The thickness, chemical composition and microstructure of anodised coatings formed on magnesium alloy AZ91D at various anodising current densities were measured. It was found that all these parameters could be affected by anodising current density, and hence the coatings formed at different anodising current densities had different corrosion resistances. This suggests that the corrosion performance of an anodised coating could be improved if a properly designed current waveform is used for anodising. In addition, based on the experimental results, some physical, chemical and electrochemical reactions involved in the anodising process were proposed to explain the anodising behaviour in this paper. (c) 2005 Elsevier Ltd. All rights reserved.
Resumo:
This work studied the effect of the impurity iron and the alloying elements aluminium and zinc in single-phase substrate magnesium alloys on the corrosion resistance of the alloys after anodisation. It was found that increasing zinc content (0-2%) led to increased corrosion resistance of an anodised single-phase Mg-Zn alloy. The addition of Al lowered the corrosion resistance of an anodised commercial purity Mg-Al single-phase alloy, whereas the same addition was found to be beneficial to the corrosion resistance of an anodised high purity Mg-Al single-phase alloy. Heat-treatment made the substrate Mg-Al and Mg-Zn alloys more uniform and hence improved the corrosion resistance of the alloys after anodisation. The detrimental effect of iron impurity on corrosion performance of the unanodised substrate single-phase magnesium alloys was inherited by the anodised alloys. The corrosion resistance of the anodised Mg alloys was found to be closely correlated with the corrosion performance of the unanodised as-cast Mg alloys. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
This paper reviews various aspects of anodizing of magnesium alloys, such as the basics, processes, properties and applications. It systematically summarises the existing fundamental studies and technical developments of anodizing of magnesium alloys, and concludes that new anodizing processes based on electrolytic plasma anodizing that convert the surface of a magnesium alloy into a hard ceramic coating in an electrolytic bath using high energy electric discharges can offer improved wear and corrosion resistance. These new anodized coatings are often claimed to perform better than the traditional ones obtained through older anodizing processes, such as DOW17 or HAE. The new anodizing techniques are chromate free and hence environment friendly. It is expected that more cost-effective, environment-friendly and non-toxic anodizing techniques will be developed and applied to magnesium alloy components in the future.
Resumo:
The corrosion performance of anodised magnesium and its alloys, such as commercial purity magnesium (CP-Mg) and high-purity magnesium (HP-Mg) ingots, magnesium alloy ingots of MEZ, ZE41, AM60 and AZ91D and diecast AM60 (AM60-DC) and AZ91D (AZ91D-DC) plates, was evaluated by salt spray and salt immersion testing. The corrosion resistance was in the sequential order: AZ91D approximate to AM60 approximate to MEZ >= AZ91D-DC >= AM60-DC > HP-Mg > ZE41 > CP-Mg. It was concluded the corrosion resistance of an anodised magnesium alloy was determined by the corrosion performance of the substrate alloy due to the porous coating formed on the substrate alloy acting as a simple corrosion barrier. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Although monomeric Al species are often toxic in acidic soils, the effects of the aluminate ion (Al(OH)4-) on roots grown in alkaline media are still unclear. Dilute, alkaline (pH 9.5) nutrient solutions were used to investigate the effects of Al(OH)4- on root growth of mungbean (Vigna radiata L.). Root growth was reduced by 13 % after 3 d growth in solutions with an Al(OH)4- activity of 16 μM and no detectable polycationic Al (Al13). This decrease in root growth was associated with the formation of lesions on the root tips (due to the rupturing of the epidermal and outer cortical cells) and a slight limitation to root hair growth (particularly on the lateral roots). When roots displaying these symptoms were transferred to fresh Al(OH)4- solutions for a further 12 h, no root tip lesions were observed and root hair growth on the lateral roots improved. The symptoms were similar to those induced by Al13 at concentrations as low as 0.50 μM Al which are below the detection limit of the ferron method. Thus, Al(OH)4- is considered to be non-toxic, with the observed reduction in root growth in solutions containing Al(OH)4- due to the gradual formation of toxic Al13 in the bulk nutrient solution resulting from the acidification of the alkaline nutrient solution by the plant roots.
Resumo:
We investigate the effect of the coefficient of the critical nonlinearity for the Neumann problem on the existence of least energy solutions. As a by-product we establish a Sobolev inequality with interior norm.
Resumo:
We give conditions on f involving pairs of lower and upper solutions which lead to the existence of at least three solutions of the two point boundary value problem y" + f(x, y, y') = 0, x epsilon [0, 1], y(0) = 0 = y(1). In the special case f(x, y, y') = f(y) greater than or equal to 0 we give growth conditions on f and apply our general result to show the existence of three positive solutions. We give an example showing this latter result is sharp. Our results extend those of Avery and of Lakshmikantham et al.
Resumo:
We are concerned with determining values of, for which there exist nodal solutions of the boundary value problems u" + ra(t) f(u) = 0, 0 < t < 1, u(O) = u(1) = 0. The proof of our main result is based upon bifurcation techniques.
Resumo:
In this paper we extend the guiding function approach to show that there are periodic or bounded solutions for first order systems of ordinary differential equations of the form x1 =f(t,x), a.e. epsilon[a,b], where f satisfies the Caratheodory conditions. Our results generalize recent ones of Mawhin and Ward.
Resumo:
Simple techniques are presented for rearrangement of an infinite series in a systematic way such that the convergence of the resulting expression is accelerated. These procedures also allow calculation of required boundary derivatives. Several examples of conduction and diffusion-reaction problems illustrate the methods.
Resumo:
Transient response of a CSTR containing porous catalyst pellets is analyzed theoretically using a matched asymptotic expansion technique. This singular perturbation technique leads directly to the conditions under which the minima of reservoir concentration occur. The existence of the minima may be used to estimate some inherent parameters of the catalyst pellet.
Resumo:
Using a novel finite integral transform technique, the problem of diffusion and chemical reaction in a porous catalyst with general activity profile is investigated theoretically. Analytical expressions for the effectiveness factor are obtained for pth order and Michaelis-Menten kinetics. Perturbation methods are employed to provide useful asymptotic solutions for large or small values of Thiele modulus and Biot number.
Resumo:
Flexible transport services (FTS) have been of increasing interest in developed countries as a bridge between the use of personal car travel and fixed route transit services. This paper reports on findings from a recent study in Queensland Australia, which identified lessons from an international review and implications for Australia. Potential strategic directions, including a vision, mission, key result areas, strategies, and identified means of measuring performance are described. Evaluation criteria for assessing flexible transport proposals were developed, and approaches to identifying and assessing needs and demands outlined. The use of emerging technologies is also a key element of successful flexible transport services.
Resumo:
Little is known about factors effecting plant growth at high pH, with research often limited by the inability to separate nutritional deficiencies and HCO3- toxicity from the direct limitations imposed under high pH conditions. Various methods of controlling dilute nutrient solutions for studies at high pH were investigated. For short-term studies, it was found that a solution without Cu, Fe, Mn and Zn and aerated with CO2 depleted air, greatly reduced nutrient precipitation at high pH, thus eliminating nutritional differences between treatments. Manual pH adjustment and the use of ion exchange resins as pH buffers were unsuitable methods of pH control. However, pH control by automated titration had little effect on solution composition while maintaining constant pH. The system described is suitable for studies in which the pH of the bulk nutrient solution must be maintained. The system was used to examine OH- toxicity in mungbeans (Vigna radiata (L.) Wilczek cv. Emerald), with root length reduced at a bulk solution pH of 8.5 and greater.
Resumo:
The electrochemical behaviour of magnesium was studied in representative chloride and sulphate solutions including NaCl, Na2SO4, NaOH and their mixed solutions, HCl, and H2SO4: (1) by measuring electrochemical polarisation curves, (2) by using electrochemical impedance spectroscopy (EIS), and (3) by simultaneous measurement of hydrogen gas evolution and measurement of magnesium dissolution rates using inductively coupled plasma atomic emission spectrophotometry (ICPEAS). These experiments showed that a partially protective surface film played an important role in the dissolution of magnesium in chloride and sulphate solutions. Furthermore, the experimental data were consistent with the involvement of the intermediate species Mg+ in magnesium dissolution at film imperfections or on a film-free surface. At such sites, magnesium first oxidised electrochemically to the intermediate species Mg+, and then the intermediate species chemically reacted with water to produce hydrogen and Mg2+. The presence of Cl- ions increased the film free area, and accelerated the electrochemical reaction rate from magnesium metal to Mg+. (C) 1997 Elsevier Science Ltd.