132 resultados para Bolingbroke, Henry St. John, Viscount, 1678-1751.
Resumo:
This paper presents a critical analysis of the Bachelor of Materials Engineering programme compared with the expectations of the Institution of Engineers Australia (IEAust) and of UQ. To set the scene, the graduate attributes are listed, the programme framework is presented and the educational culture and available facilities are described Then, the programme delivery is described; this includes an analysis of the learning opportunities that allow students to develop the graduate attributes. Finally, an assessment is made of programme outcomes relating to graduate attributes.
Resumo:
An investigation was carried out into the galvanic corrosion of magnesium alloy AZ91D in contact with zinc, aluminium alloy A380 and 4150 steel. Specially designed test panels were used to measure galvanic currents under salt spray conditions. It was found that the distributions of the galvanic current densities on AZ91D and on the cathodes were different. An insulating spacer between the AZ91D anode and the cathodes could not eliminate galvanic corrosion. Steel was the worst cathode and aluminium the least aggressive to AZ91D. Corrosion products from the anode and cathodes appeared to be able to affect the galvanic corrosion process through an alkalisation, passivation, poisoning effect or shortcut effect. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
Corrosion of magnesium engine components by coolant is an important issue in the automotive industry where magnesium alloys may be used. It is of significance to understand the corrosion behaviour of pure magnesium in ethylene glycol solutions, as this can provide a basis for developing new coolants for magnesium alloy engine blocks. In this paper, through corrosion and electrochemical tests, it was found that the corrosion rate of magnesium decreased with increasing concentration of ethylene glycol. Individual contaminants, such as NaCl, NaHCO3, Na2SO4 and NaCl can make aqueous ethylene glycol solution more corrosive to magnesium. However, in NaCl contaminated ethylene glycol, NaHCO3 and Na2SO4 showed some inhibition effect. The solution resistivity played an important role in the corrosion of magnesium in ethylene glycol solutions, and the competitive adsorption of ethylene glycol and the contaminants on the magnesium surface was also responsible for the observed corrosion behaviours. The corrosion of magnesium in ethylene glycol can be effectively inhibited by addition of fluorides that react with magnesium and form a protective film on the surface. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
The corrosion behaviour of die cast magnesium alloy AZ91D aged at 160degreesC was investigated. The corrosion rate of the alloy decreases with ageing time in the initial stages and then increases again at ageing times greater than 45 h. The dependence of the corrosion rate on ageing time can be related to the changes in microstructure and local composition during ageing. Precipitation of the beta phase (Mg17Al12) occurs exclusively along the grain boundaries during ageing. The beta phase acts as a barrier, resulting in a decreasing corrosion rate in the initial stages of ageing. In the later stages, the decreasing aluminium content of alpha grains makes the alpha matrix more active, causing an increase in the corrosion rate. Electrochemical testing results also confirm the combined effects of the changes in alpha and beta phases on the corrosion resistance of the aged die cast AZ91D alloy. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
The effect of iron on the grain refinement of high-purity Mg-3%Al and Mg-91%Al alloys has been investigated using anhydrous FeCl3 as an iron additive at 750degreesC in carbon-free aluminium titanite crucibles. It was shown that grain refinement was readily achievable for both alloys. Fe- and Al-rich intermetallic particles were observed in many magnesium grains. (C) 2004 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
Different as-cast microstructures of an AlSi7Mg alloy were produced by controlling the solidification conditions. The as-cast grain size ranged from 1.4 mm to 160 mum and the morphology varied from dendritic to rosette-like to globular. The as-cast materials were then partially remelted and isothermally held at 580degreesC for microstructure evolution. The final microstructure depended on the initial as-cast microstructure and the isothermal holding time. After partial remelting and isothermal holding, coarse-grained dendritic structures were not able to evolve to a globular structure, while structures with medium sized dendritic grains evolved to a globular structure with a relatively large particle size after a long isothermal holding time. Fine-grained structures evolved to well-rounded globular grains within times ranging front 10 min to 5 min as the dendritic nature of the starting structure diminished. An empirical equation has been established to describe the relationship between the evolved microstructure and the as-cast microstructure. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
The boundary element method (BEM) was used to study galvanic corrosion using linear and logarithmic boundary conditions. The linear boundary condition was implemented by using the linear approach and the piecewise linear approach. The logarithmic boundary condition was implemented by the piecewise linear approach. The calculated potential and current density distribution were compared with the prior analytical results. For the linear boundary condition, the BEASY program using the linear approach and the piecewise linear approach gave accurate predictions of the potential and the galvanic current density distributions for varied electrolyte conditions, various film thicknesses, various electrolyte conductivities and various area ratio of anode/cathode. The 50-point piecewise linear method could be used with both linear and logarithmic polarization curves.
Resumo:
Additions of strontium to hypoeutectic aluminum-silicon alloys modify the morphology of the eutectic silicon phase from a coarse platelike structure to a fine fibrous structure. Thermal analysis, interrupted solidification, and microstructural examination of sand castings in this work revealed that, in addition to a change in silicon morphology, modification with strontium also causes an increase in the size of eutectic grains. The eutectic grain size increases because fewer grains nucleate, possibly due to poisoning of the phosphorus-based nucleants, that are active in the unmodified alloy. A simple growth model is developed to estimate the interface velocity during solidification of a eutectic grain. The model confirms, independent of microstructural observations, that the addition of 100 ppm strontium increases the eutectic grain size by at least an order of magnitude compared with the equivalent unmodified alloy. The model predicts that the growth velocity varies significantly during eutectic growth. At low strontium levels, these variations may be sufficient to cause transitions between flake and fibrous silicon morphologies depending on the casting conditions. The model can be used to rationally interpret the eutectic grain structure and silicon morphology of fully solidified aluminum-silicon castings and, when coupled with reliable thermal data, can be used to estimate the eutectic grain size.
Resumo:
A trace of beryllium can lead to dramatic grain coarsening in Mg-Al alloys at normal cooling rates. It is, however, unclear whether this effect applies to aluminium-free magnesium alloys or not. This work shows that a trace of beryllium also causes considerable grain coarsening in Mg-Zn, Mg-Ca, Mg-Ce and Mg-Nd alloys and hinders grain refinement of magnesium alloys by zirconium as well. (C) 2004 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
Objective: To evaluate whether the introduction of a national, co-ordinated screening program using the faecal occult blood test represents 'value-for-money' from the perspective of the Australian Government as third-party funder. Methods: The annual equivalent costs and consequences of a biennial screening program in 'steady-state' operation were estimated for the Australian population using 1996 as the reference year. Disability-adjusted life years (DALYs) and the years of life lost (YLLs) averted, and the health service costs were modelled, based on the epidemiology and the costs of colorectal cancer in Australia together with the mortality reduction achieved in randomised controlled trials. Uncertainty in the model was examined using Monte Carlo simulation methods. Results: We estimate a minimum or 'base program' of screening those aged 55 to 69 years could avert 250 deaths per annum (95% uncertainty interval 99-400), at a gross cost of $A55 million (95% UI $A46 million to $A96 million) and a gross incremental cost-effectiveness ratio of $A17,000/DALY (95% UI $A13,000/DALY to $A52,000/DALY). Extending the program to include 70 to 74-year-olds is a more effective option (cheaper and higher health gain) than including the 50 to 54-year-olds. Conclusions: The findings of this study support the case for a national program directed at the 55 to 69-year-old age group with extension to 70 to 74-year-olds if there are sufficient resources. The pilot tests recently announced in Australia provide an important opportunity to consider the age range for screening and the sources of uncertainty, identified in the modelled evaluation, to assist decisions on implementing a full national program.
Resumo:
Soldering reactions are commonly observed during high pressure die casting of aluminium alloys, and involve the formation and growth of interfacial intermetallics between the die and the cast alloy. It is generally believed that close to 1% Fe is necessary in the aluminium alloy to reduce soldering. However, the role of iron in the interfacial reaction has not been studied in detail. In this investigation, reaction couples were formed between H13 tool steel substrates and an Al-11Si-2.5Cu melt containing either 0.15 or 0.60% Fe. Examination revealed distinctly different intermetallic layer morphology. The overall growth and chemistry of the reaction layer and the reaction rate measured by the consumption of the substrate were compared for the two alloy melts. It was demonstrated that a higher iron content reduces the rate of interfacial reaction, consistent with an observed thicker compact ( solid) intermetallic layer. Hence, the difference in reaction rate can be explained by a significant reduction in the diffusion flux due to a thicker compact layer. Finally, the mechanism of the growth of a thicker compact layer in the higher iron melt is proposed, based on the phase relations and diffusion both within and near the interfacial reaction zone. (C) 2004 Kluwer Academic Publishers.