189 resultados para feed additive


Relevância:

10.00% 10.00%

Publicador:

Resumo:

Silicon nitride ceramics were sintered using Y(2)O(3)-Al(2)O(3) or E(2)O(3)-Al(2)O(3) (E(2)O(3) denotes a mixed oxide Of Y(2)O(3) and rare-earth oxides) as sintering additives. The intergranular phases formed after sintering was investigated using high-resolution X-ray diffraction (HRXRD). The use of synchrotron radiation enabled high angular resolution and a high signal to background ratio. Besides the appearance Of beta-Si(3)N(4) phase the intergranular phases Y(3)Al(5)O(12) (YAG) and Y(2)SiO(5) were identified in both samples. The refinement of the structural parameters by the Rietveld method indicated similar crystalline structure Of beta-Si(3)N(4) for both systems used as sintering additive. On the other hand, the intergranular phases Y(3)Al(5)O(12) and Y(2)SiO(5) shown a decrease of the lattice parameters, when E(2)O(3) was used as additive, indicating the formation of solid solutions of E(3)Al(5)O(12) and E(2)SiO(5), respectively. (C) 2007 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper presents a formulation to deal with dynamic thermomechanical problems by the finite element method. The proposed methodology is based on the minimum potential energy theorem written regarding nodal positions, not displacements, to solve the mechanical problem. The thermal problem is solved by a regular finite element method. Such formulation has the advantage of being simple and accurate. As a solution strategy, it has been used as a natural split of the thermomechanical problem, usually called isothermal split or isothermal staggered algorithm. Usual internal variables and the additive decomposition of the strain tensor have been adopted to model the plastic behavior. Four examples are presented to show the applicability of the technique. The results are compared with other authors` numerical solutions and experimental results. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A study was performed regarding the effect of the relation between fill time, volume treated per cycle, and influent concentration at different applied organic loadings on the stability and efficiency of an anaerobic sequencing batch reactor containing immobilized biomass on polyurethane foam with recirculation of the liquid phase (AnSBBR) applied to the treatment of wastewater from a personal care industry. Total cycle length of the reactor was 8 h (480 min). Fill times were 10 min in the batch operation, 4 h in the fed-batch operation, and a 10-min batch followed by a 4-h fed batch in the mixed operation. Settling time was not necessary since the biomass was immobilized and decant time was 10 min. Volume of liquid medium in the reactor was 2.5 L, whereas volume treated per cycle ranged from 0.88 to 2.5 L in accordance with fill time. Influent concentration varied from 300 to 1,425 mg COD/L, resulting in an applied volumetric organic load of 0.9 and 1.5 g COD/L.d. Recirculation flow rate was 20 L/h, and the reactor was maintained at 30 A degrees C. Values of organic matter removal efficiency of filtered effluent samples were below 71% in the batch operations and above 74% in the operations of fed batch followed by batch. Feeding wastewater during part of the operational cycle was beneficial to the system, as it resulted in indirect control over the conversion of substrate into intermediates that would negatively interfere with the biochemical reactions regarding the degradation of organic matter. As a result, the average substrate consumption increased, leading to higher organic removal efficiencies in the fed-batch operations.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The influence of impeller type and stirring frequency on the performance of a mechanically stirred anaerobic sequencing batch reactor containing immobilized biomass on an inert support (AnSBBR - Anaerobic Sequencing Batch Biofilm Reactor) was evaluated. The biomass was immobilized on polyurethane foam cubes placed in a stainless-steel basket inside a glass cylinder. Each 8-h batch run consisted of three stages: feed (10 min), reaction (460 min) and discharge (10 min) at 30 degrees C. Experiments were performed with four impeller types, i.e., helical, flat-blade, inclined-blade and curved-blade turbines, at stirring frequencies ranging from 100 to 1100 rpm. Synthetic wastewater was used in all experiments with an organic-matter concentration of 530 +/- 37 mg/L measured as chemical oxygen demand (COD). The reactor achieved an organic-matter removal efficiency of around 87% under all investigated conditions. Analysis of the four impeller types and the investigated stirring frequencies showed that mass transfer in the liquid phase was affected not only by the applied stirring frequency but also by the agitation mode imposed by each impeller type. The best reactor performance at all stirring frequencies was obtained when agitation was provided by the flat-blade turbine impeller. (C) 2010 Elsevier Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An investigation was performed regarding the application of a mechanically stirred anaerobic sequencing batch biofilm reactor containing immobilized biomass on inert polyurethane foam (AnSBBR) to the treatment of soluble metalworking fluids to remove organic matter and produce methane. The effect of increasing organic matter and reactor fill time, as well as shock load, on reactor stability and efficiency have been analyzed. The 5-L AnSBBR was operated at 30 A degrees C in 8-h cycles, agitation of 400 rpm, and treated 2.0 L effluent per cycle. Organic matter was increased by increasing the influent concentration (500, 1,000, 2,000, and 3,000 mg chemical oxygen demand (COD)/L). Fill times investigated were in the batch mode (fill time 10 min) and fed-batch followed by batch (fill time 4 h). In the batch mode, organic matter removal efficiencies were 87%, 86%, and 80% for influent concentrations of 500, 1,000, and 2,000 mgCOD/L (1.50, 3.12, and 6.08 gCOD/L.d), respectively. At 3,000 mgCOD/L (9.38 gCOD/L.d), operational stability could not be achieved. The reactor managed to maintain stability when a shock load twice as high the feed concentration was applied, evidencing the robustness of the reactor to potential concentration variations in the wastewater being treated. Increasing the fill time to 4 h did not improve removal efficiency, which was 72% for 2,000 mgCOD/L. Thus, gradual feeding did not improve organic matter removal. The concentration of methane formed at 6.08 gCOD/L was 5.20 mmolCH(4), which corresponded to 78% of the biogas composition. The behavior of the reactor during batch and fed-batch feeding could be explained by a kinetic model that considers organic matter consumption, production, and consumption of total volatile acids and methane production.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Many lab-scale studies have been carried out regarding the effect of feed strategy on the performance of anaerobic sequencing batch reactors (ASBR); however, more detailed pilot-scale studies should be performed to assess the real applicability of this type of operation. Therefore, the objective of this work was to assess the effect of feed strategy or fill time in a 1-m(3) mechanically stirred pilot-scale sequencing batch reactor, treating 0.65 m(3) sanitary wastewater in 8-h cycles at ambient temperature. Two reactor configurations were used: one containing granular biomass (denominated ASBR) and the other immobilized biomass on polyurethane foam as inert support (denominated anaerobic sequencing batch biofilm reactor (AnSBBR)). The reactors were operated under five distinct feed strategies, namely: typical batch and fed-batch for 25%, 50%, 75%, and 100% of the cycle length. Stirring frequency in the ASBR was 40 rpm with two flat-blade turbine impellers and 80 rpm in the AnSBBR with two helix impellers. The results showed that both the ASBR and AnSBBR when operated under typical batch, fed-batch for 50% and 75% of the cycle length, presented improved organic matter removal efficiencies, without significant differences in performance, thus showing important operational flexibility. In addition, the reactors presented operation stability under all conditions.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The objective of this work was to study the operational feasibility of nitrification and denitrification processes in a mechanically stirred sequencing batch reactor (SBR) operated in batch and fed-batch mode. The reactor was equipped with a draft-tube to improve mass transfer and contained dispersed (aerobic) and granulated (anaerobic) biomass. The following reactor variables were adjusted: aeration time during the nitrification step; dissolved oxygen concentration, feed time defining batch and fed-batch phases, concentration of external carbon source used as electron donor during the denitrification stage and volumetric ammonium nitrogen load in the influent. The reactor (5 L volume) was maintained at 30 +/- 1 degrees C and treated either 1.0 or 1.5 L wastewater in 8-h cycles. Ammonium nitrogen concentrations assessed were: 50 (condition 1) and 100 mgN-NH(4)(+).L(-1) (condition 2), resulting in 29 and 67 mgN-NH(4)(+).L-1-d(-1), respectively. A synthetic medium and ethanol were used as external carbon sources (ECS). Total nitrogen removal efficiencies were 94.4 and 95.9% when the reactor was operated under conditions 1 and 2, respectively. Low nitrite (0.2 and 0.3 mgN-NO(2)(-).L(-1), respectively) and nitrate (0.01 and 0.3 mgN-NO(3)(-).L(-1), respectively) concentrations were detected in the effluent and ammonium nitrogen removal efficiencies were 97.6% and 99.6% under conditions 1 and 2, respectively.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The perfect mixing model (PMM) is based on parameters derived from the equipment characteristics as well as ore breakage characteristics. Ore characteristics are represented through the appearance function. This function may be determined using JKMRC laboratorial methods or by standard functions. This work describes the model fitting process of the Carajas grinding circuit, using the JKSimMet simulator Two scenarios were used in model fitting exercises: 1) standard appearance function; and 2) appearance fund ion based on testing carried out on samples taken at circuit feed. From this assessment, the appearance function`s influence in the PMM,fit and it`s relation with the breakage rate were determined. The influence of the appearance function on the respective breakage rate distribution was assessed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The purpose of this paper was to study the main effects of the turning in the superficial integrity of the duplex stainless steel ASTM A890-6A. The tests were conducted on a turning centre with carbide tools and the main entrances variables were: tool material class, feed rate, cutting depth, cutting speed and cutting fluid utilisation. The answers were analysed: microstructural analysis by optical microscopy and x-ray diffraction, cutting forces measurements by a piezoelectric dynamometer, surface roughness, residual stress by x-ray diffraction technique and the microhardness measurements. The results do not show any changes in the microstructural of the material, even when the greater cutting parameters were used. The smaller feed rate (0.1 mm/v), smaller cutting speed (110 m/min) and the greater cutting depth (0.5 mm) provided the smaller values for the tensile residual stress, the smaller surface roughness and the greater microhardness.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An investigation was conducted on pollutants emitted from steady-state, steady-flow gasification and combustion of polyethylene (PE) in a two-stage furnace. The polymer, in pulverized form, was first pyrolyzed at 1000 degrees C, and subsequently, its gaseous pyrolyzates were burned, upon mixing with air at high temperatures (900-1100 degrees C). The motivation for this indirect type of burning PE was to attain nominally premixed combustion of the pyrolyzate gases with air, thereby achieving lower pollutant emissions than those emanating from the direct burning of the solid PE polymer. This work assessed the effluents of the two-stage furnace and examined the effects of the combustion temperature, as well as the polymer feed rate and the associated fuel/air equivalence ratio (0.3 < phi < 1.4). It was found that, whereas the yield of pyrolysis gas decreased with an increasing polymer feed rate, its composition was nearly independent of the feed rate. CO2 emissions peaked at an equivalence ratio near unity, while the CO emissions increased with an increasing equivalence ratio. The total light volatile hydrocarbon and semivolatile polycyclic aromatic hydrocarbon (PAH) emissions of combustion increased with an increasing equivalence ratio. The generated particulates were mostly submicrometer in size. Overall, PAH and soot emissions from this indirect burning of PE were an order of magnitude lower than corresponding emissions from the direct burning of the solid polymer, obtained previously in this laboratory using identical sampling and analytical techniques. Because pyrolysis of this polymer requires a nominal heat input that amounts to only a diminutive fraction of the heat released during its combustion, implementation of this technique is deemed advantageous.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The influence of Sri in Fe(2)O(3) thin films is addressed. The presence of the tin ions decreases the Fe(2)O(3) particle sizes and surface roughness decreasing of the films` surface is observed as a consequence. X-ray diffraction and atomic force microscopy measurements together with literature results support this phenomenon to be related to the segregation of the additive onto the surface and consequently surface energy decrease, which constitutes the driving force for the microstructure modification, similarly to results previously obtained for powders with same compositions. The effect of the anions introduced in the system as counter-ions of the precursors is also discussed.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Alumina ceramics with high in-line transmittance at 0.5-1.0 mm-thickness were prepared with different doping additives by sintering at 1850 degrees C in vacuum for 1-8 h. Depending on the additive contents and sintering variables bi-dimensionally large surface grains, caused by surface evaporation of MgO, had grown parallel to the surface with similar to 100 mu m thickness and lateral sizes up to the millimeter range. The abnormal grain-growth process also resulted in the formation of pores entrapped inside the large surface grains within a narrow zone at 10-20 mu m distance from the surface. The fraction of these pores is thickness-invariant. Scattering factors associated to the pores entrapped inside the bi-dimensionally large surface grains, second-phase particles, grain-boundaries, and microstructural surface defects are derived from the results of in-line transmission (at 600 nm) and are used together with microstructural characteristics to explain the light transmittance in these materials. (C) 2008 Elsevier Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This work analyses pellets prepared with iron ore that has been mechanically activated by high energy ball milling. Pellet feed iron ore was submitted to high-energy ball milling for 60 minutes, and the resulting material was analysed through measurements of particle size and specific surface area, as well as X-ray diffraction. Pellets were prepared from this material. The pellets were heated at temperatures ranging from 1000 to 1250 degrees C in a muffle furnace, and submitted to the maximum temperature during 10 - 12 minutes. The samples were then tested regarding crushing strength, densification and porosity, and were examined in a scanning electronic microscope. The results were compared to those obtained with similar samples made from non-milled pellet feed. It has been shown that through high-energy ball milling of iron ore it is possible to achieve pellets presenting high densification and compressive strength at firing temperatures lower than the usual ones.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This work presents a mathematical model for the vinyl acetate and n-butyl acrylate emulsion copolymerization process in batch reactors. The model is able to explain the effects of simultaneous changes in emulsifier concentration, initiator concentration, monomer-to-water ratio, and monomer feed composition on monomer conversion, copolymer composition and, to lesser extent, average particle size evolution histories. The main features of the system, such as the increase in the rate of polymerization as temperature, emulsifier, and initiator concentrations increase are correctly represented by the model. The model accounts for the basic features of the process and may be useful for practical applications, despite its simplicity and a reduced number of adjustable parameters.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This work aims to study the adsorption of phenol on activated carbons (ACs) and the consecutive in situ regeneration of carbon by Fenton oxidation. Two different operations have been carried Out: (1) a batch procedure in order to investigate the influence of Fe(2+) and H(2)O(2) concentrations; (2) continuous fixed bed adsorption, followed by a batch circulation of the Fenton`s reagent through the saturated AC bed. to examine the efficiency of the real process. Two different activated carbons have been also studied: a both micro- and mesoporous AC (L27) and an only microporous One (S23). In the batch reactor the best conditions found for pollutant mineralization in the homogeneous Fenton system are not the best For AC regeneration: a continuous reduction of adsorption capacity of L27 is observed after 3 oxidations, due to the decrease of both AC weight and surface area. Higher concentration of Fe(2+) and lower concentration of H(2)O(2) (2 times the stoichiometry) lead to a 50% recovery of the initial adsorption capacity during at least four consecutive cycles for L27, while about 20% or less for S23. In the consecutive continuous adsorption/batch Fenton oxidation process, the regeneration efficiency reaches 30-40% for L27 after two cycles whatever the feed concentration and less than 10% for S23. A photo-Fenton test performed on L27 shows almost complete mineralization (contrary to ""dark"" Fenton) and further improves recovery of AC adsorption capacity although not complete (56% after two cycles).