35 resultados para Vinyl chloride polymers


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objective: To investigate the impact characteristics of an ethylene vinyl acetate (EVA) mouthguard material with regulated air inclusions, which included various air cell volumes and wall thickness between air cells. In particular, the aim was to identify the magnitude and direction of forces within the impacts. Method: EVA mouthguard material, A mm thick and with and without air inclusions, was impacted with a constant force impact pendulum with an energy of 4.4 J and a velocity of 3 m/s. Transmitted forces through the EVA material were measured using an accelerometer, which also allowed the determination of force direction and magnitude within the impacts. Results: Statistically significant reductions in the transmitted forces were observed with all the air inclusion materials when compared with EVA without air inclusions. Maximum transmitted force through one air inclusion material was reduced by 32%. Force rebound was eliminated in one material, and reduced second force impulses were observed in all the air inclusion materials. Conclusion: The regulated air inclusions improved the impact characteristics of the EVA mouthguard material, the material most commonly used in mouthguards world wide.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Objectives: To compare transmitted forces through ethylene vinyl acetate (EVA) mouthguard material and the same EVA material with gas inclusions in the form of a closed cell foam. Method: EVA mouthguard materials with and without foam gas inclusions and 4 mm thick were impacted with a constant force from an impact pendulum. Various porosity levels in the foam materials were produced by 1%, 5%, and 10% by weight foaming agent. The forces transmitted through the EVA after energy absorption by the test materials were measured with a force sensor and compared. Results: Only minor non-significant differences in transmitted forces through the EVA with and without foam were shown. Conclusions: The inclusion of gas in the form of a closed cell foam in 4 mm thick EVA mouthguard materials did not improve the impact performance of the EVA mouthguard material.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Two studies were conducted to examine the effects of including NaCl at various rates in grain-based supplements for Friesian cows grazing established, dominant (>90%), rainfed kikuyu (Pennisetum clandestinum cv. Common) pastures during summer and autumn in a humid sub-tropical environment. In study 1 (19 January-27 March 1998), 48 cows (36 multiparous, 12 primiparous; 27-96 days postpartum) were allocated to one of four groups based on genetic merit, milk production, liveweight (LW) and days postpartum. They were fed (2.7 kg dry matter (DM) per cow, twice-a-day) one of four isoenergetic and isonitrogenous barley grain-based concentrates containing NaCl at concentrations (% as-fed) of either 0 (SC1), 1.1 (SC2), 2.2 (SC3) or 3.3 (SC4). Maximum temperature humidity index (THImax) was greater than or equal to78 during 50% of the experimental period. Concentrate NaCl content had no effect (P>0.05) on daily milk yield or LW change but daily yields of 4% fat corrected milk (FCM), fat and protein were higher (P0.05) among treatments at 7.6+/-1.24 kg DM per cow. In study 2 (18 January 1999-1 March 1999), 48 cows (32 pluriparous, 16 primiparous: 32-160 days postpartum) were fed (2.7 kg DM per cow twice-a-day) one of two isoenergetic and isonitrogenous barley grain-based concentrates containing NaCl at concentrations (% as-fed) of 0 (control) or 2.2 (HSC). THImax was greater than or equal to78 during 34% of days in the experimental period. Yields of milk, FCM, fat and protein were lower (P0.05) by concentrate NaCl content. These studies indicate that NaCl supplementation can be beneficial in terms of milk production during warm, humid conditions as opposed to milder conditions. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A comparative study has been made of the radiation grafting of styrene onto poly(tetrafluoroethylene-co-perfluoropropyl vinyl ether) (PFA) and polypropylene (PP) substrates, using the simultaneous irradiation method. Effects of grafting conditions such as monomer concentrations, type of solvent, dose rate and irradiation dose on the grafting yield were investigated. Under the same grafting conditions it was found that a higher degree of grafting of styrene was obtained using a mixture of dichloromethane/methanol solvents for PFA and methanol for PP and the degree of grafting was higher in PP than in PFA at all doses. However, the micro-Raman spectroscopy analysis of the graft revealed that, for the same degree of grafting, the penetration depth of the grafted polystyrene into the substrate was higher in PFA than in PP substrates. In both polymers the crystallinity was hardly affected by the grafting process and the degree of crystallinity decreased slightly with grafting dose. The dependence of the initial rate of grafting on the dose rate and the monomer concentration was found to be 0.6 and 1.4 order for PFA and 0.15 and 2.2 for PP, respectively. The degree of grafting increased with increasing radiation dose in both polymers. However, the grafting yield decreased with an increase in the dose rate. The increase in the overall grafting yield for PFA and PP was accompanied by a proportional increase in the penetration depth of the graft into the substrates. (C) 2003 Society of Chemical Industry.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Poly(tetrafluoroethylene-co-perfluoropropyI vinyl ether), PFA, was grafted with styrene from the vapor phase using a simultaneous radiation grafting method. The graft yields were measured as a function of the dose and dose rate and were found to be initially linearly dependent on the dose and independent of the dose rate up to dose rates of similar to3 kGy/h. However, at a dose rate of 6.2 kGy/h, the slope of the yield-grafting time plot decreased. Raman depth profiles of the grafts showed that the polystyrene concentrations were greatest near the surface of the grafted samples and decreased with depth. The maximum penetration depth of the graft depended on the radiation dose for a fixed dose rate. Fmoc-Rink loading tests showed that the grafts displayed superior loading compared to grafts prepared from bulk styrene or from styrene solutions other than methanol.