104 resultados para Neutron scattering and diffraction
Resumo:
Bi(4-x)La(x)Ti(3)O(12) (BLT) ceramics were prepared and studied in this work in terms of La(3+)-modified microstructure and phase development as well as electrical response. According to the results processed from X-ray diffraction and electrical measurements, the solubility limit (XL) of La(3+) into the Bi(4)Ti(3)O(12) (BIT) matrix was here found to locate slightly above x = 1.5. Further, La(3+) had the effect of reducing the material grain size, while changing its morphology from the plate-like form, typical of BIT ceramics, to a spherical-like one. The electrical results presented and discussed here also include the behavior of the temperature of the ferroelectric-paraelectric phase transition as well as the normal or diffuse and/or relaxor nature of this transition depending on the La(3+) content. (c) 2008 Elsevier Ltd. All fights reserved.
Resumo:
[Ba(1-x)Y(2x/3)](Zr(0.25)Ti(0.75))O(3) powders with different yttrium concentrations (x = 0, 0.025 and 0.05) were prepared by solid state reaction. These powders were analyzed by X-ray diffraction (XRD). Fourier transform Raman scattering (FT-RS), Fourier transform infrared (FT-IR) and X-ray absorption near-edge (XANES) spectroscopies. The optical properties were investigated by means of ultraviolet-visible (UV-vis) absorption spectroscopy and photoluminescence (PL) measurements. Even with the addition of yttrium, the XRD patterns revealed that all powders crystallize in a perovskite-type cubic structure. FT-RS and FT-IR spectra indicated that the presence of [YO(6)] clusters is able to change the interaction forces between the O-Ti-O and O-Zr-O bonds. XANES spectra were used to obtain information on the off-center Ti displacements or distortion effects on the [TiO(6)] clusters. The different optical band gap values estimated from UV-vis spectra suggested the existence of intermediary energy levels (shallow or deep holes) within the band gap. The PL measurements carried out with a 350 nm wavelength at room temperature showed that all powders present typical broad band emissions in the blue region. (C) 2010 Elsevier Masson SAS. All rights reserved.
Resumo:
Pure N,N`-di(methoxycarbonylsulfenyl)urea, [CH(3)OC(O)SNH](2)CO, is quantitatively prepared by the hydrolysis reaction of CH(3)OC(O)SNCO and characterized by (1)H NMR, GC-MS and FTIR spectroscopy techniques. Structural and conformational properties are analyzed using a combined approach with data obtained from X-ray diffraction, vibrational spectra and theoretical calculation methods. The IR and Raman spectra for normal and deuterated species are reported. The crystal structure of [CH(3)OC(O)SNH](2)CO was determined by X-ray diffraction methods. The substance crystallizes in the orthorhombic P2(1)2(1)2 space group with a = 9.524(2), b = 12.003(1), c = 4.481 (1) angstrom, and Z = 2 moieties in the unit cell. The molecule is sited on a twofold crystallographic axis (C(2)) parallel to c and shows the anti-anti conformation (S-N single bonds antiperiplanar with respect to the opposite C-N single bonds in sulfenyl-urea-sic group). Neighboring molecules are arranged in a chain motif that extends along the C(2)-axis and is held by bifurcated NH center dot center dot center dot O center dot center dot center dot HN intermolecular bonds. A local planar symmetry is observed in the crystal for the central -SN(H)C(O)N(H)S- skeleton. Experimental and calculated data allow to trace this structural feature to the occurrence of N-H center dot center dot center dot O=C hydrogen bonding interactions. Calculated vibrational and structural properties are in good agreement with the experimentally determined features. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
The local structure of an ion-conducting glass with nominal composition 50B(2)O(3)-10PbO-40LiF has been investigated by complementary (7)Li, (11)B, (19)F, and (207)Pb single- and double-resonance experiments. The results give insight into the structural role of the lithium fluoride additive in borate glasses: (1) LiF is seen to actively participate in the network transformation process contributing to the conversion of three- into four-coordinate boron units, as shown by (11)B single-resonance as well as by (11)B{(19)F} and (19)F{(11)B} double-resonance experiments. (2) (19)F signal quantification experiments suggest substantial fluoride loss, presumably caused by formation of volatile BF(3). A part of the fluoride remains in the dopant role, possibly in the form of small LiF-like cluster domains, which serve as a mobile ion supply. (3) The extent of lithium-fluorine and lead-fluorine interactions has been characterized by (7)Li{(19)F} and (207)Pb{(19)F} REDOR and SEDOR experiments. On the basis of these results, a quantitative structural description of this system has been developed.
Resumo:
The synthesis, structural characterization, voltammetric experiments and antibacterial activity of [Ni(sulfisoxazole)(2)(H2O)(4)] center dot 2H(2)O and [Ni(sulfapyridine)(2)] were studied and compared with similar previously reported copper complexes. [Ni(sulfisoxazole)(2)(H2O)(4)] center dot 2H(2)O crystallized in a monoclinic system, space group C2/c where the nickel ion was in a slightly distorted octahedral environment, coordinated with two sulfisoxazole molecules through the heterocyclic nitrogen and four water molecules. [Ni(sulfapyridine)(2)] crystallized in a orthorhombic crystal system, space group Pnab. The nickel ion was in a distorted octahedral environment, coordinated by two aryl amine N from two sulfonamides acting as monodentate ligands and four N atoms (two sulfonamidic N and two heterocyclic N) from two different sulfonamide molecules acting as bidentate ligands. Differential pulse voltammograms were recorded showing irreversible peaks at 1040 and 1070 mV, respectively, attributed to Ni(II)/Ni(III) process. [Ni(sulfisoxazole)(2)(H2O)(4)] center dot 2H(2)O and [Ni(sulfapyridine)(2)] presented different antibacterial behavior against Staphylococcus aureus and Escherichia coli from the similar copper complexes and they were inactive against Mycobacterium tuberculosis. (c) 2007 Elsevier Inc. All rights reserved.
Resumo:
Structural and conformational properties of 1H-Isoindole-1,3(2H)-dione, 2-[(methoxycarbonyl)thio] (S-phthalimido O-methyl thiocarbonate) are analyzed using a combined approach including X-ray diffraction, vibrational spectra and theoretical calculation methods. The vibrational properties have been studied by infrared and Raman spectroscopies along with quantum chemical calculations (B3LYP and B3PW91 functional in connection with the 6-311++G** and aug-cc-pVDZ basis sets). The crystal structure was determined by X-ray diffraction methods. The substance crystallizes in the monoclinic P2(1)/c space group with a = 6.795(1), b = 5.109(1), c = 30.011(3) angstrom, beta = 90.310(3)degrees and Z = 4 molecules per unit cell. The conformation adopted by the N-S-C=O group is syn (C=O double bond in synperiplanar orientation with respect to the N-S single bond). The experimental molecular structure is well reproduced by the MP2/aug-cc-pVDZ method. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
A new occurrence of rankamaite is here described at the Urubu pegmatite, Itinga municipality, Minas Gerais, Brazil. The mineral forms cream-white botryoidal aggregates of acicular to fibrous crystals, intimately associated with simpsonite, thoreaulite, cassiterite, quartz, elbaite, albite, and muscovite. The average of six chemical analyses obtained by electron microprobe is (range in parentheses, wt%): Na(2)O 2.08 (1.95-2.13), K(2)O 2.61 (2.52-2.74), Al(2)O(3) 1.96 (1.89-2.00), Fe(2)O(3) 0.01 (0.00-0.03), TiO(2) 0.02 (0.00-0.06), Ta(2)O(5) 81.04 (79.12-85.18), Nb(2)O(5) 9.49 (8.58-9.86), total 97.21 (95.95-101.50). The chemical formula derived from this analysis is (Na(1.55)K(1.28))(Sigma 2.83)(Ta(8.45)Nb(1.64)Al(0.89)Fe(0.01)(3+)Ti(0.01))(Sigma 11.00)[O(25.02)(OH)(5.98)](Sigma 31.00). Rankamaite is an orthorhombic ""tungsten bronze"" (OTB), crystallizing in the space group Cmmm. Its unit-cell parameters refined from X-ray diffraction powder data are: a = 17.224(3), b = 17.687(3), c = 3.9361(7) angstrom, V = 1199.1(3) angstrom(3), Z = 2. Rietveld refinement of the powder data was undertaken using the structure of LaTa(5)O(14) as a starting model for the rankamaite structure. The structural formula obtained with the Rietveld analyses is: (Na(2.21)K(1.26))Sigma(3.37)(Ta(9.12)NB(1.30) Al(0.59))(Sigma 11.00)[O(26.29)(OH)(4.71)](Sigma 31.00). The tantalum atoms are coordinated by six and seven oxygen atoms in the form of distorted TaO(6) octahedra and TaO(2) pentagonal bipyramids, respectively. Every pentagonal bipyramid shares edges with four octahedra, thus forming Ta(5)O(14) units. The potassium atom is in an 11-fold coordination, whereas one sodium atom is in a 10-fold and the other is in a 12-fold coordination. Raman and infrared spectroscopy were used to investigate the room-temperature spectra of rankamaite.
Resumo:
This work deals with the structural and vibrational characterization of PANI nanofibers prepared through interfacial polymerization using different concentrations of HCl aqueous solution. The results were compared to those obtained by PANI prepared through the conventional route. X-ray diffraction and small-angle X-ray scattering techniques showed that high concentrations of HCl solutions used in the preparation of the PANI nanofibers reduce their crystallinity. The increase of regions with granular morphology was also observed in the scanning electron microscopy images. The changes in the resonance Raman spectra from 200 to 500 cm(-1), FTIR spectra, and the EPR data of the PANI nanofibers reveal an increase in the torsion angles of C-ring-N-C-ring segments owing the formation of bipolarons in the PANI backbone higher than the PANI samples prepared by conventional route.
Resumo:
Nanocomposites of carbon nanotubes and titanium dioxide (TiO(2)) have attracted much attention due to their photocatalytic properties. Although many examples in the literature have visualized these nanocomposites by electron microscopic images, spectroscopic characterization is still lacking with regard to the interaction between the carbon nanotube and TiO(2). In this work, we show evidence of the attachment of nanostructured TiO(2) to multiwalled carbon nanotubes(MWNTs) by Raman spectroscopy. The nanostructured TiO(2) was characterized by both full-width at half-maximum (FWHM) and the Raman shift of the TiO(2) band at ca 144 cm(-1), whereas the average diameter of the crystallite was estimated as approximately 7 nm. Comparison of the Raman spectra of the MWNTs and MWNTs/TiO(2) shows a clear inversion of the relative intensities of the G and D bands, suggesting a substantial chemical modification of the outermost tubes due to the attachment of nanostructured TiO(2). To complement the nanocomposite characterization, scanning electronic microscopy and X-ray diffraction were performed. Copyright (C) 2011 John Wiley & Sons, Ltd.
Resumo:
Asystematic study on the surface-enhanced Raman scattering (SERS) for 3,6-bi-2-pyridyl-1,2,4,5-tetrazine (bptz) adsorbed onto citrate-modified gold nanoparticles (cit-AuNps) was carried out based on electronic and vibrational spectroscopy and density functional methods. The citrate/bptz exchange was carefully controlled by the stepwise addition of bptz to the cit-AuNps, inducing flocculation and leading to the rise of a characteristic plasmon coupling band in the visible region. Such stepwise procedure led to a uniform decrease of the citrate SERS signals and to the rise of characteristic peaks of bptz, consistent with surface binding via the N heterocyclic atoms. In contrast, single addition of a large amount of bptz promoted complete aggregation of the nanoparticles, leading to a strong enhancement of the SERS signals. In this case, from the distinct Raman profiles involved, the formation of a new SERS environment became apparent, conjugating the influence of the local hot spots and charge-transfer (CT) effects. The most strongly enhanced vibrations belong to a(1) and b(2) representations, and were interpreted in terms of the electromagnetic and the CT mechanisms: the latter involving significant contribution of vibronic coupling in the system. Copyright (C) 2010 John Wiley & Sons, Ltd.
Resumo:
This paper studies the selectivity of Well-defined Au and Ag nanostructures as substrates for the SERS, (surface-enhanced Raman scattering) detection of simazine (6-chloro-N,N`-diethyl-1,3,5-triazine-2,4-diamine) and atrazine (6-chloro-N-ethyl-N`-isopropyl-1,3,5-triazine-2,4-diamine). Our data showed that simazine and atrazine displayed similar SERS spectra when the Au was employed as substrate. Conversely, distinct SERS signatures were obtained upon the utilization of Ag substrates. Density functional theory (DFT) calculations and vibrational assignments suggested that, while simazine and atrazine adsorbed on Au via the N3 position of the triazine ring, simazine adsorbed on Ag via N3 and atrazine via N5. The results presented herein demonstrated that the adsorption geometry of analyte molecules can play a central role over substrate selectivity in SERS, which is particularly important in applications involving ultrasensitive analysis of mixtures containing structurally similar molecules.
Resumo:
Stokes and anti-Stokes SERRS intensity fluctuations were observed from a roughened silver electrode immersed in diluted solutions of Brilliant Green (BG), a behaviour linked to single-molecule events. The distributions of the anti-Stokes to Stokes ratios were obtained and their shape showed a strong dependence on the applied potential.
Resumo:
Lead iodide thin films were fabricated using the spray pyrolysis technique. Milli-Q water and N.N-dimethylformamide were used as solvents under varying deposition conditions. Films as thick as 60 mu m were obtained. The optical and structural properties of the samples were investigated using Photoluminescence, Raman scattering, X-ray diffraction, and Scanning electron microscopy. In addition, the study included also the electronic properties which were investigated by measuring the dark conductivity as a function of temperature. The deposition technique seems to be promising for the development of thick films to be used in medical imaging.
Resumo:
The interaction of emeraldine base (PANI-EB) with silver and gold colloids was probed by using Surface-Enhanced Resonance Raman Scattering (SERRS) at 3 different exciting radiations. Due to the great sensitivity of SERRS technique the detection limit of PANI-EB concentration was ca. 2 x 10(-7) mol L(-1) in Ag and Au colloidal suspensions. The UV-vis-NIR spectra of metal colloids in function of PANI-EB concentrations showed that gold colloids present a higher degree of aggregation than silver colloids. SERRS of PANI-EB on metal colloids allowed the study of the polymeric species formed primarily on the metallic surface. The polymer formed after the adsorption of PANI-EB on metallic nanoparticles is strongly dependent on the nature of the metal colloids. The oxidation of PANI-EB to pernigraniline occurred for silver colloids, while a doping process of PANI-EB on Au nanoparticles was evidenced through the observation of the characteristic SERRS spectrum of emeraldine salt at 1064nm.