37 resultados para Titanium films
em University of Queensland eSpace - Australia
Resumo:
Optically transparent, mesostructured titanium dioxide thin films were fabricated using an amphiphilic poly(alkylene oxide) block copolymer template in combination with retarded hydrolysis of a titanium isopropoxide precursor. Prior to calcination, the films displayed a stable hexagonal mesophase and high refractive indices (1.5 to 1.6) relative to mesostructured silica (1.43). After calcination, the hexagonal mesophase was retained with surface areas >300 m2 g-1. The dye Rhodamine 6G (commonly used as a laser dye) was incorporated into the copolymer micelle during the templating process. In this way, novel dye-doped mesostructured titanium dioxide films were synthesised. The copolymer not only directs the film structure, but also provides a solubilizing environment suitable for sustaining a high monomer-to-aggregate ratio at elevated dye concentrations. The dye-doped films displayed optical thresholdlike behaviour characteristic of amplified spontaneous emission. Soft lithography was successfully applied to micropattern the dye-doped films. These results pave the way for the fabrication and demonstration of novel microlaser structures and other active optical structures. This new, high-refractive index, mesostructured, dye-doped material could also find applications in areas such as optical coatings, displays and integrated photonic devices.
Resumo:
A comparison has been made between the spectroscopic properties of the laser dye rhodamine 6G (R6G) in mesostructured titanium dioxide (TiO2) and in ethanol. Steady-state excitation and emission techniques have been used to probe the dye-matrix interactions. We show that the TiO2-nanocomposite studied is a good host for R6G, as it allows high dye concentrations, while keeping dye molecules isolated, and preventing aggregation. Our findings have important implications in the context of solid state dye-lasers and microphotonic device applications. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Mesostructured titania thin films were prepared by an evaporation-induced self-assembly process. The highly acidic sot precursors contained titanium(IV) tetraisopropoxide (TTIP) as a titanium source, a tri-block copolymer Pluronic P123 as a template, and acetylacetonate and HCl as hydrolysis inhibitors. Characteristics of the resultant titania thin films were studied using X-ray diffraction (XRD) analysis, N-2-adsorption/desorption analysis, and transmission electron microscopy (TEM). XRD and TEM investigations on the as-synthesised films revealed the appearance of cubic-like, pseudohexagonal, and lamellar mesophases; depending on the amount of water in the sols of film precursors. Template removal by a calcination process yields high surface area (320-360 m(2)/g) mesoporous materials with crystalline anatase frameworks. Water content also influences the degree of anatase crystallinity of the calcined films. Higher water content resulted in improved anatase crystallinity. These nanostructured materials are of interest for photocatalysts, pbotoelectrochemical solar cells and other photonic devices. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
Environmental issues due to increases in emissions of air pollutants and greenhouse gases are driving the development of clean energy delivery technologies such as fuel cells. Low temperature Proton Exchange Membrane Fuel Cells (PEMFC) use hydrogen as a fuel and their only emission is water. While significant advances have been made in recent years, a major limitation of the current technology is the cost and materials limitations of the proton conduction membrane. The proton exchange membrane performs three critical functions in the PEMFC membrane electrode assembly (MEA): (i) conduction of protons with minimal resistance from the anode (where they are generated from hydrogen) to the cathode (where they combine with oxygen and electrons, from the external circuit or load), (ii) providing electrical insulation between the anode and cathode to prevent shorting, and (iii) providing a gas impermeable barrier to prevent mixing of the fuel (hydrogen) and oxidant. The PFSA (perfluorosulphonic acid) family of membranes is currently the best developed proton conduction membrane commercially available, but these materials are limited to operation below 100oC (typically 80oC, or lower) due to the thermochemical limitations of this polymer. For both mobile and stationary applications, fuel cell companies require more durable, cost effective membrane technologies capable of delivering enhanced performance at higher temperatures (typically 120oC, or higher. This is driving research into a wide range of novel organic and inorganic materials with the potential to be good proton conductors and form coherent membranes. There are several research efforts recently reported in the literature employing inorganic nanomaterials. These include functionalised silica phosphates [1,2], fullerene [3] titania phosphates [4], zirconium pyrophosphate [5]. This work addresses the functionalisation of titania particles with phosphoric acid. Proton conductivity measurements are given together with structural properties.
Resumo:
We present models for the optical functions of 11 metals used as mirrors and contacts in optoelectronic and optical devices: noble metals (Ag, Au, Cu), aluminum, beryllium, and transition metals (Cr, Ni, Pd, Pt, Ti, W). We used two simple phenomenological models, the Lorentz-Drude (LD) and the Brendel-Bormann (BB), to interpret both the free-electron and the interband parts of the dielectric response of metals in a wide spectral range from 0.1 to 6 eV. Our results show that the BE model was needed to describe appropriately the interband absorption in noble metals, while for Al, Be, and the transition metals both models exhibit good agreement with the experimental data. A comparison with measurements on surface normal structures confirmed that the reflectance and the phase change on reflection from semiconductor-metal interfaces (including the case of metallic multilayers) can be accurately described by use of the proposed models for the optical functions of metallic films and the matrix method for multilayer calculations. (C) 1998 Optical Society of America.
Resumo:
X-Ray diffraction is reported from mesoporous silicate films grown at the air/water interface. The films were studied both as powdered films, and oriented on silicon or mica sheets. At early stages of growth we observe Bragg diffraction from a highly ordered cubic phase, with both long and short d-spacing peaks. We have assigned this as a discontinuous micellar Pm3n phase in which the silica is partly ordered. Later films retain only the known hexagonal p6m peaks and have lost any order both at short d-spacings and the longer d-spacing Bragg peaks characteristic of the cubic structure. The silica framework is considerably expanded from that in bulk amorphous silica, average Si Si distances are some 30% greater. Incorporation of glycerol or polyethylene glycol preserves the earlier cubic structure. To be consistent with earlier, in situ, X-ray and neutron reflectivity data we infer that both structures are produced after a phase transition from a less-ordered him structure late in the induction phase. The structural relations between the film Pm3n and p6m phase(s) and the known bulk SBA-1 and MCM-41 phases are briefly discussed.
Resumo:
We have grown surfactant-templated silicate films at the air-water interface using n-alkyltrimethylammonium bromide and chloride in an acid synthesis with tetraethyl orthosilicate as the silicate source. The films have been grown with and without added salt (sodium chloride, sodium bromide) and with n-alkyl chain lengths from 12 to 18, the growth process being monitored by X-ray reflectometry. Glassy, hexagonal, and lamellar structures have been produced in ways that are predictable from the pure surfactant-water phase diagrams. The synthesis appears to proceed initially through an induction period characterized by the accumulation of silica-coated spherical micelles near the surface. All syntheses, except those involving C(12)TACl, show a sudden transformation of the spherical micellar phase to a hexagonal phase. This occurs when the gradually increasing ionic strength and/or changing ethanol concentration is sufficient to change the position of boundaries within the phase diagram. A possible mechanism for this to occur may be to induce a sphere to rod transition in the micellar structure. This transformation, as predicted from the surfactant-water phase diagram, can be induced by addition of salts and is slower for chloride than bromide counteranions. The hexagonal materials change in cell dimension as the chain length is changed in a way consistent with theoretical model predictions. All the materials have sufficiently flexible silica frameworks that phase interconversion is observed both from glassy to hexagonal and from hexagonal, to lamellar and vice versa in those surfactant systems where multiple phases are found to exist.
Resumo:
TiO2 in anatase crystal phase is a very effective catalyst in the photocatalytic oxidation of organic compounds in water. To improve the recovery rate of TiO2 photocatalysts, which in most cases are in fine powder form, the chemical vapor deposition (CVD) method was used to load TiO2 onto a bigger particle support, silica gel. The amount of titania coating was found to depend strongly on the synthesis parameters of carrier gas flow rate and coating time. XPS and nitrogen ads/desorption results showed that most of the TiO2 particles generated from CVD were distributed on the external surface of the support and the coating was stable. The photocatalytic activities of TiO2/silica gel with different amounts of titania were evaluated for the oxidation of phenol aqueous solution and compared with that of Degussa P25. The optimum titania loading rate was found around 6 wt % of the TiO2 bulk concentration. Although the activity of the best TiO2/silica gel sample was still lower than that of P25, the synthesized TiO2/silica gel catalyst can be easily separated from the treated water and was found to maintain its TiO2 content and catalytic activity.
Resumo:
The mechanism of growth of silicate films at the air/liquid interface has been investigated in situ by a series of grazing incidence diffraction experiments using a 20 x 25 cm(2) imaging plate as the detector. C(18)TAX (X = Br- or Cl-) has been used as the film templating surfactant. The formation of a layered phase, prior to growth of the hexagonal mesophase in C(18)TABr templated films. has been seen. This layered structure has a significantly shorter d spacing compared to the final hexagonal film (43 versus 48 Angstrom, respectively). The correlation lengths associated with the development of the hexagonal in-plane diffraction spots are much longer in-plane than perpendicular to the air/liquid interface (300 Angstrom versus 50 Angstrom). This implies that the film forms via the growth or aggregation of islands that are initially only a micelle or two thick. which then grow down into the solution.
Resumo:
The development of structure perpendicular to and in the plane of the interface has been studied for mesoporous silicate films self-assembled at the air/water interface. The use of constrained X-ray and neutron specular reflectometry has enabled a detailed study of the structural development perpendicular to the interface during the pre-growth phase. Off-specular neutron reflectometry and grazing incidence X-ray diffraction has enabled the in-plane structure to be probed with excellent time resolution. The growth mechanism under the surfactant to silicate source ratios used in this work is clearly due to the self-assembly of micellar and molecular species at the air/liquid interface, resulting in the formation of a planar mesoporous film that is tens of microns thick. (C) 2003 Elsevier Science B.V. All rights reserved.
Resumo:
Langmuir and Langmuir-Blodgett (LB) films of a cationic amphiphilic porphyrin mixed with n-alkanes octadecane and hexatriacontane were prepared and characterized, to examine the influence of the alkanes on film structure and stability. While the structure present in these films was controlled primarily by the porphyrin, the addition of the alkanes resulted in significant changes to both the phase behavior of the Langmuir films and the molecular arrangement of the LB films. These changes, as well as the observed chain length effects, are explained in terms of the intermolecular interactions present in the films.
Resumo:
Simple equations are proposed for determining elastic modulus and hardness properties of thin films on substrates from nanoindentation experiments. An empirical formulation relates the modulus E and hardness H of the film/substrate bilayer to corresponding material properties of the constituent materials via a power-law relation. Geometrical dependence of E and H is wholly contained in the power-law exponents, expressed here as sigmoidal functions of indenter penetration relative to film thickness. The formulation may be inverted to enable deconvolution of film properties from data on the film/substrate bilayers. Berkovich nanoindentation data for dense oxide and nitride films on silicon substrates are used to validate the equations and to demonstrate the film property deconvolution. Additional data for less dense nitride films are used to illustrate the extent to which film properties may depend on the method of fabrication.
Resumo:
This paper reports an investigation on techniques for determining elastic modulus and intrinsic stress gradient in plasma-enhanced chemical vapor deposition (PECVD) silicon nitride thin films. The elastic property of the silicon nitride thin films was determined using the nanoindentation method on silicon nitride/silicon bilayer systems. A simple empirical formula was developed to deconvolute the film elastic modulus. The intrinsic stress gradient in the films was determined by using micrometric cantilever beams, cross-membrane structures and mechanical simulation. The deflections of the silicon nitride thin film cantilever beams and cross-membranes caused by in-thickness stress gradients were measured using optical interference microscopy. Finite-element beam models were built to compute the deflection induced by the stress gradient. Matching the deflection computed under a given gradient with that measured experimentally on fabricated samples allows the stress gradient of the PECVD silicon nitride thin films introduced from the fabrication process to be evaluated.
Resumo:
An experimental investigation of mechanical properties of thin films using nanoindentation was reported. Silicon nitride thin films with different thicknesses were deposited using plasma enhanced chemical vapor deposition (PECVD) on Si substrate. Nanoindentation was used to measure their elastic modulus and hardness. The results indicated that for a film/substrate bilayer system, the measured mechanical properties are significantly affected by the substrate properties. Empirical formulas were proposed for deconvoluting the film properties from the measured bilayer properties.
Resumo:
The 4-carboxyphenyl-appended macrocyclic ligand trans-6,13-dimethyl-6-((4-carboxybenzyl)amino)-1,4,8,11-tetraazacyclotetradecane-6-amine (HL10) has been synthesised and complexed with Co-III. The mononuclear complexes [Co(HL10)(CN)](2+) and [CoL10(OH)](+) have been prepared and the crystal structures of their perchlorate salts are presented, where the ligand is bound in a pentadentate mode in each case while the 4-carboxybenzyl-substituted pendent amine remains free from the metal. The cyano-bridged dinuclear complex [CoL10-mu-NC-Fe(CN)(5)](2-) was also prepared and chemisorbed on titania-coated ITO conducting glass. The adsorbed complex is electrochemically active and cyclic voltammetry of the modified ITO working electrode in both water and MeCN solution was undertaken with simultaneous optical spectroscopy. This experiment demonstrates that reversible electrochemical oxidation of the Fe-II centre is coupled with rapid changes in the optical absorbance of the film.