Resumo:
The thermoluminescence (TL) response of Dy and Li doped 20CaB(4)O(7)-80CaB(2)O(4) (Wt%) glass-ceramic irradiated with ultraviolet (UV) radiation was studied. In order to act as TL activator ions, the Dy and Li ions were included in the matrix during the melting process to increase its TL efficiency. A single crystalline CaB2O4 phase was present in the glass-ceramic as determined by X-ray diffraction (XRD). The glass-ceramic 20CaB(4)O(7)-80CaB(2)O(4):Dy,Li wt% (named 20CBO7:Dy,Li) is a newly prepared TL material. Its thermoluminescent dosimetric characteristics have shown a linear response under UV radiation exposure and a good TL signal reproducibility, thus proving to be a promising material for using as an ultraviolet radiation dosimeter. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Perovskite-structured Ba(0.90)Ca(0.10)(Ti(1-x)Zr(x))O(3) ceramics were prepared in this work and subsequently studied in terms of composition-dependent dielectric and high-resolution long-range order structural properties from 30 to 450 K. The dielectric response of these materials was measured at several frequencies in the range from 1 kHz to 1 MHz. Combining both techniques, including Rietveld refinement of the X-ray diffraction data, allowed observing that, when increasing Zr(4+) content, the materials change from conventional to diffuse and relaxor ferroelectric compounds, the transition occurring spontaneously at the x = 0.18 composition. Interestingly, this spontaneous transition turned out to be prevented for a further increase of Zr(4+). On the basis of all the dielectric and structural results processed, a phase diagram of this system is presented. (C) 2010 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim
Resumo:
Confined water, such as those molecules in nanolayers of 2-3 nm in length, plays an important role in the adhesion of hydrophilic materials, mainly in cementitious ones. In this study, the effects of water containing kosmotropic substances on adhesion, known for their ability of enhancing the hydrogen bond (H-bond) network of confined water, were evaluated using mechanical strength tests. Indeed, to link adhesion provided by water confined in nanolayers to a macro-response of the cementitious samples, such as the bending strength, requires the evaluation of local water H-bond network configuration in the presence of kosmotropes, considering their influences on the extent and the strength of H-bonds. Among the kosmotropes, trimethylamine and sucrose provided a 50% increase in bending strength compared to the reference samples, the latter just using water as an adhesive, whereas trehalose was responsible for reducing the bending strength to a value close to the samples without any adhesive. The results attained opened up perspectives regarding exploring the confined water behavior which naturally occurs throughout the hydration process in cement-based materials.
Resumo:
This paper presents the results of a new investigation of the Guarani Aquifer System (SAG) in Sao Paulo state. New data were acquired about sedimentary framework, flow pattern, and hydrogeochemistry. The flow direction in the north of the state is towards the southwest and not towards the west as expected previously. This is linked to the absence of SAG outcrop in the northeast of Sao Paulo state. Both the underlying Piramboia Formation and the overlying Botucatu Formation possess high porosity (18.9% and 19.5%, respectively), which was not modified significantly by diagenetic changes. Investigation of sediments confirmed a zone of chalcedony cement close to the SAG outcrop and a zone of calcite cement in the deep confined zone. The main events in the SAG post-sedimentary history were: (1) adhesion of ferrugineous coatings on grains, (2) infiltration of clays in eodiagenetic stage, (3) regeneration of coatings with formation of smectites, (4) authigenic overgrowth of quartz and K-feldspar in advanced eodiagenetic stage, (5) bitumen cementation of Piramboia Formation in mesodiagenetic stage, (6) cementation by calcite in mesodiagenetic and telodiagenetic stages in Piramboia Formation, (7) formation of secondary porosity by dissolution of unstable minerals after appearance of hydraulic gradient and penetration of the meteoric water caused by the uplift of the Serra do Mar coastal range in the Late Cretaceous, (8) authigenesis of kaolinite and amorphous silica in unconfined zone of the SAG and cation exchange coupled with the dissolution of calcite at the transition between unconfined and confined zone, and (9) authigenesis of analcime in the confined SAG zone. The last two processes are still under operation. The deep zone of the SAG comprises an alkaline pH, Na-HCO(3) groundwater type with old water and enriched delta(13)C values (<-3.9), which evolved from a neutral pH, Ca-HCO(3) groundwater type with young water and depleted delta(13)C values (>-18.8) close to the SAG outcrop. This is consistent with a conceptual geochemical model of the SAG, suggesting dissolution of calcite driven by cation exchange, which occurs at a relatively narrow front recently moving downgradient at much slower rate compared to groundwater flow. More depleted values of delta(18)O in the deep confined zone close to the Parana River compared to values of relative recent recharged water indicate recharge occur during a period of cold climate. The SAG is a ""storage-dominated"" type of aquifer which has to be managed properly to avoid its overexploitation. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
The Patino Formation sandstones, which crop out in Aregua neighborhood in Eastern Paraguay and show columnar joints near the contact zone with a nephelinite dyke, have as their main characteristics the high proportion of syntaxial quartz overgrowth and a porosity originated from different processes, initially by dissolution and later by partial filling and fracturing. Features like the presence of floating grains in the syntaxial cement, the transitional interpenetrative contact between the silica-rich cement and grains as well as the intense fracture porosity are strong indications that the cement has been formed by dissolution and reprecipitation of quartz from the framework under the effect of thermal expansion followed by rapid contraction. The increase of the silica-rich cement towards the dyke in association with the orthogonal disposition of the columns relative to dyke walls are indicative that the igneous body may represent the main heat source for the interstitial aqueous solutions previously existing in the sediments. At macroscopic scale, the increasing of internal tensions in the sandstones is responsible for the nucleation of polygons, leading to the individualization of prisms, which are interconnected by a system of joints, formed firstly on isotherm surfaces of low temperature and later on successive adjacent planes towards the dyke heat source.
Resumo:
The coastal plains of the States of Parana and Santa Catarina, in Southern Brazil, were first settled around 6000 B.P. by shellmound builders, a successful fisher-hunter-gatherer population that inhabited the coastal lowlands practically unchanged for almost five thousand years. Shellmounds were typically occupied as residential sites as well as cemeteries, and are usually associated with rich alimentary zones. Around 1200 B.P., the first evidence of ceramics brought from the interior is found in coastal areas, and together with ceramics there is a progressive abandonment of shellmound construction in favor of flat cold shallow sites. Here we consider if these changes were reflected in the postmarital residence practice of coastal groups, i.e., if the arrival or intensification of contact with groups from the interior resulted in changes in this aspect of social structure among the coastal groups. To test the postmarital residence practice we analyzed within-group variability ratios between males and females, following previous studies on the topic. and between-group, correlations between Mahalanobis distances and geographic distances. The results suggest that in the pre-ceramic series a matrilocal, postmarital residential system predominated, while in the ceramic period there was a shift toward patrilocality. This favors the hypothesis that the changes experienced by coastal groups after 1200 B.P. affected not only their economy and material culture, but important aspects of their sociopolitical organization as well.
Resumo:
Near Guarau Ceramic, localized southwest of Salto city in the State of Sao Paulo, two granite outcrops, distant some tens of meters from each other, display Neopaleozoic striated surfaces. These surfaces are in contact with diamictites from the Itarare Subgroup. The striae correspond to sub parallel grooves with millimetric spacing and depth, oriented about N48E and dipping 12 degrees to 42 degrees towards SE. Observed features and association with diamictites indicate an origin by glacial abrasion due to ice movement from southeast towards northwest. About 1.8 km east of Salto, unconsolidated material containing flat-iron-shaped and striated clasts was found on top of granite outcrops, interpreted as clasts pavement remains.
Resumo:
This paper reports a method for the direct and simultaneous determination of Cr and Mn in alumina by slurry sampling graphite furnace atomic absorption spectrometry (SiS-SIMAAS) using niobium carbide (NbC) as a graphite platform modifier and sodium fluoride (NaF) as a matrix modifier. 350 mu g of Nb were thermally deposited on the platform surface allowing the formation of NbC (mp 3500 degrees C) to minimize the reaction between aluminium and carbon of the pyrolytic platform, improving the graphite tube lifetime up to 150 heating cycles. A solution of 0.2 mol L(-1) NaF was used as matrix modifier for alumina dissolution as cryolite-based melt, allowing volatilization during pyrolysis step. Masses (c.a. 50 mg) of sample were suspended in 30 ml of 2.0% (v/v) of HNO(3). Slurry was manually homogenized before sampling. Aliquots of 20 mu l of analytical solutions and slurry samples were co-injected into the graphite tube with 20 mu l of the matrix modifier. In the best conditions of the heating program, pyrolysis and atomization temperatures were 1300 degrees C and 2400 degrees C, respectively. A step of 1000 degrees C was optimized allowing the alumina dissolution to form cryolite. The accuracy of the proposed method has been evaluated by the analysis of standard reference materials. The found concentrations presented no statistical differences compared to the certified values at 95% of the confidence level. Limits of detection were 66 ng g(-1) for Cr and 102 ng g(-1) for Mn and the characteristic masses were 10 and 13 pg for Cr and Mn, respectively.
Resumo:
In this present work a method for the determination of Ca, Fe, Ga, Na, Si and Zn in alumina (Al(2)O(3)) by inductively coupled plasma optical emission spectrometry (ICP OES) with axial viewing is presented. Preliminary studies revealed intense aluminum spectral interference over the majority of elements and reaction between aluminum and quartz to form aluminosilicate, reducing drastically the lifetime of the torch. To overcome these problems alumina samples (250 mg) were dissolved with 5 mL HCl + 1.5 mLH(2)SO(4) + 1.5 mL H(2)O in a microwave oven. After complete dissolution the volume was completed to 20 mL and aluminum was precipitated as Al(OH)(3) with NH(3) (by bubbling NH(3) into the solution up to a pH similar to 8, for 10 min). The use of internal standards (Fe/Be, Ga/Dy, Zn/In and Na/Sc) was essential to obtain precise and accurate results. The reliability of the proposed method was checked by analysis of alumina certified reference material (Alumina Reduction Grade-699, NIST). The found concentrations (0.037%w(-1) CaO, 0.013% w w(-1) Fe(2)O(3), 0.012%w w(-1)Ga(2)O(3), 0.49% w w(-1) Na(2)O, 0.014% w w(-1) SiO(2) and 0.013% w w(-1) ZnO) presented no statistical differences compared to the certified values at a 95% confidence level. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Hybrid photocatalysts based on an adsorbent SiMgOx and a photocatalyst TiO(2) were developed in a plate shape. The ceramic surface was coated with TiO(2) by the slip-casting technique. The effect of the support in the photocatalytic degradation of trichloroethylene (TCE) was analyzed by modifying TiO(2) loading and the layer thickness. Photocatalysts were characterised by N(2) adsorption-desorption, mercury intrusion porosimetry, SEM, UV-vis spectroscopy and XRD. A direct relationship between the TiO(2) content and the photocatalytic activity was observed up to three layers of TiO(2) (0.66 wt.%). Our results indicate that intermediate species generated on the TiO(2) layer can migrate through relatively long distances to react with the OH(-) surface groups of the support. By increasing the TiO(2) loading of the photocatalyst two effects were observed: trichloroethylene conversion is enhanced, while the efficiency of the oxidation process is decreased at expenses of increasing the selectivity to COCl(2) and dichloroacetylchloride (DCAC). The results are discussed in terms of the layer thickness, TiO(2) amount, TCE conversion and CO(2), and COCl(2) selectivity. (C) 2009 Elsevier B.V. All rights reserved.