4 resultados para BIO-09
em WestminsterResearch - UK
Resumo:
The decolourisation of acid orange 7 (AO7) (C.I.15510) through co-metabolism in a microbial fuel cell by Shewanella oneidensis strain 14063 was investigated with respect to the kinetics of decolourisation, extent of degradation and toxicity of biotransformation products. Rapid decolourisation of AO7 (>98% within 30 h) was achieved at all tested dye concentrations with concomitant power production. The aromatic amine degradation products were recalcitrant under tested conditions. The first-order kinetic constant of decolourisation (k) decreased from 0.709 ± 0.05 h−1 to 0.05 ± 0.01 h−1 (co-substrate – pyruvate) when the dye concentration was raised from 35 mg l−1 to 350 mg l−1. The use of unrefined co-substrates such as rapeseed cake, corn-steep liquor and molasses also indicated comparable or better AO7 decolourisation kinetic constant values. The fully decolourised solutions indicated increased toxicity as the initial AO7 concentration was increased. This work highlights the possibility of using microbial fuel cells to achieve high kinetic rates of AO7 decolourisation through co-metabolism with concomitant electricity production and could potentially be utilised as the initial step of a two stage anaerobic/aerobic process for azo dye biotreatment.
Resumo:
In the present study, a novel enzyme-based methodology for grafting Polyhydroxyalkanoates (PHAs) onto the ethyl cellulose (EC) as a backbone polymer was developed. Laccase assisted copolymerization was carried out under mild and eco-friendly reaction conditions. The resulting homogeneous composite membranes were characterized by Fourier-transformed infrared spectroscopy (FTIR), scanning electron microscopy (SEM), X-ray diffraction (XRD), differential scanning calorimetry (DSC), and Atomic Force Microscopy (AFM). The FTIR spectra of pure PHAs and PHAs containing graft composites (PHAs-g-EC) showed their strong characteristic bands at 1721 cm1, 1651 cm-1 and 1603 cm-1 respectively. Other accompanying bands in the range of 900-1300 cm-1 correspond to C=O vibration and C-O-C bond stretching, which could be contributed from PHAs and EC, respectively. The high intensity of the 3358 cm-1 band in the graft composite may have corresponded to the degradation of the carboxylic group from PHAs and also showed an increase of hydrogen-bonded groups at that distinct band region. The morphology was examined by SEM, which showed the well dispersed PHAs crystals in the backbone polymer of EC. XRD pattern for PHAs showed distinct peaks at 2-Theta values of 28o, 32o, 34o, 39o, 46o, 57o, 64o, 78o and 84o that represent the crystalline nature of PHAs. In comparison with those of neat PHAs, the degree of crystallinity for PHAs-g-EC decreased and this reduction is mainly because of the new cross-linking of PHAs within the EC backbone that changes the morphology and destroys the crystallites. Improved mechanical properties were observed for the PHAs-g-EC as compared to the individual components due to the impregnation of EC as reinforcement into the PHAs matrix. Improved mechanical strength enhanced thermal properties, along with low crystallinity of the present PHAs-g-EC suggesting its potential for various industrial and bio-medical applications.
Resumo:
Today more than 99% of plastics are petroleum-based because of availability and cost of the raw material. The durability of these disposed plastics contributes to the environmental problems as waste and their persistence in the environment causes deleterious effects on the ecosystem. Environmental pollution awareness and the demand for green technology have drawn considerable attention of both academia and industry into biodegradable polymers. In this regard green chemistry technology has the potential to provide solution to this problematic issue. Laccase bio-grafting has recently been the focus of green chemistry technologies due to the growing environmental concerns, legal restrictions and increasing availability of scientific knowledge. In the last several years, research covering various applications of laccases has been increased rapidly particularly in the field of grafting. In principle, laccase-assisted graft co-polymerization may impart a variety of new functionalities to a polymer. The modified polymers through grafting have a bright future and their development is practically boundless. In present work, novel biodegradable graft copolymers combining the advantages of bacterial cellulose backbone and PHB side chains will be prepared by introducing enzymatic grafting technique. The present research will be a first step in the biopolymer modification. To date no report has been found in literature explaining the enzymatic grafting of PHAs. The technique would also provide an efficient modulation approach to improve the biodegradability and biocompatibility of the graft copolymer. The newly grafted copolymers will exhibit unique functionalities with wider range of potential applications mainly in tissue engineering, biosensors, pharmaceutical industry (drug delivery systems) and bio-plastics.
Resumo:
Recently, the development of highly inspired biomaterials with multi-functional characteristics has gained considerable attention, especially in biomedical, and other health-related areas of the modern world. It is well-known that the lack of antibacterial potential has significantly limited biomaterials for many challenging applications such as infection free wound healing and/or tissue engineering etc. In this perspective, herein, a series of novel bio-composites with natural phenols as functional entities and keratin-EC as a base material were synthesised by laccase-assisted grafting. Subsequently, the resulting composites were removed from their respective casting surfaces, critically evaluated for their antibacterial and biocompatibility features and information is also given on their soil burial degradation profile. In-situ synthesised phenol-g-keratin-EC bio-composites possess strong anti-bacterial activity against Gram-positive and Gram-negative bacterial strains i.e., B. subtilis NCTC 3610, P. aeruginosa NCTC 10662, E. coli NTCT 10418 and S. aureus NCTC 6571. More specifically, 10HBA-g-keratin-EC and 20T-g-keratin-EC composites were 100% resistant to colonisation against all of the aforementioned bacterial strains, whereas, 15CA-g-keratin-EC and 15GA-g-keratin-EC showed almost negligible colonisation up to a variable extent. Moreover, at various phenolic concentrations used, the newly synthesised composites remained cytocompatible with human keratinocyte-like HaCaT, as an obvious cell ingrowth tendency was observed and indicated by the neutral red dye uptake assay. From the degradation point of view, an increase in the degradation rate was recorded during their soil burial analyses. Our investigations could encourage greater utilisation of natural materials to develop bio-composites with novel and sophisticated characteristics for potential applications.