2 resultados para 310-M0023A
em University of Queensland eSpace - Australia
Resumo:
Magnetic resonance imaging has been used to monitor the diffusion of water at 310 K into a series of semi-IPNs of poly(ethyl methacrylate), PEM, and copolymers of 2-hydroxyethyl methacrylate, HEMA, and tetrahydrofurfuryl methacrylate, THFMA. The diffusion was found to be well described by a Fickian kinetic model in the early stages of the water sorption process, and the diffusion coefficients were found to be slightly smaller than those for the copolymers of HEMA and THFMA, P(HEMA-co-THFMA), containing the same mole fraction of HEMA in the matrix. A second stage sorption process was identified in the later stage of water sorption by the PEM/PTHFMA semi-IPN and for the systems containing a P(HEMA-co-THFMA) component with a mole fraction HEMA of 0.6 or less. This was characterized by the presence of Water near the surface of the cylinders with a longer NMR T-2 relaxation time, which would be characteristic of mobile water, such as water present in large pores or surface fissures. The presence of the drug chlorhexidine in the polymer matrixes at a concentration of 5.625 wt % was found not to modify the properties significantly, but the diffusion coefficients for the water sorption were systematically smaller when the drug was present.
Resumo:
The ingress of water into copolymers of 2-hydroxyethyl methacrylate (HEMA) and tetrahydrofurfuryl methacrylate (THFMA) loaded with either one of two model drugs, ie vitamin B-12 or aspirin, was studied at 310 K using three-dimensional nuclear magnetic resonance (3D NMR) imaging. The poly(HEMA) was loaded with 5 wt% of the drugs. From the imaging profiles it was observed that incorporation of vitamin B-12 into the polymers rich in HEMA resulted in crack formation at the interface between the rubbery region and the glassy core on sorption of water, although these cracks were 'healed' behind the diffusion front. However, for the copolymers with low HEMA contents and for those containing aspirin, no evidence for similar crack formation was found. For the copolymers loaded with 5 wt% of aspirin or vitamin B-12 the values of the water diffusion coefficients, determined by curve-fitting the relative water concentration profiles from magnetic resonance imaging (MRI) measurements, were found to be smaller than those obtained from a mass uptake study. (C) 2004 Society of Chemical Industry.