Miscibility and phase separation in the blends of phenolphthalein poly(aryl ether ketone) (PPAEK) and poly(ethylene oxide) (PEO) were investigated by means of differential scanning calorimetry (DSC). The PPAEK/PEO blends prepared by solution casting from N,N-dimethylformamide (DMF) displayed single composition-dependent glass transition temperatures (T-g), intermediate between those of the pure components, suggesting that the blend system is miscible in the amorphous state at all compositions. All the blends underwent phase separation at higher temperatures and the system exhibited a lower critical solution temperature (LCST) behavior. A step-heating thermal analysis was designed to determine the phase boundaries with DSC. The significant changes in the thermal properties of blends were utilized to judge the mixing status for the blends and the phase diagram was thus established. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Thermosetting blends of an aliphatic epoxy resin and a hydroxyl-functionalized hyperbranched polymer (HBP), aliphatic hyperbranched polyester Boltorn H40, were prepared using 4,4'-diaminodiphenylmethane (DDM) as the curing agent. The phase behavior and morphology of the DDM-cured epoxy/HBP blends with HBP content up to 40 wt% were investigated by differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA), and scanning electron microscopy (SEM). The cured epoxy/HBP blends are immiscible and exhibit two separate glass transitions, as revealed by DMA. The SEM observation showed that there exist two phases in the cured blends, which is an epoxy-rich phase and an HBP-rich phase, which is responsible for the two separate glass transitions. The phase morphology was observed to be dependent on the blend composition. For the blends with HBP content up to 10 wt%, discrete HBP domains are dispersed in the continuous cured epoxy matrix, whereas the cured blend with 40 wt% HBP exhibits a combined morphology of connected globules and bicominuous phase structure. Porous epoxy thermosets with continuous open structures on the order of 100-300 nm were formed after the HBP-rich phase was extracted with solvent from the cured blend with 40 wt% HBP. The DSC study showed that the curing rate is not obviously affected in the epoxy/HBP blends with HBP content up to 40 wt %. The activation energy values obtained are not remarkably changed in the blends; the addition of HBP to epoxy resin thus does not change the mechanism of cure reaction of epoxy resin with DDM. (c) 2006 Wiley Periodicals, Inc.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

We show that the simple quasi-static technique, also called the adiabatic mapping technique, can be used to determine the energetics of rotation of methyl and methoxy groups in amorphous poly(vinyl methyl ether) even though the latter process is too slow to be amenable to direct molecular dynamics simulation. For the methyl group rotation, we find that the mean and standard deviation of the simulated rotational barrier heights agree well with experimental data from quasi-elastic neutron scattering. In the case of the methoxy groups we find that just 4% of the groups contribute more than 90% of the observed dielectric relaxation strength. The groups which make the most contribution are those which, by virtue of their particular conformation and local environment, have two alternative positions of similar energy.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Thermosetting blends of a biodegradable poly(ethylene glycol)-type epoxy resin (PEG-ER) and poly(epsilon-caprolactone) (PCL) were prepared via an in situ curing reaction of poly(ethylene glycol) diglycidyl ether (PEGDGE) and maleic anhydride (MAH) in the presence of PCL. The miscibility, phase behavior, crystallization, and morphology of these blends were investigated. The uncured PCL/PEGDGE blends were miscible, mainly because of the entropic contribution, as the molecular weight of PEGDGE was very low. The crystallization and melting behavior of both PCL and the poly(ethylene glycol) (PEG) segment of PEGDGE were less affected in the uncured PCL/PEGDGE blends because of the very close glass-transition temperatures of PCL and PEGDGE. However, the cured PCL/PEG-ER blends were immiscible and exhibited two separate glass transitions, as revealed by differential scanning calorimetry and dynamic mechanical analysis. There existed two phases in the cured PCL/PEG-ER blends, that is, a PCL-rich phase and a PEG-ER crosslinked phase composed of an MAH-cured PEGDGE network. The crystallization of PCL was slightly enhanced in the cured blends because of the phase-separated nature; meanwhile, the PEG segment was highly restricted in the crosslinked network and was noncrystallizable in the cured blends. The phase structure and morphology of the cured PCL/PEG-ER blends were examined with scanning electron microscopy; a variety of phase morphologies were observed that depended on the blend composition. (C) 2004 Wiley Periodicals, Inc.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

preparation of liposomes, as a new, continuous and potentially scaleable method for the preparation of ISCOMs. Phosphatidylcholine (PC) and cholesterol (Chol) were dissolved in ether, which was injected into an aqueous solution, maintained at 55 degrees C, containing Quil A. The influences of the following variables on ISCOM formation were investigated: ratio of PC:Quil A:Chol used, pumping rate, total lipid mass and concentration of buffer salts and Quil A in the aqueous phase. All samples were characterized by negative stain transmission electron microscopy, photon correlation spectroscopy and sucrose ultracentrifugation gradient. It was demonstrated that ISCOMs could be produced by this method but the homogeneity of the preparation was influenced by the conditions used. Homogeneous ISCOM preparations were consistently produced only when the weight ratio of PC:Quil A:Chol was 5:3:2 with a total lipid mass of 20 mg, the Quil A dissolved in a 0.01 M phosphate buffer at a concentration of 6 mg in 4 ml, and the ether solution injected into the warmed buffer solution at a rate of 0.2 ml/min. Changing any of these variables resulted in more heterogeneous preparations in which ISCOMs typically co-existed with other colloidal structures such as worm-like and helical micelles, liposomes, lamellae and lipidic particles. (C) 2005 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The chemical structure, synthesis, morphology, and properties of polyurethane elastomers are briefly discussed. The current understanding of the effect of chemical structure and the associated morphology on the stability of polyurethanes in the biological environments is reviewed. The degradation of conventional polyurethanes appears as surface or deep cracking, stiffening, and deterioration of mechanical properties, such as flex-fatigue resistance. Polyester and poly( tetramethylene oxide) based polyurethanes degrade by hydrolytic and oxidative degradation of ester and ether functional groups, respectively. The recent approaches to develop polyurethanes with improved long-term biostability are based on developing novel polyether, hydrocarbon, polycarbonate, and siloxane macrodiols to replace degradation-prone polyester and polyether macrodiols in polyurethane formulations. The new approaches are discussed with respect to synthesis, properties and biostability based on reported in vivo studies. Among the newly developed materials, siloxane-based polyurethanes have exhibited excellent biostability and are expected to find many applications in biomedical implants.