18 resultados para Cathodic cage. Iron nitride film. Saturation magnetization


Relevância:

100.00% 100.00%

Publicador:

Resumo:

This study investigated the relationship between iron deficiency/iron deficiency anaemia, assessed by several parameters, and blood lead concentration in children. This cross-sectional study involved 384 Brazilian children, aged 2-11 years, who lived near a lead-manipulating industry. Complete blood counts were obtained by an automated cell counter. Serum iron, total iron binding capacity (TIBC) and ferritin were determined respectively, by colorimetric, turbidimetric methods and chemiluminescence. Blood lead was measured by atomic absorption spectrophotometry. The impact of several parameters for assessment of iron status (haemoglobin, serum iron, TIBC, transferrin saturation, ferritin, red cell indices and red cell distribution width) and variables (gender, age, mother`s education, income, body mass index, iron intake, and distance from home to lead-manipulating industry) on blood lead concentration was determined by multiple linear regression. There were significant negative associations between blood lead and the distance from home to the lead-manipulating industry (P < 0.001), Hb (P = 0.019), and ferritin (P=0.023) (R(2)=0.14). Based on these results, further epidemiological studies are necessary to investigate the impact of interventions like iron supplementation or fortification, as an attempt to decrease blood lead in children. (C) 2011 Royal Society of Tropical Medicine and Hygiene. Published by Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Glass microspheres containing radionuclides are used to treat liver cancer. A promising alternative therapy is being developed based on the magnetic hyperthermia which is related to the heat supplied by a magnetic material under an alternating current magnetic field. The advantage of this option is that most of killed cells are cancer cells which are more susceptible to the temperature raise. In the present work aluminum iron silicate glasses containing minor glass modifiers and nucleating agents were synthesized as irregular shape particles which were further transformed in microspheres by using a petrol liquefied gas-oxygen torch. The optimized processing parameters which lead to microspheres that give a response to the magnetic field were determined. The dissolution rate in water at 90 degrees C was determined to be 3 x 10(-8) g cm(-2) min(-1). The microsphere size distribution was determined by laser scattering. The crystalline phase responsible for the ferromagnetic response was identified as magnetite. Since this phase has a high saturation magnetization and high Curie temperature, it is potentially useful for biomedical applications. The hysteresis magnetic loop was measured for materials produced in different conditions, and some of them showed to be appropriated for thermotherapy. The ratio Fe(3+)/Fe(total) was determined by Mossbauer spectroscopy. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Iron supplementation in hemodialysis patients is fundamental to erythropoiesis, but may cause harmful effects. We measured oxidative stress using labile plasma iron (LPI) after parenteral iron replacement in chronic hemodialysis patients. Intravenous iron saccharate (100 mg) was administered in patients undergoing chronic hemodialysis (N = 20). LPI was measured by an oxidant-sensitive fluorescent probe at the beginning of dialysis session (T0), at 10 min (T1), 20 min (T2), and 30 min (T3) after the infusion of iron and at the subsequent session; P < 0.05 was significant. The LPI values were significantly raised according to the time of administration and were transitory: -0.02 +/- 0.20 mu mol/L at the beginning of the first session, 0.01 +/- 0.26 mu mol/L at T0, 0.03 +/- 0.23 mu mol/L at T1, 0.09 +/- 0.28 mmol/L at T2, 0.18 +/- 0.52 mmol/L at T3, and -0.02 +/- 0.16 mmol/L (P = 0.001 to 0.041) at the beginning of the second session. The LPI level in patients without iron supplementation was -0.06 +/- 0.16 mmol/L. Correlations of LPI according to time were T1, T2, and T3 vs. serum iron (P = 0.01, P = 0.007, and P = 0.0025, respectively), and T2 and T3 vs. transferrin saturation (P = 0.001 and P = 0.0003, respectively). LPI generation after intravenous saccharate administration is time-dependent and transitorily detected during hemodialysis. The LPI increment had a positive correlation to iron and transferrin saturation.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Hydrogen interaction with oxide films grown on iron electrodes at open circuit potential (E-oc) and in the passive region (+0.30 V-ECS) was studied by chronopotentiometry, chronoamperometry and electrochemical impedance spectroscopy techniques. The results were obtained in deaerated 0.3 mol L-1 H3BO3 + 0.075 mol L-1 Na2B4O7 (BB, pH 8.4) solution before, during and after hydrogen permeation. The iron oxide film modification was also investigated by means of in situ X-ray absorption near-edge spectroscopy (XANES) and scanning electrochemical microscopy (SECM) before and during hydrogen permeation. The main conclusion was that the passive film is reduced during the hydrogen diffusion. The hydrogen permeation stabilizes the iron surface at a potential close to the thermodynamic water stability line where hydrogen evolution can occur. The stationary condition required for the determination of the permeation parameters cannot be easily attained on iron surface during hydrogen permeation. Moreover, additional attention must be paid when obtaining the transport parameters using the classical permeation cell. (c) 2007 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This work involved an investigation to ascertain how the substitution of nickel ions for zinc ions affects the structural, morphological and magnetic properties of NiFe(2)O(4) ferrite samples. Ni(1-x)Zn(x)Fe(2)O(4) (x = 0.0, 0.3 0.5, 0.7) powders were prepared by combustion reaction and characterized structurally by X-ray diffraction. The specific surface area of the powders was determined by the nitrogen adsorption method (BET). Magnetization measurements were taken using an alternative gradient magnetometer (AGM), which revealed that the powders prepared by combustion reaction resulted in nanosized particles with a particle size of 18-27 nm. The crystallite size and lattice parameter increased as the concentration of Zn increased. Moreover, augmenting the Zn content in the NiFe(2)O(4) ferrite increased the saturation magnetization and coercive field. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ni-Zn ferrites have been widely used in components for high-frequency range applications due to their high electrical resistivity, mechanical strength and chemical stability. Ni-Zn ferrite nanopowders doped with samarium with a nominal composition of Ni0.5Zn0.5Fe2-xSmxO4 (x = 0.0, 0.05, and 0.1 mol) were obtained by combustion synthesis using nitrates and urea as fuel. The morphological aspects of Ni-Zn-Sm ferrite nanopowders were investigated by X-ray diffraction, nitrogen adsorption by BET, sedimentation, scanning electron microscopy and magnetic properties. The results indicated that the Ni-Zn-Sm ferrite nanopowders were composed of soft agglomerates of nanoparticles with a high surface area (55.8-64.8 m(2)/g), smaller particles (18-20 nm) and nanocrystallite size particles. The addition of samarium resulted in a reduction of all the magnetic parameters evaluated, namely saturation magnetization (24-40 emu/g), remanent magnetization (2.2-3.5 emu/g) and coercive force (99.3-83.3 Oe). (c) 2007 Elsevier B. V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The goal of this study is to evaluate the influence of the urea and glycine fuels on the synthesis of Mn-Zn ferrite by combustion reaction The morphology and magnetic properties of the resulting powders were investigated. The powders were characterized by X-ray diffraction (XRD), nitrogen adsorption (BET), scanning and transmission electron microscopy (SEM and TEM), and magnetic measurement of M x H curves. The X-lay diffraction patterns indicated that the samples containing urea resulted in the formation of crystalline powders and the presence of hematite as a secondary phase The samples containing glycine presented only the formation of crystalline and monophases (Mn,Zn)Fe(2)O(4). The average crystallite size was 18 and 35 nm and saturation magnetization was 3.6 and 75 emu/g, respectively, for the samples containing urea and glycine. The samples synthesized with glycine fuel showed better magnetic properties for application as soft magnetic devices. (C) 2009 Elsevier B.V All rights reserved

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This paper reports on a study of Cr(3+)-doped nanosized Ni-Zn ferrites produced by combustion reaction, and evaluates their morphological and magnetic properties. The powders were characterized by X-ray diffraction (XRD) and SEM and magnetic properties. All the compositions showed the formation of the inverse spinel phase of Ni-Zn ferrite. The average crystallite size ranged from 21 to 26 nm. The saturation magnetization was found to be in the range of 53-43 emu/g. The increase in Cr(3+) concentration in the Ni-Zn ferrite caused a reduction in hysteresis losses and a slight reduction in the saturation magnetization. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The disclosure of magnetic ionic liquids (MILs) as stable dispersions of surface modified gamma-Fe(2)O(3) or CoFe(2)O(4) nanoparticles (NPs) in the 1-n-butyl-3-methylimidazolium tetrafluoroborate (BMIBF(4)) ionic liquid is reported. The magnetic NPs were characterized by X-ray powder diffraction, transmission electron microscopy, and Raman spectroscopy. The surface modified NPs have proved to form stable dispersions in BMIBF(4) in the absence of water and behave like a magnetic ionic liquid. The MILs have been characterized by Raman spectroscopy, magnetic measurements, and DSC. The stability of the magnetic NPs in BMIBF(4) is consistently explained by assuming the formation of a semiorganized protective layer composed of supramolecular aggregates in the form of [(BMI)(2)(BF(4))(3)](-). A superparamagnetic behavior and saturation magnetization of ca. 18 emu/g for a sample containing 30% w/w maghemite NPs/BMIBF(4) have been inferred from static and dynamic magnetic measurements. DSC results have shown that the MIL composed of 30% w/w CoFe(2)O(4) NPs/BMIBF(4) remains a liquid phase down to -84 degrees C.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We have studied the magnetic and power absorption properties of a series of magnetic nanoparticles (MNPs) of Fe(3)O(4) with average sizes < d > ranging from 3 to 26 rim. Heating experiments as a function of particle size revealed a strong increase in the specific power absorption (SPA) values for particles with < d > = 25-30 mn. On the other side saturation magnetization M(s) values of these MNPs remain essentially constant for particles with < d > above 10 rim, suggesting that the absorption mechanism is not determined by Ms. The largest SPA value obtained was 130 W/g, corresponding to a bimodal particle distribution with average size values of 17 and 26 nm.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Thin silicon nitride films were prepared at 350 degrees C by inductively coupled plasma chemical vapor deposition on Si(100) substrates under different NH(3)/SiH(4) or N(2)/SiH(4) gas mixture. The chemical composition and bonding structure of the deposited films were investigated as a function of the process parameters, such as the gas flow ratio NH(3)/SiH(4) or N(2)/SiH(4) and the RF power, using X-ray photoelectron spectroscopy (XPS). The gas flow ratio was 1.4, 4.3, 7.2 or 9.5 and the RF power, 50 or 100 W. Decomposition results of Si 2p XPS spectra indicated the presence of bulk Si, under-stoichiometric nitride, stoichiometric nitride Si(3)N(4), oxynitride SiN(x)O(y), and stoichiometric oxide SiO(2), and the amounts of these compounds were strongly influenced by the two process parameters. These results were consistent with those obtained from N 1s XPS spectra. The chemical composition ratio N/Si in the film increased with increasing the gas flow ratio until the gas flow ratio reached 4.3, reflecting the high reactivity of nitrogen, and stayed almost constant for further increase in gas flow ratio, the excess nitrogen being rejected from the growing film. A considerable and unexpected incorporation of contaminant oxygen and carbon into the depositing film was observed and attributed to their high chemical reactivity. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Thin zirconium nitride films were prepared on Si(l 00) substrates at room temperature by ion beam assisted deposition with a 2 keV nitrogen ion beam. Arrival rate ratios ARR(N/Zr) used were 0.19, 0.39, 0.92, and 1.86. The chemical composition and bonding structure of the films were analyzed with X-ray photoelectron spectroscopy (XPS). Deconvolution results for Zr 3d, Zr 3p(3/2), N 1s, O 1s, and C 1s XPS spectra indicated self-consistently the presence of metal Zr-0, nitride ZrN, oxide ZrO2, oxymnide Zr2N2O, and carbide ZrC phases, and the amounts of these compounds were influenced by ARR(N/Zr). The chemical composition ratio N/Zr in the film increased with increasing ARR(N/Zr) until ARR(N/Zr) reached 0.92, reflecting the high reactivity of nitrogen in the ion beam, and stayed almost constant for ARR(N/Zr) >= 1, the excess nitrogen being rejected from the growing film. A considerable incorporation of contaminant oxygen and carbon into the depositing film was attributed to the getter effect of zirconium. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The perpendicular exchange bias and magnetic anisotropy were investigated in IrMn/Pt/[Co/Pt](3) multilayers through the analysis of in-plane and out-of-plane magnetization hysteresis loops. A phenomenological model was used to simulate the in-plane curves and the effective perpendicular anisotropies were obtained employing the area method. The canted state anisotropy was introduced by taking into account the first and second uniaxial anisotropy terms of the ferromagnet with the corresponding uniaxial anisotropy direction allowed to make a nonzero angle with the film`s normal. This angle, obtained from the fittings, was of approximately 15 degrees for IrMn/[Co/Pt](3) film and decreases with the introduction of Pt in the IrMn/Pt/[Co/Pt](3) system, indicating that the Pt interlayer leads to a predominant perpendicular anisotropy. A maximum of the out-of-plane anisotropy was found between 0.5 and 0.6 nm of Pt, whereas a maximum of the perpendicular exchange bias was found at 0.3 nm. These results are very similar to those obtained for IrMn/Cu/[Co/Pt](3) system; however, the decrease of the exchange bias with the spacer thickness is more abrupt and the enhacement of the perpendicular anisotropy is higher for the case of Cu spacer as compared with that of Pt spacer. The existence of a maximum in the perpendicular exchange bias as a function of the Pt layer thickness was attributed to the predominance of the enhancement of exchange bias due to more perpendicular Co moment orientation over the exponential decrease of the ferromagnetic/antiferromagnetic exchange coupling and, consequently, of the exchange-bias field. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Magnetic properties of nanocrystalline NiFe(2)O(4) spinel mechanically processed for 350 h have been studied using temperature dependent from both zero-field and in-field (57)Fe Mossbauer spectrometry and magnetization measurements. The hyperfine structure allows us to distinguish two main magnetic contributions: one attributed to the crystalline grain core, which has magnetic properties similar to the NiFe(2)O(4) spinel-like structure (n-NiFe(2)O(4)) and the other one due to the disordered grain boundary region, which presents topological and chemical disorder features(d-NiFe(2)O(4)). Mossbauer spectrometry determines a large fraction for the d-NiFe(2)O(4) region(62% of total area) and also suggests a speromagnet-like structure for it. Under applied magnetic field, the n-NiFe(2)O(4) spins are canted with angle dependent on the applied field magnitude. Mossbauer data also show that even under 120 kOe no magnetic saturation is observed for the two magnetic phases. In addition, the hysteresis loops, recorded for scan field of 50 kOe, are shifted in both field and magnetization axes, for temperatures below about 50 K. The hysteresis loop shifts may be due to two main contributions: the exchange bias field at the d-NiFe(2)O(4)/n-NiFe(2)O(4) interfaces and the minor loop effect caused by a high magnetic anisotropy of the d-NiFe(2)O(4) phase. It has also been shown that the spin configuration of the spin-glass like phase is modified by the consecutive field cycles, consequently the n-NiFe(2)O(4)/d-NiFe(2)O(4) magnetic interaction is also affected in this process. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

An approach is presented that can also account for the description of small ferromagnetic particle magnetization tunneling. An estimate of the saturation value of an external applied magnetic field along the easy axis is obtained. An analytic expression for the tunneling factor in the absence of an external magnetic field is deduced from the present approach that also allows one to obtain the crossover temperature characterizing the regime where tunneling is dominated by quantum effects. (C) 2009 Published by Elsevier B.V.