276 resultados para dentin permeability


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Acid etching procedures may disrupt residual bacteria and contribute to the success of incomplete caries removal followed by adhesive restoration. This study evaluated the in vivo effect of acid etching on cariogenic bacterial activity within affected dentin after minimally invasive treatment of caries lesions. Twenty-eight carious permanent teeth received standardized selective caries removal and random acid etch treatment (E) or not (NE) prior to adhesive restoration. Baseline and 3-month dentin biopsies were collected. The number of bacteria and activity of total bacterial cells and Streptococcus mutans were determined by quantitative PCR and RT-PCR. No statistically significant differences were observed in total bacterial number and activity between E and NE treatments (p > 0.3008). For NE, however, the residual S. mutans bacterial cells were reduced (p = 0.0027), while the activity per cell was significantly increased (p = 0.0010) after reentry at 3 months after restoration. This effect was not observed in group E. Although no significant differences were found between groups, this study suggests that acid etching of affected dentin prior to adhesive restoration may directly or indirectly have an inhibitive effect on the activity of residual cariogenic bacteria. Further research is required to investigate this potential effect. Copyright (C) 2010 S. Karger AG, Basel

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Introduction: The present study evaluated the effect of a reducing agent on the bond strength of deproteinized root canal dentin surfaces when using a self-adhesive versus dual-cured cement. Regional differences were also evaluated. Methods: A total of 45 bovine incisor roots were divided into 3 groups: irrigation with physiologic solution (control), 10-minute deproteinization with 5% NaOCl, and 10-minute deproteinization with 5% NaOCl followed by 10 minutes of 10% ascorbic acid. Fiber posts were cemented with either RelyX 0100 or RelyX ARC (with SingleBond 2 or Clearfil SE Bond). The push-out bond strength was evaluated after 24 hours of storage. Data were submitted to three-way analyses of variance and Dunnett 13 tests (alpha = 0.05). Results: No differences between cements were observed within the testing conditions, regardless of the adhesive (P < .05). Deproteinization reduced bond strengths. Subsequent treatment with ascorbic acid was capable of reversing bond strength value changes to levels similar to those of controls. Regional radicular differences were also found, where coronal > middle > apical. Conclusions: The reducing agent was capable. of reversing the effect of dentin deproteinization, and RelyX U100 behaved similarly to RelyX ARC. (J Endod 2010;36:130-134)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Introduction: The aim of this study was to evaluate the biofilm dissolution and cleaning ability of different irrigant solutions on intraorally infected dentin. Methods: One hundred twenty bovine dentin specimens were infected intraorally by using a removable orthodontic device. Thirty samples were used for each irrigant solution: 2% chlorhexidine and 1%, 2.5%, and 5.25% sodium hypochlorite (NaOCl). The solutions were used for 5, 15, and 30 minutes and at 2 experimental volumes, 500 mu L and 1 mL. The samples were stained by using acridine orange dye before and after the experiments and evaluated by using a confocal microscope. The percentage of biofilm, isolated cells, and noncolonized dentin was measured by using a grid system. Differences in the reduction or increase of the studied parameters were assessed by using nonparametric methods (P < .05). Results: The higher values of biofilm dissolution and noncolonized dentin were found in the 30-minute NaOCl group and in the 5-minute and 15-minute groups of 5.25% NaOCL. The use of 2% chlorhexidine solution did not improve the biofilm dissolution or increase the cleaning of the dentin in comparison with the NaOCl solutions (P < .05). Conclusions: Two percent chlorhexidine does not dissolve the biofilms. Thirty minutes of NaOCl are necessary to have higher values of biofilm dissolution and to increase the cleaning of the dentin independently of the concentration in comparison with the 5-minute and 15-minute contact times. (J Endod 2011;37:1134-1138)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objective: The aim of this in vitro study was to analyze the effect of glass-ionomer cement as a liner on the dentin/resin adhesive interface of lateral walls of occlusal restorations after thermocycling. Materials and Methods: Occlusal cavities were prepared in 60 human molars, divided into six groups: no liner (1 and 4); glass-ionomer cement (GIC, Ketac Molar Easymix, 3M ESPE) (2 and 5); and resin-modified glass-ionomer cement (RMGIC, Vitrebond, 3M ESPE) (3 and 6). Resin composite (Filtek Z250, 3M ESPE) was placed after application of an adhesive system (Adper Single Bond 2, 3M ESPE) that was mixed with a fluorescent reagent (Rhodamine B) to allow confocal microscopy analysis. Specimens of groups 4, 5 and 6 were thermocycled (5 degrees C-55 degrees C) with a dwell time of 30 seconds for 5000 cycles. After this period, teeth were sectioned in approximately 0.8-mm slices. One slice of each tooth was randomly selected for confocal microscopy analysis. The other slices were sectioned into 0.8 nun x 0.8 mm beams, which were submitted to microtensile testing (MPa). Data were analyzed using two-way ANOVA and Tukey test (p < 0.05). Results: There was no detectedstatistical difference on bond strength among groups (alpha < 0.05). Confocal microscopy analysis showed a higher mean gap size in group 4(12.5 mu m) and a higher percentage of marginal gaps in the thermocycled groups. The RNIGIC liner groups showed the lowest percentage of marginal gaps. Conclusions: Lining with RMGIC resulted in less gap formation at the dentin/resin adhesive interface after artificial aging. RMGIC or GIC liners did not alter the microtensile bond strength of adhesive system/resin composite to dentin on the lateral walls of Class I restorations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The purpose of this study was to explore the potential of confocal laser scanning microscopy (CLSM) for in situ identification of live and dead Enterococcus faecalis in infected dentin. Eight cylindrical dentin specimens were infected with Enterococcus faecalis in BHI for 21 days. After the experimental period, the specimens were stained with fluorescein diacetate (FDA) and propidium iodide (PI) or acridine orange (0.01 %) and analyzed by CLSM. Two noninfected dentin specimens were used as negative controls. CLSM analysis shows that the discrimination between viable (green) and dead (red) bacteria in infected dentinal tubules could be observed after staining with FDA/PI. Acridine orange was able to show metabolic activity of the E. faecalis cells inside the dentinal tubules showed by its red fluorescence. The viability of bacteria in infected dentin can be determined in situ by CLSM. FDA/PI and acricline orange are useful for this technique.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Statement of the Problem: Adhesive systems can spread differently onto a substrate and, consequently, influence bonding. Purpose: The purpose of this study was to evaluate the effect of differently oriented dentin surfaces and the regional variation of specimens on adhesive layer thickness and microtensile bond strength (MTBS). Materials and Methods: Twenty-four molars were sectioned mesiodistally to expose flat buccal and lingual halves. Standardized drop volumes of adhesive systems (Single Bond [SB] and Prime & Bond 2.1 [PB2.1]) were applied to dentin according to the manufacturer`s instructions. Teeth halves were randomly divided into groups: 1A-SB/parallel to gravity; 1B-SB/perpendicular to gravity; 2A-PB2.1/parallel to gravity; and 2B-PB2.1/perpendicular to gravity. The bonded assemblies were stored in 37 degrees C distilled water for 24 hours and then sectioned to obtain dentin sticks (0.8 mm(2)). The adhesive layer thickness was determined in a light microscope (x200), and after 48 hours the specimens were subjected to MTBS test. Data were analyzed by one-way and two-way analysis of variance and Student-Newman-Keuls tests. Results: Mean values (MPa +/- SD) of MTBS were: 39.1 +/- 12.9 (1A); 32.9 +/- 12.4 (1B); 52.9 +/- 15.2 (2A); and 52.3 +/- 16.5 (2B). The adhesive systems` thicknesses (mu m +/- SD) were: 11.2 +/- 2.9 (1A); 18.1 +/- 7.3 (1B); 4.2 +/- 1.8 (2A); and 3.9 +/- 1.3 (2B). No correlation between bond strength and adhesive layer thickness for both SB and PB2.1 (r = -0.224, p = 0.112 and r = 0.099, p = 0.491, respectively) was observed. Conclusions: The differently oriented dentin surfaces and the regional variation of specimens on the adhesive layer thickness are material-dependent. These variables do not influence the adhesive systems` bond strength to dentin. CLINICAL SIGNIFICANCE Adhesive systems have different viscosities and spread differently onto a substrate, influencing the bond strength and also the adhesive layer thickness. Adhesive thickness does not influence dentin bond strength, but it may impair adequate solvent evaporation, polymer conversion, and may also determine water sorption and adhesive degradation over time. In the literature, many studies have shown that the adhesive layer is a permeable membrane and can fail over timebecause ofits continuous plasticizing and degradation when in contact with water. Therefore, avoiding thick adhesive layers may minimize these problems and provide long-term success for adhesive restorations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The progressive degradation of resin-dentin bonds is due, in part, to the slow degradation of collagen fibrils in the hybrid layer by endogenous matrix metalloproteinases (MMPs) of the dentin matrix. In in vitro durability studies, the storage medium composition might be important because the optimum activity of MMPs requires both zinc and calcium. Objective. This study evaluated the effect of different storage media on changes in matrix stiffness, loss of dry weight or solubilization of collagen from demineralized dentin beams incubated in vitro for up to 60 days. Methods. Dentin beams (1 mm x 2 mm x 6 mm) were completely demineralized in 10% phosphoric acid. After baseline measurements of dry mass and elastic modulus (E) (3-point bending, 15% strain) the beams were divided into 5 groups (n = 11/group) and incubated at 37 degrees C in either media containing both zinc and calcium designated as complete medium (CM), calcium-free medium, zinc-free medium, a doubled-zinc medium or water. Beams were retested at 3, 7, 14, 30, and 60 days of incubation. The incubation media was hydrolyzed with HCl for the quantitation of hydroxyproline (HOP) as an index of solubilization of collagen by MMPs. Data were analyzed using repeated measures of ANOVA. Results. Both the storage medium and the storage time showed significant effects on E, mass loss and HOP release (p < 0.05). The incubation in CM resulted in relatively rapid and significant (p < 0.05) decreases in stiffness, and increasing amounts of mass loss. The HOP content of the experimental media also increased with incubation time but was significantly lower (p < 0.05) than in the control CM medium, the recommended storage medium. Conclusions. The storage solutions used to age resin-dentin bonds should be buffered solutions that contain both calcium and zinc. The common use of water as an aging medium may underestimate the hydrolytic activity of endogenous dentin MMPs. (c) 2010 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives. To better comprehend the role of CHX in the preservation of resin-dentin bonds, this study investigated the substantivity of CHX to human dentin. Material and methods. Dentin disks (n = 45) were obtained from the mid-coronal portion of human third molars. One-third of dentin disks were kept mineralized (MD), while the other two-thirds had one of the surfaces partially demineralized with 37% phosphoric acid for 15 s (PDD) or they were totally demineralized with 10% phosphoric acid (TDD). Disks of hydroxyapatite (HA) were also prepared. Specimens were treated with: (1) 10 mu L of distilled water (controls), (2) 10 mu L of 0.2% chlorhexidine diacetate (0.2% CHX) or (3) 10 mu L of 2% chlorhexidine diacetate (2% CHX). Then, they were incubated in 1 mL of PBS (pH 7.4, 37 degrees C). Substantivity was evaluated as a function of the CHX-applied dose after: 0.5 h, 1 h, 3 h, 6 h, 24 h, 168 h (1 week), 672 h (4 weeks) and 1344 h (8 weeks) of incubation. CHX concentration in eluates was spectrophotometrically analyzed at 260 nm. Results. Significant amounts of CHX remained retained in dentin substrates (MD, PPD or TDD), independent on the CHX-applied dose or time of incubation (p < 0.05). High amounts of retained CHX onto HA were observed only for specimens treated with the highest concentration of CHX (2%) (p < 0.05). Conclusion. The outstanding substantivity of CHX to dentin and its reported effect on the inhibition of dentinal proteases may explain why CHX can prolong the durability of resin-dentin bonds. (C) 2010 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives: This in vitro study aimed to analyse the effect of a single application of TiF(4) and NaF varnishes and solutions to protect against dentin erosion. Methods: Bovine root dentin samples were pre-treated with NaF-Duraphat varnish (2.26%F, pH 4.5), NaF/CaF(2)-Duofluorid varnish (5.63%F, pH 8.0), NaF-experimental varnish (2.45%F, pH 4.5), TiF(4)-experimental varnish (2.45%F, pH 1.2), NaF solution (2.26%F, pH 4.5), TiF(4) solution (2.45%F, pH 1.2) and placebo varnish (pH 5.0, no-F varnish control). Controls remained untreated. Ten samples in each group were then subjected to an erosive demineralisation (Sprite Zero, 4x 90 s/day) and remineralisation (artificial saliva, between the erosive cycles) cycling for S days. Dentin loss was measured profilometrically after pretreatment and after 1, 3 and 5 days of de-remineralisation cycling. The data were statistically analysed by two-way ANOVA and Bonferroni`s post hoc test (p < 0.05). Results: After pre-treatment, TiF(4) solution significantly induced surface loss (1.08 +/- 0.53 mu m). Only Duraphat reduced the dentin loss overtime, but it did not significantly differ from placebo varnish (at 3rd and 5th days) and TiF(4) varnish (at 3rd day). Conclusions: Duraphat varnish seems to be the best option to partially reduce dentin erosion. However, the maintenance of the effects of this treatment after successive erosive challenges is limited. (C) 2009 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives: This study examined the retention of solvents within experimental HEMA/solvent primers after two conditions for solvent evaporation: from a free surface or from dentine surface. Methods: Experimental primers were prepared by mixing 35% HEMA with 65% water, methanol, ethanol or acetone (v/v). Aliquots of each primer (50 mu l) were placed on glass wells or they were applied to the surface of acid-etched dentine cubes (2 mm x 2 mm x 2 mm) (n = 5). For both conditions (i.e. from free surface or dentine cubes), change in primers mass due to solvent evaporation was gravimetrically measured for 10 min at 51% RH and 21 degrees C. The rate of solvent evaporation was calculated as a function of loss of primers mass (%) over time. Data were analysed by two-way ANOVA and Student-Newman-Keuls (p < 0.05). Results: There were significant differences between solvent retention(%) and evaporation rate (%/min) depending on the solvent present in the primer and the condition for evaporation (from free surface or dentine cubes) (p < 0.05). For both conditions, the greatest amount of retained solvent was observed for HEMA/water primer. The rate of solvent evaporation for HEMA/acetone primer was almost 2- to 10-times higher than for HEMA/water primer depending whether evaporation occurred, respectively, from a free surface or dentine cubes. The rate of solvent evaporation varied with time, being in general highest at the earliest periods. Conclusions: The rate of solvent evaporation and its retention into HEMA/solvent primers was influenced by the type of the solvent and condition allowed for their evaporation. (C) 2009 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study evaluated the effect of 2% chlorhexidine digluconate (CHX) used as a therapeutic primer on the long-term bond strengths of two etch-and-rinse adhesives to normal (ND) and caries-affected (CAD) dentin. Forty extracted human molars with coronal carious lesions, surrounded by normal dentin, were selected for this study. The flat surfaces of two types of dentin (ND and CAD) were prepared with a water-cooled high-speed diamond disc, then acidetched, rinsed and air-dried. In the control groups, the dentin was re-hydrated with distilled water, blot-dried and bonded with a three-step (Scotchbond Multi-Purpose-MP) or two-step (Single Bond 2-SB) etch-and-rinse adhesive. In the experimental groups, the dentin was rehydrated with 2% CHX (60 seconds), blot-dried and bonded with the same adhesives. Resin composite build-ups were made. The specimens were prepared for microtensile bond testing in accordance with the non-trimming technique, then tested either immediately or after six-months storage in artificial saliva. The data were analyzed by ANOVA/Bonferroni tests (alpha=0.05). CHX did not affect the immediate bond strength to ND or CAD (p>0.05). CHX treatment significantly lowered the loss of bond strength after six months as seen in the control bonds for ND (p<0.05), but it did not alter the bond strength of CAD (p>0.05). The application of NIP on CHX-treated ND or CAD produced bonds that did not change over six months of storage.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Purpose: To verify the influence of cavity access diameter on demineralized dentin removal in the ART approach. Methods: 40 non-carious human premolars were randomly divided into four groups. The occlusal surface was ground flat and the teeth were sectioned mesio-distally. The hemi-sections were reassembled and occlusal access preparations were carried out using ball-shaped diamonds. The resulting size of the occlusal opening was 1.0 mm, 1.4 mm, 1.6 mm and 1.8 mm for Groups A, B, C, and D, respectively. Standardized artificial carious lesions were created and demineralized dentin was excavated. After excavation, the cavities were analyzed using: (a) the tactile method, (b) caries-detection dye to stain demineralized dentin, as proposed by Smales & Fang, and (c) Demineralized Tissue Removal index, as proposed in this study. Statistical analysis was performed using Fisher, Spearman correlation coefficient, kappa, Kruskal-Wallis and Miller tests (P < 0.05). Results: The three methods of evaluation showed no significant difference between Groups A vs. B, and C vs. D, while statistically significant differences were observed between Groups A vs. C, A vs. D, B vs. C and B vs. D. Based on the results of this study, the size of occlusal access significantly affected the efficacy of demineralized tissue removal.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study evaluated the microhardness of superficial and deep dentin irradiated with different erbium:yttrium-aluminum-garnet (Er:YAG) laser energies. Seventy-two molars were bisected and randomly assigned to two groups (superficial dentin or deep dentin) and into six subgroups (160 mJ, 200 mJ, 260 mJ, 300 mJ, 360 mJ, and control). After irradiation, the cavities were longitudinally bisected. Microhardness was measured at six points (20 A mu m, 40 A mu m, 60 A mu m, 80 A mu m, 100 A mu m, and 200 A mu m) under the cavity floor. Data were submitted to analysis of variance (ANOVA) and Fisher`s tests (alpha = 0.05). Superficial dentin presented higher microhardness than deep dentin; energy of 160 mJ resulted in the highest microhardness and 360 mJ the lowest one. Values at all points were different, exhibiting increasing microhardness throughout; superficial dentin microhardness was the highest at 20 A mu m with 160 mJ energy; for deep dentin, microhardness after irradiation at 160 mJ and 200 mJ was similar to that of the control. The lowest energy increased superficial dentin microhardness at the closest extent under the cavity; deep dentin microhardness was not altered by energies of 160 mJ and 200 mJ.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: It remains unclear as to whether or not dental bleaching affects the bond strength of dentin/resin restoration. Purpose: To evaluated the bond strength of adhesive systems to dentin submitted to bleaching with 38% hydrogen peroxide (HP) activated by LED-laser and to assess the adhesive/dentin interfaces by means of SEM. Study design: Sixty fragments of dentin (25 mm(2)) were included and divided into two groups: bleached and unbleached. HP was applied for 20 s and photoactivated for 45 s. Groups were subdivided according to the adhesive systems (n = 10): (1) two-steps conventional system (Adper Single Bond), (2) two-steps self-etching system (Clearfil standard error (SE) Bond), and (3) one-step self-etching system (Prompt L-Pop). The specimens received the Z250 resin and, after 24 h, were submitted to the bond strength test. Additional 30 dentin fragments (n = 5) received the same surface treatments and were prepared for SEM. Data were analyzed by ANOVA and Tukey`s test (alpha = 0.05). Results: There was significant strength reduction in bleached group when compared to unbleached group (P < 0.05). Higher bond strength was observed for Prompt. Single Bond and Clearfil presented the smallest values when used in bleached dentin. SEM analysis of the unbleached specimens revealed long tags and uniform hybrid layer for all adhesives. In bleached dentin, Single Bond provided open tubules and with few tags, Clearfil determined the absence of tags and hybrid layer, and Prompt promoted a regular hybrid layer with some tags. Conclusions: Prompt promoted higher shear bond strength, regardless of the bleaching treatment and allowed the formation of a regular and fine hybrid layer with less deep tags, when compared to Single Bond and Clearfil. Microsc. Res. Tech. 74:244-250, 2011. (C) 2010 Wiley-Liss, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Introduction: The greatest reduction in microhardness of the most superficial layer of dentin of the root canal lumen is desired. The use of chelating agents during biomechanical preparation of root canals removes smear layer, increasing the access of the irrigant into the dentin tubules to allow adequate disinfection, and also reduces dentin microhardness, facilitating the action of endodontic instruments. This study evaluated the effect of different chelating solutions on the microhardness of the most superficial dentin layer from the root canal lumen. Methods: Thirty-five recently extracted single-rooted maxillary central incisors were instrumented, and the roots were longitudinally sectioned in a mesiodistal direction to expose the entire canal extension. The specimens were distributed in seven groups according to the final irrigation: 15% EDTA, 10% citric acid, 5% malic acid, 5% acetic acid, apple vinegar, 10% sodium citrate, and control (no irrigation). A standardized volume of 50 mu L of each chelating solution was used for 5 minutes. Dentin microhardness was measured with a Knoop indenter under a 10-g load and a 15-second dwell time. Data were analyzed statistically by one-way analysis of variance and Tukey-Kramer multiple-comparison test at 5% significance level. Results: EDTA and citric acid had the greatest overall effect, causing a sharp decrease in dentin microhardness without a significant difference (p > .05) from each other. However, both chelators differed significantly from the other solutions (p < .001). Sodium citrate and deionized water were similar to each other (p > .05) and did not affect dentin microhardness. Apple vinegar, acetic acid, and malic acid were similar to each other (p > .05) and presented intermediate results. Conclusion: Except for sodium citrate, all tested chelating solutions reduced microhardness of the most superficial root canal dentin layer. EDTA and citric acid were the most efficient. (J Endod 2011;37:358-362)