210 resultados para Crystallographic crack growth

em University of Queensland eSpace - Australia


Relevância:

90.00% 90.00%

Publicador:

Resumo:

This paper presents the recent finding by Muhlhaus et al [1] that bifurcation of crack growth patterns exists for arrays of two-dimensional cracks. This bifurcation is a result of the nonlinear effect due to crack interaction, which is, in the present analysis, approximated by the dipole asymptotic or pseudo-traction method. The nonlinear parameter for the problem is the crack length/ spacing ratio lambda = a/h. For parallel and edge crack arrays under far field tension, uniform crack growth patterns (all cracks having same size) yield to nonuniform crack growth patterns (i.e. bifurcation) if lambda is larger than a critical value lambda(cr) (note that such bifurcation is not found for collinear crack arrays). For parallel and edge crack arrays respectively, the value of lambda(cr) decreases monotonically from (2/9)(1/2) and (2/15.096)(1/2) for arrays of 2 cracks, to (2/3)(1/2)/pi and (2/5.032)(1/2)/pi for infinite arrays of cracks. The critical parameter lambda(cr) is calculated numerically for arrays of up to 100 cracks, whilst discrete Fourier transform is used to obtain the exact solution of lambda(cr) for infinite crack arrays. For geomaterials, bifurcation can also occurs when array of sliding cracks are under compression.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

This paper reviews the current knowledge and understanding of martensitic transformations in ceramics - the tetragonal to monoclinic transformation in zirconia in particular. This martensitic transformation is the key to transformation toughening in zirconia ceramics. A very considerable body of experimental data on the characteristics of this transformation is now available. In addition, theoretical predictions can be made using the phenomenological theory of martensitic transformations. As the paper will illustrate, the phenomenological theory is capable of explaining all the reported microstructural and crystallographic features of the transformation in zirconia and in some other ceramic systems. Hence the theory, supported by experiment, can be used with considerable confidence to provide the quantitative data that is essential for developing a credible, comprehensive understanding of the transformation toughening process. A critical feature in transformation toughening is the shape strain that accompanies the transformation. This shape strain, or nucleation strain, determines whether or not the stress-induced martensitic transformation can occur at the tip of a potentially dangerous crack. If transformation does take place, then it is the net transformation strain left behind in the transformed region that provides toughening by hindering crack growth. The fracture mechanics based models for transformation toughening, therefore, depend on having a full understanding of the characteristics of the martensitic transformation and, in particular, on being able to specify both these strains. A review of the development of the models for transformation toughening shows that their refinement and improvement over the last couple of decades has been largely a result of the inclusion of more of the characteristics of the stress-induced martensitic transformation. The paper advances an improved model for the stress-induced martensitic transformation and the strains resulting from the transformation. This model, which separates the nucleation strain from the subsequent net transformation strain, is shown to be superior to any of the constitutive models currently available. (C) 2002 Elsevier Science Ltd. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

This paper reports on measurements of crack growth by environmental assisted fracture (EAF) for 4340 steel in water and in air at various relative humidities. Of most interest is the observation of slow crack propagation in dry air. Fractographic analysis leads to the strong suggestion that this slow crack propagation is due to hydrogen cracking caused by internal hydrogen in solid solution inside the sample material.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Stress corrosion cracks (SCC) had been found in a natural gas transmission pipeline during a dig-up and inspection program. The question was raised as to whether the SCC was active or dormant. This paper describes the resultant investigation to determine if a particular service crack was actively growing. The strategy adopted was to assess the appearance of the fracture surface of the service crack and to compare with expectations from laboratory specimens with active SCC. The conclusions from this study are as follows. To judge whether a crack in the service pipe is active or dormant, it is reasonable to compare the very crack tip of the service crack and a fresh crack in a laboratory sample. If the crack tip of the active laboratory sample is similar to that of the service pipe, it means the crack in the service pipe is likely to be active. From the comparison of the crack tip between the service pipe and the laboratory samples, it appears likely that the cracks in the samples extracted from service were most likely to have been active intergranular stress corrosion cracks. (C) 2003 Elsevier Ltd. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The addition of small quantities (similar to 5 wt pct) layered silicates into polymer materials has the potential to greatly increase the modulus without adversely affecting the toughness or processability of the composite. The effect of microstructural features in the polymer nanocomposite and their possible effects on the mechanical properties with particular reference to linear low density polyethylene (LLDPE)/montmorillonite nanocomposites was discussed.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

While the general mechanisms of hot tearing are understood, i.e. the inability of liquid to feed imposed strain on the mushy material, work continues on improving the understanding of the mechanisms at play. A hot tear test rig that measures the temperature and load imposed on the mushy zone during solidification has been successfully used to study hot tearing. The mould has now been modified to incorporate a window above the hot spot region to allow observation of hot tear formation and growth. Combining information from visual observation with load and temperature data has led to a better understanding of the mechanism of hot tearing. Tests were carried out on an Al-0.5 wt-% Cu alloy. It was found that load development began at about 90% solid and a hot tear formed a short time later, at between 93% and 96% solid. Hot tearing started at a very low load.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Many potential applications for sintered aluminium are limited by the poor fatigue properties of the material. In order to increase understanding of the fatigue mechanisms in sintered aluminium, fatigue tests were carried out on a sintered 2xxx series aluminium alloy, AMB-2712. The alloy has a fatigue endurance strength of approximately 145 MPa (R = 0.1). Three regions were identified on the fatigue fracture surfaces. Region I contains the initiation site and transgranular crack propagation. When the size of the cyclic plastic zone ahead of the crack becomes comparable to the grain size, microstructural damage at the crack tip results in a transition to intergranular propagation. Region 2 mainly contains intergranularly fractured material, whilst the final fracture area makes up Region 3, in the form of dimple coalescence and intergranular failure. Transgranular fractographic features observed on fatigued specimens include fissure-type striations, cross-hatched grains, furrowed grains and grains containing step-like features. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The level set method has been implemented in a computational volcanology context. New techniques are presented to solve the advection equation and the reinitialisation equation. These techniques are based upon an algorithm developed in the finite difference context, but are modified to take advantage of the robustness of the finite element method. The resulting algorithm is tested on a well documented Rayleigh–Taylor instability benchmark [19], and on an axisymmetric problem where the analytical solution is known. Finally, the algorithm is applied to a basic study of lava dome growth.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Copper concentrate (chalcopyrite) was granulated in a rotating drum with a diameter of 0.3 m and a length of 0.2 m. Water was used as the binder and it was sprayed onto the powder bed with a nozzle. This material exhibited induction type behaviour, which was defined by Iveson and Litster [AIChE J. 44 (1998) 1510]. Induction type behaviour is characterized by the occurrence of an induction stage, during which the granules are gradually being compacted and little or no growth occurs. At the end of this induction stage, binder liquid is squeezed from the interior of the granules onto the granule surface and the granules are then surface-wet. This results in a rapid growth rate of the granules. Different types of experiments were conducted. The influence of the nozzle pressure and the distance from the nozzle to the powder bed on the growth behaviour of the granules as well as on the binder distribution was examined. The results of these experiments led to the postulation of a modified mechanism for induction type behaviour: it was found that after the binder was delivered, there were large granules containing a high amount of binder and small granules containing less binder. During the induction stage, the granules are compacted and binder liquid continuously appears at the surface of the large granules. These wet spots that are continuously being formed pick up the dry and small granules. When all the small granules have been picked up, further expulsion of binder liquid onto the granules' surface results in granules that remain surface-wet. This phenomenon marks the end of the induction stage and it coincides with the disappearance of the small granules. The hypothesis was tested by selectively removing the smaller granules during an experiment. As expected, this resulted in a shorter induction time.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

[beta]-Hydroxy [beta]-methylbutyrate (HMB), a metabolite of the essential amino acid leucine, is one of the latest dietary supplements promoted to enhance gains in strength and lean body mass associated with resistance training. Unlike anabolic hormones that induce muscle hypertrophy by increasing muscle protein synthesis, HMB is claimed to influence strength and lean body mass by acting as an anticatabolic agent, minimising protein breakdown and damage to cells that may occur with intense exercise. Research on HMB has recently tested this hypothesis, under the assumption that it may be the active compound associated with the anticatabolic effects of leucine and its metabolites. While much of the available literature is preliminary in nature and not without methodological concern, there is support for the claims made regarding HMB supplementation, at least in young, previously untrained individuals. A mechanism by which this may occur is unknown, but research undertaken to date suggests there may be a reduction in skeletal muscle damage, although this has not been assessed directly. The response of resistance trained and older individuals to HMB administration is less clear. While the results of research conducted to date appear encouraging, caution must be taken when interpreting outcomes as most manuscripts are presented in abstract form only, not having to withstand the rigors of peer review. Of the literature reviewed relating to HMB administration during resistance training, only 2 papers are full manuscripts appearing in peer reviewed journals. The remaining 8 papers are published as abstracts only, making it difficult to critically review the research. There is clearly a need for more tightly controlled, longer duration studies to verify if HMB enhances strength and muscular hypertrophy development associated with resistance training across a range of groups, including resistance trained individuals.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report on a quantitative study of the growth process of 87Rb Bose-Einstein condensates. By continuous evaporative cooling we directly control the thermal cloud from which the condensate grows. We compare the experimental data with the results of a theoretical model based on quantum kinetic theory. We find quantitative agreement with theory for the situation of strong cooling, whereas in the weak cooling regime a distinctly different behavior is found in the experiment.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Modeling volcanic phenomena is complicated by free-surfaces often supporting large rheological gradients. Analytical solutions and analogue models provide explanations for fundamental characteristics of lava flows. But more sophisticated models are needed, incorporating improved physics and rheology to capture realistic events. To advance our understanding of the flow dynamics of highly viscous lava in Peléean lava dome formation, axi-symmetrical Finite Element Method (FEM) models of generic endogenous dome growth have been developed. We use a novel technique, the level-set method, which tracks a moving interface, leaving the mesh unaltered. The model equations are formulated in an Eulerian framework. In this paper we test the quality of this technique in our numerical scheme by considering existing analytical and experimental models of lava dome growth which assume a constant Newtonian viscosity. We then compare our model against analytical solutions for real lava domes extruded on Soufrière, St. Vincent, W.I. in 1979 and Mount St. Helens, USA in October 1980 using an effective viscosity. The level-set method is found to be computationally light and robust enough to model the free-surface of a growing lava dome. Also, by modeling the extruded lava with a constant pressure head this naturally results in a drop in extrusion rate with increasing dome height, which can explain lava dome growth observables more appropriately than when using a fixed extrusion rate. From the modeling point of view, the level-set method will ultimately provide an opportunity to capture more of the physics while benefiting from the numerical robustness of regular grids.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Accurate determination of the rhizotoxicity of Cu in dilute nutrient solutions is hindered by the difficulty of maintaining constant, pre-determined concentrations of Cu (micromolar) in solution. The critical Cu2+ activity associated with a reduction in the growth of solution-grown cowpea (Vigna unguiculata (L.) Walp. cv Caloona) was determined in a system in which Cu was maintained constant through the use of a cation exchange resin. The growth of roots and shoots was found to be reduced at solution Cu2+ activities ≥ 1.7 µM (corresponding to 90 % maximum growth). Although root growth was most likely reduced due to a direct Cu2+ toxicity, it is considered that the shoot growth reduction is attributable to a decrease in tissue concentrations of K, Ca, Mg, and Fe and the formation of interveinal chlorosis. At high Cu2+ activities, roots were brown in color, short and thick, had bent root tips with cracking of the epidermis and outer cortex, and had local swellings behind the roots tips due to a reduction in cell elongation. Root hair growth was reduced at concentrations lower than that which caused a significant reduction in overall root fresh weight.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Although the effect of salinity on plant growth has been the focus of a substantive research effort, much of this research has failed to adequately separate the various growth limiting aspects of salinity; thus the results are confounded by multiple factors. Eight perennial grass species were grown in a sand culture system dominated by NaCl (electrical conductivities (ECs) between 1.4 and 38 dS m 1), with sufficient Ca added to each treatment to ensure that Na-induced Ca deficiency did not reduce growth. Of the eight perennial grass species examined, Chloris gayana cv. Pioneer (Rhodes grass) was the most salt tolerant species, whilst in comparison, Chrysopogon zizanioides cv. Monto (vetiver) was of only moderate tolerance. However, observed salinity tolerances tended to be lower than those expected from published values based on the threshold salinity model (bent stick model). This discrepancy may be due in part to differences in the evapotranspirational demand between studies; an increase in demand accelerating the accumulation of Na in the shoots and hence decreasing apparent salinity tolerance. It was also observed that the use of a non-saline growth period to allow seed germination and establishment results in the overestimation of vegetative salinity tolerance if not taken into consideration. This is particularly true for species of low salt tolerance due to their comparatively rapid growth in the non-saline medium compared to that at full salinity.