Resumo:
In Australia people aged 65 years or older currently comprise 12.1% of the population. This has been estimated to rise to 24.2% by 2051. Until recently there has been relatively little research on alcohol and other drug use disorders among these individuals but, given the ageing population, this issue is likely to become of increasing importance and prominence. Epidemiological research shows a strong age-related decline in the prevalence of alcohol and other drug use disorders with age. Possible reasons for this include: age-related declines in the use and misuse of alcohol and other drugs; increased mortality among those with a lifetime history of alcohol and other drug use disorders; historical differences in exposure to and use of alcohol and other drugs. Despite the age-related decline in the prevalence of these disorders, they do still occur among those aged 65 years or older and, given historical changes in exposure to and use of illicit drugs, it likely that the prevalence of these disorders among older-aged individuals will rise. Specific issues faced by older-aged individuals with alcohol and other drug use problems are discussed. These include: interactions with prescribed medications, under-recognition and treatment of alcohol and drug problems, unintentional injury and social isolation. Finally, a brief discussion of treatment issues is provided.
Resumo:
The consumption of excess alcohol in patients with liver iron storage diseases, in particular the iron-overload disease hereditary haemochromatosis (HH), has important clinical consequences. HH, a common genetic disorder amongst people of European descent, results in a slow, progressive accumulation of excess hepatic iron. If left untreated, the condition may lead to fibrosis, cirrhosis and primary hepatocellular carcinoma. The consumption of excess alcohol remains an important cause of hepatic cirrhosis and alcohol consumption itself may lead to altered iron homeostasis. Both alcohol and iron independently have been shown to result in increased oxidative stress causing lipid peroxidation and tissue damage. Therefore, the added effects of both toxins may exacerbate the pathogenesis of disease and impose an increased risk of cirrhosis. This review discusses the concomitant effects of alcohol and iron on the pathogenesis of liver disease. We also discuss the implications of co-existent alcohol and iron in end-stage liver disease.
Resumo:
The radiation chemistry of PCTFE at different temperatures has been studied. The polymer was irradiated under vacuum to absorbed doses of up to 1500 kGy. Three irradiation temperatures were chosen. These included ambient temperature, a temperature well above the T, and a temperature above the crystalline melting temperature. These were 298, 423 and 493 K, respectively. The formation of new structures was identified by solid-state FTIR and F-19 NMR. No branching was observed below the melting temperature, but branches were observed above the melting temperature. G-values for chain-end formation were 1.5 and 2.4 at room temperature and 423 K, respectively and the G-value for the formation of double bonds was found to be < 0.1. For the irradiations at 493 K, the G-values for the formation of chain ends, double bonds and branching points were 3.6, 0.2 and 0.5, respectively. The presence of long-chain branches within the polymer structure could not be proven for radiolysis at 493 K, but scission predominates and network formation does not occur upon irradiation. DSC studies of the polymers irradiated at ambient temperature were consistent with chain scission leading to an increase in the percentage crystallinity, as observed for other fluoropolymers. (C) 2003 Elsevier Science Ltd. All rights reserved.
Resumo:
The radicals formed on gamma-radiolysis of a series of copolymers of methacrylic acid and acrylonitrile have been investigated by ESR spectroscopy. This series of copolymers spanned the full composition range and the study was carried out at 77 K and ambient temperature. The radicals formed in the copolymers at 77 and 303 K were found to be similar to those found in the two homopolymers, but in the intermediate composition range the presence of acrylonitrile propagation radicals was also detected. These radicals were not observed to be formed in significant quantities on the radiolysis of polyacrylonitrile. They are believed to result from a scission of the main chain at methacrylic acid/acrylonitrile diad sequences following loss of the methacrylic acid carboxyl group. At 77 K, the copolymers with high methacrylic acid contents were found to be more sensitive to radical formation than the methacrylic acid homopolymer, but this enhanced sensitivity was not evident at ambient temperature, where the G-values for radical formation for the copolymers were slightly less than the values for the homopolymers. (C) 2003 Society of Chemical Industry.
Resumo:
The ESR spectra of poly(chlorotrifluoroethylene) were recorded following gamma-radiolysis under vacuum at room temperature and 77 K. The very broad spectrum at 77 K revealed little fine structure with which to identity the radicals formed upon irradiation, but subsequent photobleaching and annealing studies, together with radiolytic studies at higher temperatures, afforded scope for making radical assignments. Both main-chain radicals and a range of chain-end radicals have been identified. The G-values for radical formation were 1.55, 0.36 and 0.32 at 77 K, 273 K and room temperature, respectively. (C) 2003 Elsevier Science Ltd. All rights reserved.
Resumo:
Poly(tetrafluoroethylene-co-perfluoropropyI vinyl ether), PFA, was grafted with styrene from the vapor phase using a simultaneous radiation grafting method. The graft yields were measured as a function of the dose and dose rate and were found to be initially linearly dependent on the dose and independent of the dose rate up to dose rates of similar to3 kGy/h. However, at a dose rate of 6.2 kGy/h, the slope of the yield-grafting time plot decreased. Raman depth profiles of the grafts showed that the polystyrene concentrations were greatest near the surface of the grafted samples and decreased with depth. The maximum penetration depth of the graft depended on the radiation dose for a fixed dose rate. Fmoc-Rink loading tests showed that the grafts displayed superior loading compared to grafts prepared from bulk styrene or from styrene solutions other than methanol.