conditions, ultrasonic root-end resection took a longer time and resulted in rougher surfaces compared with the use of carbide burs at both high and low speed. (J Endod 2009;35:265-268)
Resumo:
This study evaluated the surface integrity of sutures after immersion in mouthrinse or water, by scanning electron microscopy (SEM) analysis. Pieces of resorbable suture remaining after oral surgery were immediately collected. Twelve pieces each of catgut, chromed catgut, and polyglactin 910 were divided into four groups and immersed in pure mouthrinse, mouthrinse diluted in water at 1:1 and 1:2, or water (positive control), for 24 h. Three pieces each of new sutures were used as negative control. Specimens were placed on stubs and sputter coated with gold for SEM analysis. Observation of experimental groups and comparison with controls revealed that immersion in the mouthrinse at different dilutions did not alter their surface; slight, nonsignificant changes were found in some experimental specimens yet also in the positive control group. It was concluded that immersion of resorbable sutures in water or non-alcoholic benzydamine hydrochloride mouthrinse did not produce any significant change; therefore, this mouthrinse may be safely employed after oral surgery.
Resumo:
This study evaluated the cytotoxic effects of a carbamide peroxide (CP) bleaching gel at different concentrations on odontoblast-like cells. Immortalized cells of the MDPC-23 cell line (30,000 cells/cm(2)) were incubated for 48 h. The bleaching gel was diluted in DMEM culture medium originating extracts with different CP concentrations. The amount (mu g/mL) of hydrogen peroxide (H(2)O(2)) released from each extract was measured by the leukocrystal violet/horseradish peroxidase enzyme assay. Five groups (n = 10) were formed according to the CP concentration in the extracts: G1-DMEM (control); G2-0.0001 % CP (0.025 mu g/mL H(2)O(2)); G3-0.001% CP (0.43 mu g/mL H(2)O(2)); G4-0.01% CP (2.21 mu g/mL H(2)O(2)); and G5-0.1 % CP (29.74 mu g/mL H(2)O(2)). MDPC-23 cells were exposed to the bleaching gel extracts for 60 min and cell metabolism was evaluated by the NITT assay. Data were analyzed statistically by one-way ANOVA and Tukey`s test (alpha = 0.05). Cell morphology was examined by scanning electron microscopy. The percentages of viable cells were as follows: G1, 100%; G2, 89.41%; G3, 82.4%; G4, 61.5%; and G5, 23.0%. G2 and G3 did not differ significantly (p > 0.05) from G1. The most severe cytotoxic effects were observed in G3 and G4. In conclusion, even at low concentrations, the CP gel extracts presented cytotoxic effects. This cytotoxicity was dose-dependent, and the 0.1% CP concentration caused the most intense cytopathic effects to the MDPC-23 cells. (C) 2009 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater 9013: 907-912, 2009
Resumo:
The aims of this study were 1) to verify how close to the theoretically presumed areas are the areas of enamel microbiopsies carried out in vivo or in exfoliated teeth; 2) to test whether the etching solution penetrates beyond the tape borders: 3) to test whether the etching solution demineralizes the enamel in depth. 24 shed upper primary central incisors were randomly divided into two groups: the Rehydrated Teeth Group and the Dry Teeth Group. An enamel microbiopsy was performed, and the enamel microbiopsies were then analyzed by Scanning Electron Microscopy (SEMI) and Polarizing Microscopy (PM). Quantitative birefringence measurements were performed. The ""true"" etched area was determined by measuring the etched enamel using the NIH Image analysis program. Enamel birefringence was compared using the paired t test. There was a statistically significant difference when the etched areas in the Rehydrated teeth were compared with those of the Dry teeth (p = 0.04). The etched areas varied from -11.6% to 73.5% of the presumed area in the Rehydrated teeth, and from 6.6% to 61.3% in the Dry teeth. The mean percentage of variation in each group could be used as a correction factor for the etched area. Analysis of PM pictures shows no evidence of in-depth enamel demineralization by the etching solution. No statistically significant differences in enamel birefringence were observed between values underneath and outside the microbiopsy area in the same tooth, showing that no mineral loss occurred below the enamel superficial layer. Our data showed no evidence of in-depth enamel demineralization by the etching solution used in the enamel microbiopsy proposed for primary enamel. This study also showed a variation in the measured diameter of the enamel microbiopsy in nineteen teeth out of twenty four, indicating that in most cases the etching solution penetrated beyond the tape borders. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Background: There are no reported studies comparing different parameter settings of the CO(2) laser and irradiation direction considering their effect on the morphology of radicular dentine surface. Purpose: To evaluate the alterations of radicular dentine (cervical, middle, and apical thirds) irradiated with CO(2) laser at different potencies and irradiation directions. Study Design: Roots of 35 canines were prepared and randomly distributed according to the laser potency: GI: no laser treatment (control) (n = 5); GII, 2 W (n = 10); GIII: 4 W (n = 10); GIV: 6 W (n = 10). Each group (excepting GI) was divided in two subgroups according to the irradiation distance (n = 5): (A) parallel and (B) perpendicular to the root canal walls. The roots were splited longitudinally and analyzed by scanning electron microscopy in a qualiquatitative way. The scores were submitted to Kruskal-Wallis and Dunn`s tests. Results: No significant statistical differences were observed among root canal thirds (P > 0.05). The specimens irradiated with 2 W were statistically different (P < 0.05) from those irradiated with 4 and 6 W, which were statistically similar between themselves (P > 0.05). With 2, 4, and 6 W at in parallel irradiation and 2 W in perpendicular direction, the surface showed a fissured aspect. With 4 W in perpendicular direction and 6 W in parallel and perpendicular direction, surface was modified by laser action and exhibited fused areas. Conclusions: The intensity of the effects is dependent on the laser-irradiation dosimetries. Alterations were more intense when higher parameters were used. Microsc. Res. Tech. 72:737-743, 2009. (C) 2009 Wiley-Liss, Inc.
Resumo:
Aim. The aim of this study was to evaluate the concentration of calcium ions and smear layer removal by using root canal chelators according to flame atomic absorption spectrophotometry and scanning electron microscopy. Forty-two human maxillary central incisors were irrigated with 15% ethylenediaminetetraacetic acid (EDTA), 10% citric acid, 10% sodium citrate, apple vinegar, 5% acetic acid, 5% malic acid, and sodium hypochlorite. The concentration of calcium ions was measured by using flame atomic absorption spectrometry, and smear layer removal was determined by scanning electron microscopy. Mean +/- standard deviation, one-way analysis of variance, Tukey-Kramer, Kruskal-Wallis, Dunn, and kappa tests were used for statistical analysis. The use of 15% EDTA resulted in the greatest concentration of calcium ions followed by 10% citric acid; 15% EDTA and 10% citric acid were the most efficient solutions for removal of smear layer. (J Endod 2009;35:727-730)
Resumo:
Background: The topographical features of intraradicular dentine pretreated with sodium hypochlorite (NaOCl) or ethylenediamine tetraacetic acid (EDTA) followed by diode laser irradiation have not yet been determined. Purpose: To evaluate the alterations of dentine irradiated with 980-nm diode laser at different parameters after the surface treatment with NaOCl and EDTA. Study design: Roots of 60 canines were biomechanically prepared and irrigated with NaOCl or EDTA. Groups were divided according to the laser parameters: 1.5 W/CW; 1.5 W/100 Hz; 3.0 W/CW; 3.0 W/100 Hz and no irradiation (control). The roots were splited longitudinally and analyzed by scanning electron microscopy (SEM) in a quali-quatitative way. The scores were submitted to two-way Kruskal-Wallis and Dunn`s tests. Results: The statistical analysis demonstrated that the specimens treated only with NaOCl or EDTA (control groups) were statistically different (P < 0.05) from the laser-irradiated specimens, regardless of the parameter setting. The specimens treated with NaOCl showed a laser-modified surface with smear layer, fissures, and no visible tubules. Those treated with EDTA and irradiated by laser presented absence of smear layer, tubules partially exposed and melting areas. Conclusions: The tested parameters of 980-nm diode laser promoted similar alterations on dentine morphology, dependent to the type of surface pretreatment. Microsc. Res. Tech. 72:22-27, 2009. (C) 2008 Wiley-Liss, Inc.
Resumo:
Cigarette smoke is a significant source of cadmium, lead, and toxic elements, which are absorbed into the human organism. In this context, the aim of this study was to investigate in vitro the presence of toxic elements, cadmium, and lead deriving from cigarette smoke in the resin composite, dentine, and dental enamel. Eight cylindrical specimens were fabricated from resin composite, bovine enamel, and root dentin fragments that were wet ground and polished with abrasive paper to obtain sections with 6-mm diameter and 2-mm thickness. All specimens were exposed to the smoke of 10 cigarettes/day during 8 days. After the simulation of the cigarette smoke, the specimens were examined with scanning electron microscopy (SEM) and the energy-dispersive X-ray analysis. In the photomicrographic analysis in SEM, no morphological alterations were found; however, the microanalysis identified the presence of cadmium, arsenic, and lead in the different specimens. These findings suggest that the deposition of these elements derived from cigarette smoke could be favored by dental structures and resin composite. Microsc. Res. Tech. 74:287-291, 2011. (C) 2010 Wiley-Liss, Inc.
Resumo:
Background Long-term success of the implant restorations is based upon the biology and vasculature of the bone surrounding the implants, especially for the bone between two implants. Purpose The aim of this study was to evaluate how loaded implants placed 2 or 3 mm apart influence bone vessel organization. Material and methods Six mongrel dogs were used for the study. The four mandibular premolars were extracted and 3 months later, four 4.5 x 10 mm implants were placed on each side of the mandible. The implants were placed so that two adjacent implants were 2 mm (group 1) or 3 mm (group 2) distant from each other. After 12 weeks, the implants were loaded with provisional prostheses, then metallic crowns were placed 4 weeks later. Both temporary and metallic restorations were made so that the distance between the contact point and the bone crest was 5 mm. The animals were sacrificed after 8 weeks. The hemi-mandibles were removed and prepared for analysis. The interimplant bone vasculature of the two groups was studied using scanning electron microscopic images fractal analysis. The fractal dimension (D(f)) was calculated using the box-counting method. Results The values of the D(f) for the blood vessels were significantly higher (P <.05) in the specimens of the group 2 (1.969 +/- 0.169) than the group 1 (1.556 +/- 0.246). Conclusion The presence of more blood vessels in the group 2 is another indication that 3 mm is a preferable distance for contiguous implants than the 2 mm distance. To cite this article:Traini T, Novaes AB, Piattelli A, Papalexiou V, Muglia VA. The relationship between interimplant distances and vascularization of the interimplant bone.Clin. Oral Impl. Res. 21, 2010; 822-829.doi: 10.1111/j.1600-0501.2010.01926.x.
Resumo:
Modified fluorcanasite glasses were fabricated by either altering the molar ratios of Na(2)O and CaO or by adding P(2)O(5) to the parent stoichiometric glass compositions. Glasses were converted to glass-ceramics by a controlled two-stage heat treatment process. Rods (2 mm x 4 mm) were produced using the conventional lost-wax casting technique. Osteoconductive 45S5 bioglass was used as a reference material. Biocompatibility and osteoconductivity were investigated by implantation into healing defects (2 mm) in the midshaft of rabbit femora. Tissue response was investigated using conventional histology and scanning electron microscopy. Histological and histomorphometric evaluation of specimens after 12 weeks implantation showed significantly more bone contact with the surface of 45S5 bioglass implants when compared with other test materials. When the bone contact for each material was compared between experimental time points, the Glass-Ceramic 2 (CaO rich) group showed significant difference (p = 0.027) at 4 weeks, but no direct contact at 12 weeks. Histology and backscattered electron photomicrographs showed that modified fluorcanasite glass-ceramic implants had greater osteoconductivity than the parent stoichiometric composition. Of the new materials, fluorcanasite glass-ceramic implants modified by the addition of P(2)O(5) showed the greatest stimulation of new mineralized bone tissue formation adjacent to the implants after 4 and 12 weeks implantation. (C) 2010 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 94A: 760-768, 2010