6 resultados para Y2O3

em University of Queensland eSpace - Australia


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Y2O3 is a c-type rare earth oxide with a fluorite-related structure. This material has been used to refractory because of its high thermal stability and excellent resistance to hydration. In this study, the effective index was suggested in order to improve the electrolytic properties of Y2O3-based oxide. (CexY1-x)(2)O3+delta (x = 0.25 and 0.3) and [LaaSrbCe0.25Y(1-a-b)](2)O3+delta (a = 0.05, 0.1 and 0.15, b = 0, 0.006 and 0.0125) were prepared as the examples with intermediate and high index, respectively. The specimens with high index value such as (La0.15Ce0.25Y0.60)(2)O-3.25 and (La0.1Sr0.0125Ce0.25Y0.6375)(2)O-3.24 consisted of two phases such as c-type and fluorite, although (Ce0.25Y0.75)(2)O-3.25 with intermediate index value had a single phase of c-type rare earth oxide. Microanalysis indicates that a grain in the (La0.1Sr0.0125Ce0.25Y0.6375)(2)O-3.23(7) sintered body consists of c-type and fluorite phases. An interface between c-type and fluorite phases is coherent in a grain. This suggests that this effective index guides the crystal structure in the specimen to fluorite and the examined composition introduces the interface between c-type and fluorite in the microstructure. The electrochemical properties of specimens including Y2O3 were characterized on the basis of the suggested index. The electrical conductivity of Y2O3-based materials increased with an increase of the index. The apparent activation energy of Y2O3-based materials decreased with increasing index. The ionic transport number of oxygen of the specimens was improved by enhancement of the index, confirming validity of the index. The oxide ionic conductive region of (La0.1Sr0.0125Ce0.25Y0.(6375))(2)O-3.23(7) with high effective index extended up to P-O2 = 10(-18) atm at 800 degreesC, although the specimens with low or intermediate index showed p- or n-type semi-conduction in the same P-O2 region at 800 and 1000 degreesC. These results suggest that the interface between c-type and fluorite phases also contributes to improve the electrolytic properties in the grain. It is concluded that the improvement of electrolytic properties in Y2O3-based materials is attributable to the microstructure with interface between two phases in a grain and the fluorite structure guided by the suggested index. (C) 2001 Published by Elsevier Science B.V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Local structures around host Ce and dopant Y cations in 10 mol% Y2O3 doped ceria solid solutions have been investigated by room and high temperature EXAFS spectroscopy. The results show that the local structures around the Cc cation in doped ceria samples are similar to that in the fluorite CeO2 structure though the coordination numbers of Ce-O tend to be smaller than 8. The local structures around Y cation, however, are significantly different from those around Ce cation, and show more resemblance to that around Y cation in the C-type Y2O3 Structure. A more accurate description of the local structures around Y cation in doped ceria was given by analyzing Y-K edge EXAFS spectra based on the C-type Y2O3 structure. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Y-Ba-Cu-O samples with additions of Y2O3 and CeO2 were quenched during seeded isothermal melt processing and examined by optical microscopy and scanning electron microscopy. Large YBa2Cu3O7-y (Y123) particles in the starting powder were found to form a distinct type of melt during heating, which was unaffected by the Y2O3 or CeO2 additives. This type of melt later formed regions with a low concentration of Y2BaCuO5 (Y211) particles in the Y123 matrix. The maximum growth rate of Y123 that could be sustained in the sample was found to be lower in the melt formed from large Y123 particles, and this may lead to growth accidents and subgrains in some samples.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper reviews the current knowledge and understanding of martensitic transformations in ceramics - the tetragonal to monoclinic transformation in zirconia in particular. This martensitic transformation is the key to transformation toughening in zirconia ceramics. A very considerable body of experimental data on the characteristics of this transformation is now available. In addition, theoretical predictions can be made using the phenomenological theory of martensitic transformations. As the paper will illustrate, the phenomenological theory is capable of explaining all the reported microstructural and crystallographic features of the transformation in zirconia and in some other ceramic systems. Hence the theory, supported by experiment, can be used with considerable confidence to provide the quantitative data that is essential for developing a credible, comprehensive understanding of the transformation toughening process. A critical feature in transformation toughening is the shape strain that accompanies the transformation. This shape strain, or nucleation strain, determines whether or not the stress-induced martensitic transformation can occur at the tip of a potentially dangerous crack. If transformation does take place, then it is the net transformation strain left behind in the transformed region that provides toughening by hindering crack growth. The fracture mechanics based models for transformation toughening, therefore, depend on having a full understanding of the characteristics of the martensitic transformation and, in particular, on being able to specify both these strains. A review of the development of the models for transformation toughening shows that their refinement and improvement over the last couple of decades has been largely a result of the inclusion of more of the characteristics of the stress-induced martensitic transformation. The paper advances an improved model for the stress-induced martensitic transformation and the strains resulting from the transformation. This model, which separates the nucleation strain from the subsequent net transformation strain, is shown to be superior to any of the constitutive models currently available. (C) 2002 Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A significant enhancement in glass formation in a newly developed Zr51Cu20.7Ni12Al16.3 alloy has been achieved by yttrium doping. With just 0.5 at.% yttrium doping, the critical diameter of the as-cast alloys for glass formation has been increased from 3 mm to at least 10 mm. In the undoped, large-sized alloys, massive oxygen stabilized crystalline phases are observed but disappear in yttrium doped alloys. Very small amounts of stable alpha-Y2O3 phases found in the yttrium doped alloys, and their negligible effect on the metallic glasses' properties, provide a superior solution to achieve metallic glasses with a high glass formability. (c) 2006 Elsevier B.V. All rights reserved.