The nanocomposites of general layered clays and metal sulfides could be produced from reactions of the layered clay aqueous suspensions and water-soluble metal-thiourea complexes. The clay could be saponite, montmorillonite, hectorite and laponite, while the metal sulfide could be cobalt sulfide, nickel sulfide, zinc sulfide, cadmium sulfide, and lead sulfide. In the nanocomposites, the clay could be incorporated with the metal sulfide pillars and metal sulfide nanoparticles. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The phase equilibria in the Fe-Zn-O system in the range 900-1580degreesC in air have been experimentally studied using equilibration and quenching techniques. The compositions of the phases at equilibrium were determined using electron probe X-ray microanalysis (EPMA). The ferrous and ferric bulk iron concentrations were measured with a wet chemical analysis using the ammonium metavanadate technique. X-ray powder diffraction analysis (XRD) was used to characterise the phases. Iron oxide dissolved in zincite was found to be present principally in the ferric form. The XRD analysis and the composition measurements both indicate that zincite is the only phase stable in the ZnO-rich area in the range of conditions investigated. The solubility of the iron oxide in zincite rapidly increases at temperatures above 1200degreesC; the morphology of the zincite crystals also sharply changes between 1200 and 1300degreesC from rounded to plate-like crystals. The plate-like zincite forms a refractory network-the type of microstructure beneficial to the Imperial Smelting Process (ISP) sinter performance. The software program FactSage with a thermodynamically optimised database was used to predict phase equilibria in the Fe-Zn-O system.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Zincite and spinel phases are present in the complex slag systems encountered in zinc/lead sintering and zinc smelting processes. These phases form extensive solid solutions and are stable over a wide range of compositions, temperatures and oxygen partial pressures. Accurate information on the stability of these phases is required in order to develop thermodynamic models of these slag systems. Phase equilibria in the Fe–Zn–O system have been experimentally studied for a range of conditions, between 900°C and 1580°C and oxygen partial pressures (pO2) between air and metallic iron saturation, using equilibration and quenching techniques. The compositions of the phases were measured using Electron probe X-ray microanalysis (EPMA). The ferrous and ferric bulk iron concentrations were determined using a specially developed wet-chemical analysis procedure based on the use of ammonium metavanadate. XRD was used to confirm phase identification. A procedure was developed to overcome the problems associated with evaporation of zinc at low pO2 values and to ensure the achievement of equilibria. An isothermal section of the system FeO–Fe2O3–ZnO at high ZnO concentrations at 1200°C was constructed. The maximum solubilities of iron and zinc in zincite and spinel phases in equilibrium were determined at pO2 = 1 × 10-6 atm at 1200°C and 1300°C. The morphology of the zincite crystals sharply changes in air between 1200–1300°C from rounded to plate-like. This is shown to be associated with significant increase in total iron concentration, the additional iron being principally in the form of ferric iron. Calculations performed by FactSage with a thermodynamically optimised database have been compared with the experimental results.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Single phase (Zn,Fe)(1-x) O zincite solid solution samples have been prepared by high temperature equilibration in air and in reducing atmospheres, followed by quenching to room temperature. The Fe2+/Fe3+ concentrations in the samples have been determined using wet chemical and XPS techniques. Iron is found to be present in zincite predominantly in the form of Fe3+ ions. The transition from an equiaxed grain morphology to plate-like zincite crystals is shown to be associated with increasing Fe3+ concentration, increasing elongation in < 001 > of the hexagonal crystals and increasing anisotropic strain along the c-axis. The plate-like crystals are shown to contain planar defects and zincite polytypes at high iron concentrations.