46 resultados para Maximum Modulus


Relevância:

30.00% 30.00%

Publicador:

Resumo:

Refractory castables are composed of fractions of fine to fairly coarse particles. The fine fraction is constituted primarily of raw materials and calcium aluminate cement, which becomes hydrated, forming chemical bonds that stiffen the concrete during the curing process. The present study focused on an evaluation of several characteristics of two refractory castables with similar chemical compositions but containing aggregates of different sizes. The features evaluated were the maximum load, the fracture energy, and the ""relative crack-propagation work"" of the two castables heat-treated at 110, 650, 1100 and 1550 degrees C. The results enabled us to draw the following conclusions: the heat treatment temperature exerts a significant influence on the matrix/aggregate interaction, different microstructures form in the castables with temperature, and a relationship was noted between the maximum load and the fracture energy. (C) 2009 Elsevier Ltd and Techna Group S.r.l. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Although the Hertz theory is not applicable in the analysis of the indentation of elastic-plastic materials, it is common practice to incorporate the concept of indenter/specimen combined modulus to consider indenter deformation. The appropriateness was assessed of the use of reduced modulus to incorporate the effect of indenter deformation in the analysis of the indentation with spherical indenters. The analysis based on finite element simulations considered four values of the ratio of the indented material elastic modulus to that of the diamond indenter, E/E(i) (0, 0.04, 0.19, 0.39), four values of the ratio of the elastic reduced modulus to the initial yield strength, E(r)/Y (0, 10, 20, 100), and two values of the ratio of the indenter radius to maximum total displacement, R/delta(max) (3, 10). Indenter deformation effects are better accounted for by the reduced modulus if the indented material behaves entirely elastically. In this case, identical load-displacement (P - delta) curves are obtained with rigid and elastic spherical indenters for the same elastic reduced modulus. Changes in the ratio E/E(i), from 0 to 0.39, resulted in variations lower than 5% for the load dimensionless functions, lower than 3% in the contact area, A(c), and lower than 5% in the ratio H/E(r). However, deformations of the elastic indenter made the actual radius of contact change, even in the indentation of elastic materials. Even though the load dimensionless functions showed only a little increase with the ratio E/E(i), the hardening coefficient and the yield strength could be slightly overestimated when algorithms based on rigid indenters are used. For the unloading curves, the ratio delta(e)/delta(max), where delta(e) is the point corresponding to zero load of a straight line with slope S from the point (P(max), delta(max)), varied less than 5% with the ratio E/E(i). Similarly, the relationship between reduced modulus and the unloading indentation curve, expressed by Sneddon`s equation, did not reveal the necessity of correction with the ratio E/E(i). The most affected parameter in the indentation curve, as a consequence of the indentation deformation, was the ratio between the residual indentation depth after complete unloading and the maximum indenter displacement, delta(r)/delta(max) (up to 26%), but this variation did not significantly decrease the capability to estimate hardness and elastic modulus based on the ratio of the residual indentation depth to maximum indentation depth, h(r)/h(max). In general, the results confirm the convenience of the use of the reduced modulus in the spherical instrumented indentation tests.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Objective. To compare currently available low-shrinkage composites with others regarding polymerization stress, volumetric shrinkage (total and post-gel), shrinkage rate and elastic modulus. Methods. Seven BisGMA-based composites (Durafill/DU, Filtek Z250/FZ, Heliomolar/HM, Aelite LS Posterior/AP, Point 4/P4, Filtek Supreme/SU, ELS/EL), a silorane-based (Filtek LS, LS), a urethane-based (Venus Diamond, VD) and one based on a dimethacrylate-derivative of dimer acid (N`Durance, ND) were tested. Polymerization stress was determined in 1-mm high specimens inserted between two PMMA rods attached to a universal testing machine. Total volumetric shrinkage was measured using a mercury dilatometer. Maximum shrinkage rate was used as a parameter of the reaction speed. Post-gel shrinkage was measured using strain-gages. Elastic modulus was obtained by three-point bending. Data were submitted to one-way ANOVA/Tukey test (p = 0.05), except for elastic modulus (Kruskal-Wallis). Results. Composites ranked differently for total and post-gel shrinkage. Among the materials considered as ""low-shrinkage"" by the respective manufacturers, LS, EL and VD presented low post-gel shrinkage, while AP and ND presented relatively high values. Polymerization stress showed a strong correlation with post-gel shrinkage except for LS, which presented high stress. Elastic modulus and shrinkage rate showed weak relationships with polymerization stress. Significance. Not all low-shrinkage composites demonstrated reduced polymerization shrinkage. Also, in order to effectively reduce polymerization stress, a low post-gel shrinkage must be associated to a relatively low elastic modulus. (C) 2010 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The definition of an optimal elastic modulus for a post is controversial. This work hypothesized that the influence of the posts` elastic modulus on dentin stress concentration is dependent on the load direction. The objective was to evaluate, using finite element analysis, the maximum principal stress (sigma(max)) on the root, using posts with different elastic modulus submitted to different loading directions. Nine 3D models were built, representing the dentin root, gutta-percha, a conical post and the cortical bone. The softwares used were: MSC.PATRAN2005r2 (preprocessing) and MSC.Marc2005r2 (processing). Load of 100 N was applied, varying the directions (0 degrees, 45 degrees and 90 degrees) in relation to the post`s long axis. The magnitude and direction of the sigma(max) were recorded. At the 45 degrees and 90 degrees loading, the highest values of sigma(max) were recorded for the lowest modulus posts, on the cervical region, with a direction that suggests debonding of the post. For the 0 degrees loading, the highest values of sigma(max) were recorded for higher modulus posts, on the apical region, and the circumferential direction suggests vertical root fracture. The hypothesis was accepted: the effect of the elastic modulus on the magnitude and direction of the sigma(max) generated on the root was dependent on the loading direction.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

OBJECTIVE: The aim of the present study was to determine the in vitro maximum inhibitory dilution (MID) of two chlorhexidinebased oral mouthwashes (CHX): Noplak®, Periogard®, and one polyhexamethylene biguanide-based mouthwash (PHMB): Sanifill Premium® against 28 field Staphylococcus aureus strains using the agar dilution method. MATERIALS AND METHODS: For each product, decimal dilutions ranging from 1/10 to 1/655,360 were prepared in distilled water and added to Mueller Hinton Agar culture medium. After homogenization, the culture medium was poured onto Petri dishes. Strains were inoculated using a Steers multipoint inoculator and dishes were incubated at 37ºC for 24hours. For reading, MID was considered as the maximum dilution of the mouthwash still capable of inhibiting microbial growth. RESULTS: Sanifill Premium® inhibited the growth of all strains at 1/40 dilution and of 1 strain at 1/80 dilution. Noplak® inhibited the growth of 23 strains at 1/640 dilution and of all 28 strains at 1/320 dilution. Periogard® showed inhibited growth of 7 strains at 1/640 dilution and of all 28 strains at 1/320 dilution. Data were submitted to Kruskal-Wallis statistical test, showing significant differences between the mouthwashes evaluated (p<0.05). No significant difference was found between Noplak® and Periogard® (p>0.05). Sanifill Premium® was the least effective (p<0.05). CONCLUSION: It was concluded that CHX-based mouthwashes present better antimicrobial activity against S. Aureus than the PHMB-based mouthwash.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this in vitro study was to determine the maximum inhibitory dilution (MID) of four cetylpyridinium chloride (CPC)-based mouthwashes: CPC+Propolis, CPC+Malva, CPC+Eucaliptol+Juá+Romã+Propolis (Natural Honey®) and CPC (Cepacol®), against 28 Staphylococcus aureus field strains, using the agar dilution method. Decimal dilutions ranging from 1/10 to 1/655,360 were prepared and added to Mueller Hinton Agar. Strains were inoculated using Steers multipoint inoculator. The inocula were seeded onto the surface of the culture medium in Petri dishes containing different dilutions of the mouthwashes. The dishes were incubated at 37ºC for 24 h. For readings, the MID was considered as the maximum dilution of mouthwash still capable of inhibiting microbial growth. The obtained data showed that CPC+Propolis had antimicrobial activity against 27 strains at 1/320 dilution and against all 28 strains at 1/160 dilution, CPC+Malva inhibited the growth of all 28 strains at 1/320 dilution, CPC+Eucaliptol+Juá+Romã+Propolis inhibited the growth of 2 strains at 1/640 dilution and all 28 strains at 1/320 dilution, and Cepacol® showed antimicrobial activity against 3 strains at 1/320 dilution and against all 28 strains at 1/160 dilution. Data were submitted to Kruskal-Wallis test, showing that the MID of Cepacol® was lower than that determined for the other products (p<0.05). In conclusion, CPC-mouthwashes showed antimicrobial activity against S. aureus and the addition of other substances to CPC improved its antimicrobial effect.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this study was to evaluate the following acrylic resins: Clássico®, QC-20® and Lucitone®, recommended specifically for thermal polymerization, and Acron MC® and VIPI-WAVE®, made for polymerization by microwave energy. The resins were evaluated regarding their surface nanohardness and modulus of elasticity, while varying the polymerization time recommended by the manufacturer. They were also compared as to the presence of water absorbed by the samples. The technique used was nanoindentation, using the Nano Indenter XP®, MTS. According to an intra-group analysis, when using the polymerization time recommended by the manufacturer, a variation of 0.14 to 0.23 GPa for nanohardness and 2.61 to 3.73 GPa for modulus of elasticity was observed for the thermally polymerized resins. The variation for the resins made for polymerization by microwave energy was 0.15 to 0.22 GPa for nanohardness and 2.94 to 3.73 GPa for modulus of elasticity. The conclusion was that the Classico® resin presented higher nanohardness and higher modulus of elasticity values when compared to those of the same group, while Acron MC® presented the highest values for the same characteristics when compared to those of the same group. The water absorption evaluation showed that all the thermal polymerization resins, except for Lucitone®, presented significant nanohardness differences when submitted to dehydration or rehydration, while only Acron MC® presented no significant differences when submitted to a double polymerization time. Regarding the modulus of elasticity, it was observed that all the tested materials and products, except for Lucitone®, showed a significant increase in modulus of elasticity when submitted to a lack of hydration.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

O objetivo deste experimento foi avaliar o efeito da adição de doses crescentes de P2O5 sobre a altura do dossel, o número de perfilhos e a produção de matéria seca de folhas e de colmos do capim-Mombaça, em diferentes idades. Foi conduzido um experimento implantado em um Nitossolo Vermelho Eutrófico. O delineamento experimental usado foi o de blocos completos casualizados, com quatro repetições, cinco doses de P2O5 (30, 60, 90, 120 e 150kg ha-1) e uma testemunha. Para a primeira e segunda coletas, observou-se o efeito linear do fósforo sobre o perfilhamento. Para a terceira e quarta coletas, os dados ajustaram-se ao modelo quadrático. A participação das lâminas foliares na matéria seca da parte aérea diminuiu com as doses de P2O5. Por outro lado, a participação de colmos aumentou com as doses de P2O5. A produção de matéria seca (MS) da parte aérea para primeira, segunda e terceira coletas respondeu de forma linear à aplicação de P2O5 observando-se um aumento estimado de 7, 15 e 19kg ha-1 de MS por kg ha-1 de P2O5, respectivamente. Para a quarta coleta, os dados ajustaram-se ao modelo quadrático de regressão, sendo a máxima produção, 8,3Mg ha-1 de MS, obtida com a aplicação de 103kg ha-1 de P2O5.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Plasma edge turbulence in Tokamak Chauffage Alfven Bresilien (TCABR) [R. M. O. Galvao et al., Plasma Phys. Contr. Fusion 43, 1181 (2001)] is investigated for multifractal properties of the fluctuating floating electrostatic potential measured by Langmuir probes. The multifractality in this signal is characterized by the full multifractal spectra determined by applying the wavelet transform modulus maxima. In this work, the dependence of the multifractal spectrum with the radial position is presented. The multifractality degree inside the plasma increases with the radial position reaching a maximum near the plasma edge and becoming almost constant in the scrape-off layer. Comparisons between these results with those obtained for random test time series with the same Hurst exponents and data length statistically confirm the reported multifractal behavior. Moreover, the persistence of these signals, characterized by their Hurst exponent, present radial profile similar to the deterministic component estimated from analysis based on dynamical recurrences. (C) 2008 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work, the effects of indenter tip roundness oil the load-depth indentation curves were analyzed using finite element modeling. The tip roundness level was Studied based on the ratio between tip radius and maximum penetration depth (R/h(max)), which varied from 0.02 to 1. The proportional Curvature constant (C), the exponent of depth during loading (alpha), the initial unloading slope (S), the correction factor (beta), the level of piling-up or sinking-in (h(c)/h(max)), and the ratio h(max)/h(f) are shown to be strongly influenced by the ratio R/h(max). The hardness (H) was found to be independent of R/h(max) in the range studied. The Oliver and Pharr method was successful in following the variation of h(c)/h(max) with the ratio R/h(max) through the variation of S with the ratio R/h(max). However, this work confirmed the differences between the hardness values calculated using the Oliver-Pharr method and those obtained directly from finite element calculations; differences which derive from the error in area calculation that Occurs when given combinations of indented material properties are present. The ratio of plastic work to total work (W(p)/W(t)) was found to be independent of the ratio R/h(max), which demonstrates that the methods for the Calculation of mechanical properties based on the *indentation energy are potentially not Susceptible to errors caused by tip roundness.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Currently, the acoustic and nanoindentation techniques are two of the most used techniques for material elastic modulus measurement. In this article fundamental principles and limitations of both techniques are shown and discussed. Last advances in nanoindentation technique are also reviewed. An experimental study in ceramic, metallic, composite and single crystals was also done. Results shown that ultrasonic technique is capable to provide results in agreement with those reported in literature. However, ultrasonic technique does not allow measuring the elastic modulus of some small samples and single crystals. On the other hand, the nanoindentation technique estimates the elastic modulus values in reasonable agreement with those measured by acoustic methods, particularly in amorphous materials, while in some policristaline materials some deviation from expected values was obtained.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The objective of the present study was to evaluate herbage accumulation, morphological composition, growth rate and structural characteristics in Mombasa grass swards subject to different cutting intervals (3, 5 and 7 wk) during the rainy and dry seasons of the year. Treatments were assigned to experimental units (17.5 m(2)) according to a complete randomised block design, with four replicates. Herbage accumulation was greater in the rainy than in the dry season (83 and 17%, respectively). Herbage accumulation (24,300 kg DM ha(-1)), average growth rate (140 kg DM ha(-1) d(-1)) and sward height (111 cm) were highest in the 7 wk cutting interval, but leaf proportion (56%), leaf:stem (1.6) and leaf:non leaf (1.3) ratios decreased. Herbage accumulation, morphological composition and sward structure of Mombasa grass sward may be manipulated through defoliation frequency. The highest leaf proportion was recorded in the 3-wk cutting interval. Longer cutting intervals affected negatively sward structure, with potential negative effects on utilization efficiency, animal intake and performance.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objective: To measure condylar displacement between centric relation (CR) and maximum intercuspation (MIC) in symptomatic and asymptomatic subjects. Materials and Methods: The sample comprised 70 non-deprogrammed individuals, divided equally into two groups, one symptomatic and the other asymptomatic, grouped according to the research diagnostic criteria for temporomandibular disorders (RDC/TMD). Condylar displacement was measured in three dimensions with the condylar position indicator (CPI) device. Dahlberg's index, intraclass correlation coefficient, repeated measures analysis of variance, analysis of variance, and generalized estimating equations were used for statistical analysis. Results: A greater magnitude of difference was observed on the vertical plane on the left side in both symptomatic and asymptomatic individuals (P = .033). The symptomatic group presented higher measurements on the transverse plane (P = .015). The percentage of displacement in the mesial direction was significantly higher in the asymptomatic group than in the symptomatic one (P = .049). Both groups presented a significantly higher percentage of mesial direction on the right side than on the left (P = .036). The presence of bilateral condylar displacement (left and right sides) in an inferior and distal direction was significantly greater in symptomatic individuals (P = .012). However, no statistical difference was noted between genders. Conclusion: Statistically significant differences between CR and MIC were quantifiable at the condylar level in asymptomatic and symptomatic individuals. (Angle Orthod. 2010;80:835-842.)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The VISTA near infrared survey of the Magellanic System (VMC) will provide deep YJK(s) photometry reaching stars in the oldest turn-off point throughout the Magellanic Clouds (MCs). As part of the preparation for the survey, we aim to access the accuracy in the star formation history (SFH) that can be expected from VMC data, in particular for the Large Magellanic Cloud (LMC). To this aim, we first simulate VMC images containing not only the LMC stellar populations but also the foreground Milky Way (MW) stars and background galaxies. The simulations cover the whole range of density of LMC field stars. We then perform aperture photometry over these simulated images, access the expected levels of photometric errors and incompleteness, and apply the classical technique of SFH-recovery based on the reconstruction of colour-magnitude diagrams (CMD) via the minimisation of a chi-squared-like statistics. We verify that the foreground MW stars are accurately recovered by the minimisation algorithms, whereas the background galaxies can be largely eliminated from the CMD analysis due to their particular colours and morphologies. We then evaluate the expected errors in the recovered star formation rate as a function of stellar age, SFR(t), starting from models with a known age-metallicity relation (AMR). It turns out that, for a given sky area, the random errors for ages older than similar to 0.4 Gyr seem to be independent of the crowding. This can be explained by a counterbalancing effect between the loss of stars from a decrease in the completeness and the gain of stars from an increase in the stellar density. For a spatial resolution of similar to 0.1 deg(2), the random errors in SFR(t) will be below 20% for this wide range of ages. On the other hand, due to the lower stellar statistics for stars younger than similar to 0.4 Gyr, the outer LMC regions will require larger areas to achieve the same level of accuracy in the SFR( t). If we consider the AMR as unknown, the SFH-recovery algorithm is able to accurately recover the input AMR, at the price of an increase of random errors in the SFR(t) by a factor of about 2.5. Experiments of SFH-recovery performed for varying distance modulus and reddening indicate that these parameters can be determined with (relative) accuracies of Delta(m-M)(0) similar to 0.02 mag and Delta E(B-V) similar to 0.01 mag, for each individual field over the LMC. The propagation of these errors in the SFR(t) implies systematic errors below 30%. This level of accuracy in the SFR(t) can reveal significant imprints in the dynamical evolution of this unique and nearby stellar system, as well as possible signatures of the past interaction between the MCs and the MW.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We describe the measurement of the depth of maximum, X(max), of the longitudinal development of air showers induced by cosmic rays. Almost 4000 events above 10(18) eV observed by the fluorescence detector of the Pierre Auger Observatory in coincidence with at least one surface detector station are selected for the analysis. The average shower maximum was found to evolve with energy at a rate of (106 +/- 35-21) g/cm(2)/decade below 10(18.24) +/- (0.05) eV, and d24 +/- 3 g/cm(2)/ecade above this energy. The measured shower-to-shower fluctuations decrease from about 55 to 26 g/cm(2). The interpretation of these results in terms of the cosmic ray mass composition is briefly discussed.