Resumo:
In recent years, several researchers have shown the good performance of alkali activated slag cement and concretes. Besides their good mechanical properties and durability, this type of cement is a good alternative to Portland cements if sustainability is considered. Moreover, multifunctional cement composites have been developed in the last decades for their functional applications (self-sensing, EMI shielding, self-heating, etc.). In this study, the strain and damage sensing possible application of carbon fiber reinforced alkali activated slag pastes has been evaluated. Cement pastes with 0, 0.29 and 0.58 vol % carbon fiber addition were prepared. Both carbon fiber dosages showed sensing properties. For strain sensing, function gage factors of up to 661 were calculated for compressive cycles. Furthermore, all composites with carbon fibers suffered a sudden increase in their resistivity when internal damages began, prior to any external signal of damage. Hence, this material may be suitable as strain or damage sensor.
Resumo:
An empirical model based on constant flux is presented for chloride transport through concrete in atmospherical exposure conditions. A continuous supply of chlorides is assumed as a constant mass flux at the exposed concrete surface. The model is applied to experimental chloride profiles obtained from a real marine structure, and results are compared with the classical error-function model. The proposed model shows some advantages. It yields a better predictive capacity than the classical error-function model. The previously observed chloride surface concentration increases are compatible with the proposed model. Nevertheless, the predictive capacity of the model can fail if the concrete microstructure changes with time. The model seems to be appropriate for well-maturated concretes exposed to a marine environment in atmospherical conditions.
Resumo:
La détermination directe des caractéristiques de cisaillement des bétons par des essais universels est un problème qui reste encore une préoccupation majeure des chercheurs. La plupart des études disponibles consistent à appliquer un couple de torsion à un cylindre creux ayant un rapport épaisseur/rayon le plus faible possible. Ceci pour pouvoir élaborer un critère lié au comportement du matériau et non de la structure (Fourd et al. 1982). Cependant, ces essais peuvent présenter des dispersions liées aux problèmes de fragilité à la rupture ou de non homogénéité du matériau au sein de la paroi (Gotuwka et al. 1999). Pour cela, un dispositif expérimental original a été utilisé et qui consiste en la création de deux zones de contrainte nulle par l’emplacement de corps déformables au moment du coulage de l’éprouvette. De nouvelles conditions aux frontières sont créées permettant de transformer la sollicitation de compression en cisaillement plan sur une zone bien déterminée. L’utilisation de cette technique permet la détermination de l’influence de l’inclinaison du plan de rupture sur le comportement du béton en cisaillement. Le dispositif permet d’assurer la perpendicularité NOvEMBRE 2012 5 des génératrices du cylindre ainsi que la répartition et l’homogénéité des contraintes.
Resumo:
Se plantea la combinación binaria y ternaria de cenizas de lodo de depuradora (CLD) con ceniza volante, polvo de mármol y ceniza de cáscara de arroz, como sustitución parcial o como adición respecto al cemento Portland en hormigones, con una dosificación similar a la utilizada en la prefabricación de bloques (consistencia muy seca). Se llevaron a cabo ensayos físico-mecánicos sobre probetas de mortero y hormigón con edades de curado de 28 y 90 días: densidad, absorción y resistencia a compresión. Se comprueba que la sustitución de cemento por CLD supone una disminución de la densidad y de la resistencia respecto a la muestra patrón, sin embargo, las combinaciones con otros residuos mejoran notablemente las características de los materiales cementantes. La adición de CLD proporcionó densidades y resistencias similares a la muestra de control y reduce significativamente la absorción de agua.
Resumo:
The Mediterranean wall, which is a collection of defensive constructions along the coast, was built during the Spanish War (1936-39) to prevent enemy attacks. It´s called this way like the Atlantic Wall, which was built after the Second World War. These group of buildings consist of batteries, bunkers and barracks placed along the coastline, sometimes next to another kind of infrastructure. Its location (typical of a military strategy) and its peculiar morphology are like another ones: the historical watchtowers ones. They were built by the Kingdom of Spain in the same geography four centuries earlier although, in our case, the buildings are updated to the conditions of contemporary wars: camouflage against air raids. A collection of anti-aircraft devices, placed along the coast since the late 1937, were risen following the instructions of the Valencian State to defend both citizens and cities from the aviation´s bombings. The following military settlements, organized from North to South, are part of the most relevant ones of the coast of Alicante: the Denia and Javea ones, the North of Alicante and Southwest of Alicante ones, the Portichol one, the Galvany´s Clot one and, finally, the Cape and Bay of Santa Pola ones. Remains of more than 60 architectural elements, that document the first concrete´s ruins, are still there. This paper tries to document all of them (providing their location, their morphological genealogy and including some drawings of the current state) to contribute to their revaluation and to help to their necessary protection. They are a legacy of architectural heritage which consolidates and increases the memory of our culture.
Resumo:
Measurement of concrete strain through non-invasive methods is of great importance in civil engineering and structural analysis. Traditional methods use laser speckle and high quality cameras that may result too expensive for many applications. Here we present a method for measuring concrete deformations with a standard reflex camera and image processing for tracking objects in the concretes surface. Two different approaches are presented here. In the first one, on-purpose objects are drawn on the surface, while on the second one we track small defects on the surface due to air bubbles in the hardening process. The method has been tested on a concrete sample under several loading/unloading cycles. A stop-motion sequence of the process has been captured and analyzed. Results have been successfully compared with the values given by a strain gauge. Accuracy of our methods in tracking objects is below 8 μm, in the order of more expensive commercial devices.
Resumo:
Mercury intrusion porosimetry (MIP) has been widely used to evaluate the quality of concrete through the pore size distribution parameters. Two of these parameters are the critical pore diameter (Dcrit) and the percentage of the most interconnected net of pores compared to the total volume of pores. Some researchers consider Dcrit as the diameter obtained from the inflexion point of the cumulative mercury intrusion curve while others consider Dcrit as the diameter obtained from the point of abrupt variation in the same curve. This study aims to analyze two groups of concretes of varying w/c ratios, one cast with pozzolanic cement and another with high initial strength cement, in order to determine which of these diameters feature a better correlation with the quality parameters of the concretes. The concrete quality parameters used for the evaluations were (1) the w/c ratios and (2) chloride diffusion coefficients measured at approximately 90 days. MIP cumulative distributions of the same concretes were also measured at about 90 days, and Dcrit values were determined (1) from the point of abrupt variation and alternatively, (2) from the inflexion point of each of these plots. It was found that Dcrit values measured from the point of abrupt variation were useful indicators of the quality of the concrete, but the Dcrit values based on the inflexion points were not. Hence, it is recommended that Dcrit and the percentage of the most interconnected volume of pores should be obtained considering the point of abrupt variation of the cumulative curve of pore size distribution.
Resumo:
En el conjunto de materiales de construcción habituales en la edificación y las obras de ingeniería, el hormigón destaca entre otras razones por su excelente comportamiento frente a las altas temperaturas y la exposición al fuego. El presente estudio se centra en la adherencia residual entre el hormigón y las barras de acero corrugado soldable tras exponer probetas a altas temperaturas y enfriarlas hasta temperatura ambiente por convección natural. El estudio incluye hormigones de resistencia convencional, hormigones de alta resistencia y hormigones reforzados con fibras de polipropileno y fibras de acero. La adherencia hormigón-acero se ha medido mediante el conocido ensayo de pull-out. La campaña experimental también ha incluido la resistencia a compresión y la resistencia a tracción indirecta. Parte de las probetas se han ensayado a 28 días de edad a temperatura ambiente. A 60 días de edad se han repetido los ensayos a temperatura ambiente y se han realizado esos mismos ensayos en probetas calentadas en un horno industrial hasta tres rangos de temperatura: 450°C, 650°C y 825°C. Previo al proceso de calentamiento han sido sometidas durante 3 horas a un escalón de secado a 120°C. Mediante la metodología propuesta ha sido posible caracterizar la evolución de la pérdida de adherencia residual entre el acero y el hormigón conforme se exponen los especímenes a temperaturas más elevadas. La adición de fibras no tiene una influencia clara en la adherencia a temperatura ambiente. Sin embargo, sí se ha conseguido determinar una mejora sustancial de la adherencia residual en los hormigones, reforzados con fibras de acero sometidos a altas temperaturas.
Resumo:
Concern for the environment has lately heightened awareness about the need for recycling in the construction industry. However, some standards, such as the Spanish standard, only accept the recycling of aggregates derived from concrete, which limits the extensive use of construction and demolition waste, which are produced in much bigger volumes. The aim of this work was to explore the possibility of using recycled mixed aggregates (RMA) in the preparation of precast non-structural concretes. To that end different percentages of natural aggregate were replaced by RMA in non-structural elements (25, 50, 75 and 100%). Contents of cement, water, and the dosages commonly used by companies were unchanged by the introduction of RMA. The characterization of the prepared elements has been done using the specific tests for each type of non-structural element (terrazzo for indoor use, hollow tiles, kerbstones and paving blocks): compression and flexural strength, water absorption, dimensional tolerances, abrasion and slipping resistance. The paving blocks, kerbstones, and hollow tiles prepared were tested for 360 days. The stability of the tested properties confirmed the possibility of using these wastes on an industrial scale satisfying the standard requirements. However, the surface of terrazzo with RMA is not as good as that prepared with natural aggregate.