99 resultados para Al-cu Alloys


Relevância:

30.00% 30.00%

Publicador:

Resumo:

While the general mechanisms of hot tearing are understood, i.e. the inability of liquid to feed imposed strain on the mushy material, work continues on improving the understanding of the mechanisms at play. A hot tear test rig that measures the temperature and load imposed on the mushy zone during solidification has been successfully used to study hot tearing. The mould has now been modified to incorporate a window above the hot spot region to allow observation of hot tear formation and growth. Combining information from visual observation with load and temperature data has led to a better understanding of the mechanism of hot tearing. Tests were carried out on an Al-0.5 wt-% Cu alloy. It was found that load development began at about 90% solid and a hot tear formed a short time later, at between 93% and 96% solid. Hot tearing started at a very low load.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper investigates the relationship between mechanical properties and microstructure in high pressure die cast binary Mg-Al alloys. As-cast test bars produced using high pressure die casting have been tested in tension in order to determine the properties for castings produced using this technique. It has been shown that increasing aluminium levels results in increases in yield strength and a decrease in ductility for these alloys. Higher aluminium levels also result in a decrease in creep rate at 150 degrees C. It has also been shown that an increase in aluminium levels results in an increase in the volume fraction of eutectic Mg17Al12 in the microstructure.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This paper reviews various aspects of anodizing of magnesium alloys, such as the basics, processes, properties and applications. It systematically summarises the existing fundamental studies and technical developments of anodizing of magnesium alloys, and concludes that new anodizing processes based on electrolytic plasma anodizing that convert the surface of a magnesium alloy into a hard ceramic coating in an electrolytic bath using high energy electric discharges can offer improved wear and corrosion resistance. These new anodized coatings are often claimed to perform better than the traditional ones obtained through older anodizing processes, such as DOW17 or HAE. The new anodizing techniques are chromate free and hence environment friendly. It is expected that more cost-effective, environment-friendly and non-toxic anodizing techniques will be developed and applied to magnesium alloy components in the future.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Cu-based bulk metallic glass (BMG) composites containing in situ TiB particles were successfully fabricated. The reinforcing TiB particles with a size of 5-10 mu m are uniformly distributed in the amorphous matrix. The particles have a good bonding to the matrix with a reaction layer. The BMG composites exhibit an obvious ductility with a plastic strain of 2% for the 17.5 vol.% TiB sample due to the suppression of shear band propagation and the generation of multiple shear bands during compressive testing. The hardness of the materials is increased from Hv543 for monolithic BMG to Hv650 for 23.6 vol.% TiB-containing BMG composite. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The orientation relationship (OR) between the beta(Zn) phase and the alpha(Al) phase and the corresponding habit planes in a Zn-Al eutectoid alloy were accurately determined using convergent beam Kikuchi line diffraction patterns. In addition to the previously reported OR. [11 (2) over bar0](beta)parallel to[110](alpha), (0002)(beta)parallel to ((1) over bar 11)alpha, two new ORs were observed. They are: [11 (2) over bar0](beta)parallel to [110], ((1) over bar 101)(beta) 0.82 degrees from (002)(alpha) and [(1) over bar 100](beta)parallel to[112](alpha), (0002)(beta) 4.5 degrees from (111)(alpha). These ORs can be explained and understood using the recently developed edge-to-edge matching model. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The corrosion performance of anodised magnesium and its alloys, such as commercial purity magnesium (CP-Mg) and high-purity magnesium (HP-Mg) ingots, magnesium alloy ingots of MEZ, ZE41, AM60 and AZ91D and diecast AM60 (AM60-DC) and AZ91D (AZ91D-DC) plates, was evaluated by salt spray and salt immersion testing. The corrosion resistance was in the sequential order: AZ91D approximate to AM60 approximate to MEZ >= AZ91D-DC >= AM60-DC > HP-Mg > ZE41 > CP-Mg. It was concluded the corrosion resistance of an anodised magnesium alloy was determined by the corrosion performance of the substrate alloy due to the porous coating formed on the substrate alloy acting as a simple corrosion barrier. (c) 2006 Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Analysis of intra- and inter-phase distribution of modifying elements in aluminium-silicon alloys is difficult due to the low concentrations used. This research utilises a mu-XRF (X-ray fluorescence) technique at the SPring-8 synchrotron radiation facility X-ray source and reveals that the modifying element strontium segregates exclusively to the eutectic silicon phase and the distribution of strontium within this phase is relatively homogeneous. This has important implications for the fundamental mechanisms of eutectic modification in hypoeutectic aluminium-silicon alloys. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Recent research suggest that the iron-rich intermetallic phases, such as alpha-FeAl15(Fe,Mn)(3)Si-2 and beta-Fe Al5FeSi, nucleate on oxide films entrained in aluminum casting alloys. This is evidenced by the presence of crack-like defects within these iron-rich intermetallics. In an attempt to verify the role of oxides in nucleating iron-rich intermetallics, experiments have been conducted under conditions where in-situ entrained oxide films and deliberately added oxide particles were present. Iron-rich intermetallics are observed to be associated with the oxides in the final microstructure, and crack-like defects are often observed in the beta-Fe plates. The physical association of the Fe-rich intermetallic phases with these solid oxides, either formed in situ or added, is in accordance with the mechanism suggesting that iron-rich intermetallics nucleate upon the wetted sides of double oxide films.