63 resultados para Hybrid working machines
Resumo:
Objectives. The objectives of this study were to assess the accuracy of working length determination using 3 electronic apex locators and direct digital radiography and to compare the results with those obtained using the visual method (control measurement). Study design. Twenty extracted human maxillary premolars were selected: 17 two-rooted and 3 single-rooted (total of 37 canals). Working length was measured using electronic apex locators Elements Diagnostic, Root ZX, and Just II. Subsequently, teeth were positioned in the alveolar bone of a dry skull and submitted to direct digital radiography. A variation of +/- 1 mm was considered as acceptable. Results were analyzed using the Wilcoxon and the chi(2) tests. Results. Results presented an accuracy of 94.6% for Elements Diagnostic, 91.9% for Root ZX, 73.0% for Just II, and 64.9% for direct digital radiography when considering the margin of +/- 1 mm in relation to the control measurement. Comparisons with the actual control measurements resulted in accuracy results of 13.51%, 13.51%, 10.10%, and 2.70%, respectively. Conclusions. Root ZX and Elements Diagnostic are more accurate in determining working length when compared with Just II and Schick direct digital radiography. (Oral Surg Oral Med Oral Pathol Oral Radiol Endod 2011;111:e44-e49)
Resumo:
This in vitro study aimed to determine whether the micro-hardness of a composite resin is modified by the light units or by the thickness of the increment. Composite resin disks were divided into 15 groups (n = 5), according to the factors under study: composite resin thickness (0 mm, 1 mm, 2 mm , 3 mm and 4 mm) and light units. The light activation was performed with halogen light (HL) (40 s, 500 mW/cm(2)), argon ion laser (AL) (30 s, 600 mW/cm(2)) or light-emitting diode (LED) (30 s, 400 mW/cm(2)). Vickers micro-hardness tests were performed after 1 week and were carried out on the top surface (0 mm-control) and at different depths of the samples. Analysis of variance (ANOVA) and Tukey tests (P a parts per thousand currency signaEuro parts per thousand 0.05) revealed no statistically significant difference among the light units for the groups of 0 mm and 1 mm thickness. At 2 mm depth, the AL was not statistically different from the HL, but the latter showed higher micro-hardness values than the LED. In groups with 3 mm and 4 mm thickness, the HL also showed higher micro-hardness values than the groups activated by the AL and the LED. Only the HL presented satisfactory polymerization with 3 mm of thickness. With a 4 mm increment no light unit was able to promote satisfactory polymerization.
Resumo:
Purpose: The aim of this in vitro study was to evaluate the microtensile bond strength (mu TBS) and hybrid layer morphology of different adhesive systems, either followed by treatment with Nd:YAG laser irradiation or not. Previous studies have shown the effects of Nd:YAG laser irradiation on the dentin surface at restoration margins, but there are few reports about the significance of the irradiation on the hybrid layer. Materials and Methods: The flattened coronal and root dentin samples of 24 bovine teeth were randomly divided into 8 groups, according to the adhesive system used - Scotchbond Multi Purpose (SBMP) or Clearfil SE Bond (CSEB) - and were either irradiated with Nd:YAG or not, with different parameters: 0.8 W/10 Hz, 0.8 W/20 Hz, 1.2 W/10 Hz, 1.2 W/20 Hz. The left sides of specimens were the control groups, and right sides were irradiated. A composite crown was built over bonded surfaces and stored in water (24 h at 37 degrees C). Specimens were sectioned vertically into slabs that were subjected to mu TBS testing and observed by SEM. Results: Control groups (27.81 +/- 1.38) showed statistically higher values than lased groups (21.37 +/- 0.99), and CSEB control group values (31.26 +/- 15.71) were statistically higher than those of SBMP (24.3 +/- 10.66). There were no significant differences between CSEB (20.34 +/- 10.01) and SBMP (22.43 +/- 9.82) lased groups. Among parameters tested, 0.8 W/10 Hz showed the highest value (25.54 +/- 11.74). Nd:YAG laser irradiation caused dentin to melt under the adhesive layer of both adhesive systems tested. Conclusion: With the parameters used in this study, Nd:YAG laser irradiation of the hybrid layer promoted morphological changes in dentin and negatively influenced the bond strength of both adhesive systems.