The pyrolysis and combustion of corn stover were studied by dynamic thermogravimetry and derivate thermogravimetry (TG-DTG) at heating rates of 5, 10, 20 and 50 K min−1 at atmospheric pressure. For the simulation of pyrolysis and combustion processes a kinetic model based on the distribution of activation energies was used, with three pools of reactants (three pseudocomponents) because of the complexity of the biomass samples of agricultural origin. The experimental thermogravimetric data of pyrolysis and combustion processes were simultaneously fitted to determine a single set of kinetic parameters able to describe both processes at the different heating rates. The model proposed achieves a good correlation between the experimental and calculated curves, with an error of less than 4% for fitting four heating rates simultaneously. The experimental results and kinetic parameters may provide useful data for the design of thermo decomposition processing system using corn stover as feedstock. On the other hand, analysis of the main compounds in the evolved gas is given by means of a microcromatograph.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The pyrolysis of a sludge produced in the waste water treatment plant of an oil refinery was studied in a pilot plant reactor provided with a system for condensation of semivolatile matter. The study comprises experiments at 350, 400, 470 and 530 °C in nitrogen atmosphere. Analysis of all the products obtained (gases, liquids and chars) are presented, with a thermogravimetric study of the char produced and analysis of main components of the liquid. In the temperature range studied, the composition of the gas fraction does not appreciably vary. In the liquids, the light hidrocarbon yield increases with increasing temperature, whereas the aromatic compounds diminish. The decomposition of the solid fraction has been analysed, finding a material that reacts rapidly with oxygen regardless of the conditions it is formed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The aim of this study is to investigate the effect of particle size on the non-isothermal pyrolysis of almond shells (AS) and olive stones (OS) and to show possible differences in the composition of the different fractions obtained after milling and sieving. The results obtained from the study of different particle size of AS and OS samples show significant differences in the solid residue obtained and in the shape and overlapping degree of the peaks, especially with the smaller particle size. These differences can be due to different factors: (a) the amount of inorganic matter, which increases as particle size decreases, (b) heat and mass transfer processes, (c) different sample composition as a consequence of the milling process which may provoke changes in the structure and the segregation of the components (in addition to the ashes) increasingly changes the composition of the sample as the particle size decreases.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Paper submitted to the 7th International Symposium on Feedstock Recycling of Polymeric Materials (7th ISFR 2013), New Delhi, India, 23-26 October 2013.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Paper submitted to the 31st International Symposium on Halogenated Persistent Organic Compounds (Dioxin 2011), Brussels, Belgium, 21-25 August 2011.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polyvinyl chloride (PVC) is one of the plastics most extensively used due to its versatility. The demand of PVC resin in Europe during 2012 reached 5000 ktonnes1. PVC waste management is a big problem because of the high volume generated all over the world and its chlorine content. End-of-life PVC is mainly mixed with municipal solid waste (MSW) and one common disposal option for this is waste-to-energy incineration (WtE). The presence of plastics such as PVC in the fuel mix increases the heating value of the fuel. PVC has two times higher energy content than MSW ‒around 20 MJ/kg vs 10 MJ/kg, respectively. However, the high chlorine content in PVC resin, 57 wt.%, may be a source for the formation of hazardous chlorinated organic pollutants in thermal processes. Chlorine present in the feedstock of WtE plants plays an important role in the formation of (i) chlorine (Cl2) and (ii) hydrochloric gas (HCl), both of them responsible for corrosion, and (iii) chlorinated organic pollutants2. In this work, pyrolytic and oxidative thermal degradation of PVC resin were carried out in a laboratory scale reactor at 500 ºC in order to analyze the influence of the reaction atmosphere on the emissions evolved. Special emphasis was put on the analysis of chlorinated organic pollutants such as polychlorodibenzo-p-dioxins (PCDDs), polychlorodibenzofurans (PCDFs) and other related compounds like polychlorobenzenes (PCBzs), polychlorophenols (PCPhs) and polycyclic aromatic hydrocarbons (PAHs). Another objective of this work was to compare the results with those of a previous work3 in which emissions at different temperatures in both pyrolysis and combustion of another PVC resin had been studied; in that case, experiments for PCDD/Fs emissions had been performed only at 850 ºC.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Mechanical treatments such as shredding or extrusion are applied to municipal solid wastes (MSW) to produce refuse-derived fuels (RDF). In this way, a waste fraction (mainly composed by food waste) is removed and the quality of the fuel is improved. In this research, simultaneous thermal analysis (STA) was used to investigate how different mechanical treatments applied to MSW influence the composition and combustion behaviour of fuel blends produced by combining MSW or RDF with wood in different ratios. Shredding and screening resulted in a more efficient mechanical treatment than extrusion to reduce the chlorine content in a fuel, which would improve its quality. This study revealed that when plastics and food waste are combined in the fuel matrix, the thermal decomposition of the fuels are accelerated. The combination of MSW or RDF and woody materials in a fuel blend has a positive impact on its decomposition.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A systematic investigation of the thermal decomposition of viscoelastic memory foam (VMF) was performed using thermogravimetric analysis (TGA) to obtain the kinetic parameters, and thermogravimetric analysis coupled to Fourier Transformed Infrared Spectrometry (TGA-FTIR) and thermogravimetric analysis coupled to Mass Spectrometry (TGA-MS) to obtain detailed information of evolved products on pyrolysis and oxidative degradations. Two consecutive nth-order reactions were employed to correlate the experimental data from dynamic and isothermal runs performed at three different heating rates (5, 10 and 20 K/min) under an inert atmosphere. On the other hand, for the kinetic study of the oxidative decomposition, the data from combustion (synthetic air) and poor oxygen combustion (N2:O2 = 9:1) runs, at three heating rates and under dynamic and isothermal conditions, were correlated simultaneously. A kinetic model consisting of three consecutive reactions presented a really good correlation in all runs. TGA-FTIR analysis showed that the main gases released during the pyrolysis of VMF were determined as ether and aliphatic hydrocarbons, whereas in combustion apart from the previous gases, aldehydes, amines and CO2 have also been detected as the main gases. These results were confirmed by the TGA-MS.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Thermal decomposition of printed circuits boards (PCB) is studied, using thermogravimetric analysis to compare the thermal behavior of PCB of mobile phones before and after the removal of the metallic fraction by acid washing. Several dynamic and dynamic + isothermal runs have been carried out at different heating rates (5, 10 and 20 K min−1), from room temperature to more than 1100 K. Also runs in the presence and in the absence of oxygen were performed (combustion and pyrolysis runs). Moreover, TG–MS experiments were performed (both in inert and oxidizing atmosphere) in order to better understand the thermal decomposition of these wastes and identify some compounds emitted during the controlled heating of these materials. Different reaction models are proposed, one for pyrolysis and one for combustion of the two kinds of wastes studied, which proved to simulate appropriately the experimental results at all the heating rates simultaneously.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Paper submitted to the 7th International Symposium on Feedstock Recycling of Polymeric Materials (7th ISFR 2013), New Delhi, India, 23-26 October 2013.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

The thermal decomposition of a solid recovered fuel has been studied using thermogravimetry, in order to get information about the main steps in the decomposition of such material. The study comprises two different atmospheres: inert and oxidative. The kinetics of decomposition is determined at three different heating rates using the same kinetic constants and model for both atmospheres at all the heating rates simultaneously. A good correlation of the TG data is obtained using three nth-order parallel reactions.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Tetrabromobisphenol A (TBBPA) is the most widely used brominated flame retardant worldwide. A detailed examination of the degradation products emitted during thermal decomposition of TBBPA is presented in the study. Runs were performed in a laboratory furnace at different temperatures (650 and 800 °C) and in different atmospheres (nitrogen and air). More than one hundred semivolatile compounds have been identified by GC/MS, with special interest in brominated ones. Presence of HBr and brominated light hydrocarbons increased with temperature and in the presence of oxygen. Maximum formation of PAHs is observed at pyrolytic condition at the higher temperature. High levels of 2,4-, 2,6- and 2,4,6- bromophenols were found. The levels of polybrominated dibenzo-p-dioxins and furans have been detected in the ppm range. The most abundant isomers are 2,4,6,8-TeBDF in pyrolysis and 1,2,3,7,8-PeBDF in combustion. These results should be considered in the assessment of thermal treatment of materials containing brominated flame retardants.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Different Pt- and Ru-doped Ti/SnO2–Sb electrodes were synthesized by thermal decomposition. The effect of the gradual substitution of Sb by Ru in the nominal composition on the physicochemical and electrochemical properties were evaluated. The electrochemical stability of the electrodes was estimated from accelerated tests at 0.5 A cm–2 in 1 M NaOH. Both as-synthesized and deactivated electrodes were thoroughly characterized by scanning electron microscopy (SEM), energy-dispersive X-ray microanalysis (EDX), transmission electron microscopy (TEM), X-ray photoelectron spectroscopy (XPS) and X-ray diffraction analysis (XRD). The incorporation of a small amount (about 3 at. %) of both Pt and Ru into the SnO2–Sb electrodes produced a 400-times increase in their service life in alkaline medium, with no remarkable change in the electrocatalysis of the oxygen evolution reaction (OER). It is concluded that the deactivation of the electrodes is promoted by alkaline dissolution of metal species and coating detachment at high potentials. The introduction of Pt has a coating compacting effect, and Ru(IV), at low amounts until 9.75 at. %, replaces the Sn(IV) cations in the rutile-like SnO2 structure to form a solid solution that strongly increases the stability of the electrodes. The observed Ru segregation and decreased stability for larger Ru contents (x > 9.75 at. %), together with the selective dissolution of Ru after deactivation, suggest that the formation of a homogeneous (RuδSn1−δ)O2 single-phase is crucial for the stabilization of these electrodes.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Thermal decomposition of flexible polyurethane foam (FPUF) was studied under nitrogen and air atmospheres at 550 °C and 850 °C using a laboratory scale reactor to analyse the evolved products. Ammonia, hydrogen cyanide and nitrile compounds were obtained in high yields in pyrolysis at the lower temperature, whereas at 850 °C polycyclic aromatic hydrocarbons (PAHs) and other semivolatile compounds, especially compounds containing nitrogen (benzonitrile, aniline, quinolone and indene) were the most abundant products. Different behaviour was observed in the evolution of polychlorodibenzo-p-dioxins and furans (PCDD/Fs) at 550 °C and 850 °C. At 550 °C, the less chlorinated congeners, mainly PCDF, were more abundant. Contrarily, at 850 °C the most chlorinated PCDD were dominant. In addition, the total yields of PCDD/Fs in the pyrolysis and combustion runs at 850 °C were low and quite similar.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Paper submitted to the 19th International Symposium on Analytical & Applied Pyrolysis, Linz, Austria, 21-25 May 2012.