A magnesium alloy of eutectic composition (33 wt-'%Al) was directionally solidified in mild steel tubes at two growth rates, 32 and 580 mum s(-1,) in a temperature gradient between 10 and 20 K mm(-1). After directional solidification, the composition of each specimen varied dramatically, from 32'%Al in the region that had remained solid to 18%Al (32 mum s(-1) specimen) and 13%Al (580 mum s(-1) specimen) at the plane that had been quenched from the eutectic temperature. As the aluminium content decreased, the microstructure contained an increasing volume fraction of primary magnesium dendrites and the eutectic morphology gradually changed from lamellar to partially divorced. The reduction in aluminium content was caused by the growth of an Al-Fe phase ahead of the Mg-Al growth front. Most of the growth of the Al-Fe phase occurred during the remelting period before directional solidification. The thickness of the Al-Fe phase increased with increased temperature and time of contact with the molten Mg-Al alloy. (C) 2003 Maney Publishing.
Resumo:
Due to the complexities involved with measuring activated sludge floc size distributions, this parameter has largely been ignored by wastewater researchers and practitioners. One of the major reasons has been that instruments able to measure particle size distributions were complex, expensive and only provided off-line measurements. The Focused Beam Reflectance Method (FBRM) is one of the rare techniques able to measure the particle size distribution in situ. This paper introduces the technique for monitoring wastewater treatment systems and compares its performance with other sizing techniques. The issue of the optimal focal point is discussed, and similar conclusions as found in the literature for other particulate systems are drawn. The study also demonstrates the capabilities of the FBRM in evaluating the performance of settling tanks. Interestingly, the floc size distributions did not vary with position inside the settling tank flocculator. This was an unexpected finding, and seriously questioned the need for a flocculator in the settling tank. It is conjectured that the invariable size distributions were caused by the unique combination of high solids concentration, low shear and zeolite dosing. (C) 2004 Society of Chemical Industry.