We report the experimental demonstration of quantum teleportation of the quadrature amplitudes of a light field. Our experiment was stably locked for long periods, and was analyzed in terms of fidelity F and with signal transfer T-q=T++T- and noise correlation V-q=Vinparallel to out+Vinparallel to out-. We observed an optimum fidelity of 0.64+/-0.02, T-q=1.06+/-0.02, and V-q=0.96+/-0.10. We discuss the significance of both T-q>1 and V-q

Relevância:

20.00% 20.00%

Publicador:

Resumo:

For some applications for fluoropolymers they must be subjected to high-energy radiation, e.g., when they are grafted with styrene using an irradiation method to produce fuel cell membranes or matrix supports for combinatorial chemistry. In some of these applications they may be subjected to mechanical stress or elevated temperature, so it is important to elucidate the effects of the radiolysis on these properties. In the present work the effect of gamma-radiolysis on the glass transition, melting behavior, and thermal stability of PFA has been studied as well as the effect of the radiolysis on the tensile properties of the polymer.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(tetrafluoroethylene-co-perfluoropropyI vinyl ether), PFA, was grafted with styrene from the vapor phase using a simultaneous radiation grafting method. The graft yields were measured as a function of the dose and dose rate and were found to be initially linearly dependent on the dose and independent of the dose rate up to dose rates of similar to3 kGy/h. However, at a dose rate of 6.2 kGy/h, the slope of the yield-grafting time plot decreased. Raman depth profiles of the grafts showed that the polystyrene concentrations were greatest near the surface of the grafted samples and decreased with depth. The maximum penetration depth of the graft depended on the radiation dose for a fixed dose rate. Fmoc-Rink loading tests showed that the grafts displayed superior loading compared to grafts prepared from bulk styrene or from styrene solutions other than methanol.