5 resultados para electron microprobe analyses
em University of Queensland eSpace - Australia
Resumo:
The effect of manganese on gain refinement of a commercial AZ31 alloy has been investigated using an Al-60%Mn master alloy splatter as an alloying additive at 730 degrees C in aluminium titanite crucibles. It is shown that grain refinement by manganese is readily achievable in AZ31. Electron microprobe analyses reveal that prior to the addition of extra manganese the majority of the intermetallic particles found in AZ31 are of the AL(8)Mn(5) type. However, after the addition of extra manganese in the range from 0.1% to 0.8%, the predominant group of intermetallic particles changes to the metastable AlMn type. This leads to a hypothesis that the metastable AlMn intermetallic particles are more effective than Al8Mn5 as nucleation sites for magnesium grains. The hypothesis is supported by the observation that a long period of holding at 730 degrees C leads to an increase in grain size, due probably to the transformation of the metastable AlMn to the stable Al8Mn5. The hypothesis has also been used to understand the mechanism of grain refinement by superheating.
Resumo:
The impact of fluorine in copper flotation was relatively unknown until the introduction of skarn ores in the Ok Tedi concentrator. Fluorine in the copper concentrates reports to the gas phase during the smelting stage and forms a corrosive H2SO4-HCl-HF acid brine mixture which must be neutralised. This work was aimed at studying the mineralogy of the fluorosilicate minerals contained in the various oretypes present in the Ok Tedi porphyry copper deposit. The electron microprobe was used to analyse for fluorine and hence identify the fluorosilicate minerals in each oretype. This study revealed talc, phlogopite, biotite, clays, amphiboles, fluoroapatite and titanite to be the sources of fluorine in the orebody. Laboratory and plant investigations were conducted to study the flotation response of these minerals. Chemical assaying of the products of these tests was done to determine the bulk assay of fluorine, Using Rietveld analysis, quantitative estimates of the fluorosilicate minerals in these products were generated. Marrying of the bulk assay with the respective mineralogical assay enabled the understanding of the flotation behavior of fluorine and it's associated mineralogy. Talc and phlogopite were found to be the causes of the fluorine problem at Ok Tedi. (C) 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
One hundred and twenty-five mineral grains from 45 visually pure K-bearing Mn oxide (hollandite group) samples collected from weathering profiles in the Mt Tabor region of central Queensland, Australia, were analysed by the Ar-40/Ar-39 laser probe technique. These K-Mn oxides precipitated mainly through a process of cavity filling (direct precipitation from weathering solution), with botryoidal texture formed by micrometric mineral bands. Well-defined and reproducible plateau ages have been obtained for most samples, ranging from 27.2 +/- 0.8 to 6.8 +/- 0.5 Ma (2 sigma). Statistical analysis of the geochronological results by mixture modelling suggests an episodic mineral precipitation history, with two major peaks at 20.2 +/- 0.22 Ma and 16.5 +/- 0.17 Ma. The geochronological results, when combined with information on paragenetic relationships and mineralogical textures obtained from petrographic, scanning electron microscopy, and electron microprobe investigations, indicate that warm and humid palaeoclimatic conditions favourable to intense chemical weathering prevailed in central Queensland from late Oligocene to middle Miocene, particularly in the early Miocene. These results, in conjunction with previous and ongoing investigations in NW and eastern Queensland, suggest that most of Queensland was dominated by humid climates during the Miocene. (C) 2002 Elsevier Science BN. All rights reserved.
Resumo:
The amelogenesis imperfectas (Al) area geneticatly heterogeneous group of diseases that result in defective development of tooth enamel. Although X-linked, autosomal. dominant and autosomal. recessive forms of Al have been clinically characterized, only two genes (AMELX and ENAM) have been associated with Al. To date, three enamelin (ENAM) mutations have been identified. These mutations cause phenotypically diverse forms of autosomal. dominant Al. Detailed phenotype-genotype correlations have not been performed for autosomal. dominant Al due to ENAM mutations. We identified a previously unreported kindred segregating for the ENAM mutation, g.8344delG. Light and electron microscopy analyses of unerupted permanent teeth show the enamel is markedly reduced in thickness, Lacks a prismatic structure and has a laminated appearance. Taken together these histological features support the enamelin protein as being critical for the development of a normal. enamel. thickness and that it Likely has a role in regulating c-axis crystallite growth. Because there is growing molecular and phenotypic diversity in the enamelin defects, it is critical to have a nomenclature and numbering system for characterizing these conditions. We present a standardized nomenclature for ENAM mutations that will allow consistent reporting and communication. (C) 2003 Elsevier Science Ltd. All rights reserved.