303 resultados para ETHENE POLYMERIZATION ACTIVITY
Resumo:
The purpose of this study was to evaluate the effect of diode laser (GaAlAs - 780 nm) on pain to palpation and electromyographic (EMG) activity of the masseter and anterior temporalis muscles. The laser was applied on the temporalis and masseter muscles twice a week (four weeks). Forty-eight (48) patients with myofascial pain were randomly assigned between actual and placebo treatments and between the energetic doses of 25 J/cm(2) and 60 J/cm(2), and were evaluated using VAS before, immediately after the final application, and 30 days after the laser treatment. Surface electromyography was performed with maximum dental clenching before and after laser therapy. The results show there were no significant statistical differences in the EMG activity between the groups before and after laser treatment. With regard to the pain at palpation, although both groups presented a significant difference in the symptoms before and after the treatment, only the active doses showed statistically significant reductions in pain level in all the regions of the palpated muscles. However, there was no significant statistical difference between groups (experimental and placebo). In conclusion, low level laser did not promote any changes in EMG activity. The treatment did, however, lessen the pain symptoms in the experimental groups.
Resumo:
The research diagnostic criteria for temporomandibular disorders (RDC/TMD) are used for the classification of patients with temporomandibular disorders (TMD). Surface electromyography of the right and left masseter and temporalis muscles was performed during Maximum teeth clenching in 103 TMD patients subdivided according to the RDC/TMD into 3 non-overlapping groups: (a) 25 myogenous; (b) 61 arthrogenous; and (c) 17 psycogenous patients. Thirty-two control subjects matched for sex and age were also measured. During clenching, standardized total muscle activities (electromyographic potentials over time) significantly differed: 131.7 mu V/mu V s % in the normal subjects, 117.6 mu V/mu V s % in the myogenous patients, 105.3 mu V/mu V s % in the arthrogenous patients, 88.7 mu V/mu V s % in the psycogenous patients (p < 0.001, analysis of covariance). Symmetry in the temporalis muscles was larger in normal subjects (86.3%) and in myogenous patients (84.9%) than in arthrogenous (82.7%), and psycogenous patients (80.5%) (p=0.041). No differences were found for masseter muscle symmetry and torque coefficient (p>0.05). Surface electromyography of the masticatory muscles allowed an objective discrimination among different RDC/TMD subgroups. This evaluation could assist conventional clinical assessments. (C) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Purpose: This study evaluated the effect of different microwave polymerization cycles on the color changes of a microwave-processed denture base resin after accelerated aging and immersion in beverages. Materials and Methods: Specimens of light pink acrylic resin were divided into three groups according to polymerization cycle: (A) 500 W for 3 minutes, (B) 90 W for 13 minutes + 500 W for 90 seconds, and (C) 320 W for 3 minutes + 0 W for 4 minutes + 720 W for 3 minutes. Control groups were a heat-processed acrylic resin (T) and a chemically activated denture repair resin (Q). Eight specimens per group were aged in an artificial aging chamber and evaluated at 20, 192, and 384 hours. Another series of 40 specimens per group were immersed in water, coffee, tea, cola, or red wine and evaluated at 1, 12, and 36 days. Color was measured by a spectrophotometer before and after aging or immersion. Color changes (Delta E) were analyzed by ANOVA/Bonferroni t-test (alpha = 0.05). Results: Mean Delta E (+/- SD) after 384 hours of accelerated aging were (A) 2.51 +/- 0.50; (B) 3.16 +/- 1.09; (C) 2.89 +/- 1.06; (T) 2.64 +/- 0.34; and (Q) 9.03 +/- 0.40. Group Q had a significantly higher Delta E than the other groups. Color changes of immersed specimens were significantly influenced by solutions and time, but the five groups showed similar values. Mean Delta E at 36 days were (water) 1.4 +/- 0.8; (coffee) 1.3 +/- 0.6; (tea) 1.7 +/- 0.5; (cola) 1.4 +/- 0.7; and (red wine) 10.2 +/- 2.7. Results were similar among the five test groups. Conclusions: Color changes of the microwave-polymerized denture base resin tested were not affected by different polymerization cycles after accelerated aging or immersion in beverages. These changes were similar to the conventional heat-polymerized acrylic resin test, but lower than the repair resin after accelerated aging.