70 resultados para Eutectic Solidification
Resumo:
A framework is presented for modeling the nucleation in the constitutionally supercooled liquid ahead of the advancing solid/liquid interface. The effects of temperature gradient, imposed velocity, slope of liquidus, and initial concentration have been taken into account in this model by considering the effect of interface retardation, which is caused by solute buildup at the interface. Furthermore, the effect of solute concentration on the chemical driving force for nucleation has been considered in this model. The model is used for describing the nucleation of Al-Si and Al-Cu alloys. It was found that the solute of Si has a significant impact on the chemical driving force for nucleation in AI-Si alloys whereas Cu has almost no effect in Al-Cu alloys.
Resumo:
Recently it has been shown that modification with strontium causes an increase in the size of eutectic grains. The eutectic grain size increases because there are fewer nucleation events, possibly due to the poisoning of phosphorus-based nuclei that are active in the unmodified alloy. The current paper investigates the effect of strontium concentration on the eutectic grain size. In the aluminium-10 wt.% silicon alloy used in this research, for fixed casting conditions, the eutectic grain size increases as the strontium concentration increases up to approximately 150ppm, beyond which the grain size is relatively stable. This critical strontium concentration is likely to differ depending on the composition of the base alloy, including the concentration of minor elements and impurities. It is concluded that processing and in-service properties of strontium modified aluminium-silicon castings are likely to be more stable if a minimum critical strontium concentration is exceeded. If operating below this critical strontium concentration exceptional control over composition and casting conditions is required. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The effect of Ca addition on the microstructure, physical characteristics (density/porosity), and mechanical properties (tensile and impact strength) has been investigated in an Al-7Si-0.3Mg-xFe (x = 0.2, 0.4, and 0.7) alloy. The size of Al-Fe intermetallic platelets (beta-Al5FeSi) increased with increasing Fe content. The addition of Ca modified the eutectic microstructure and also reduced the size of intermetallic Fe-platelets, causing improved elongation and impact strengths. A low level of Ca addition (39 ppm) reduced the porosity of the alloys. The tensile strength was decreased marginally with Ca addition. However, Ca addition improved the ductility of the alloy by 18.3, 16.7, and 44 pet and the impact strength by 44, 48, and 15.8 pct for Fe contents of 0.2, 0.4, and 0.7 pct, respectively.
Resumo:
The effects of process variables on the quality of high-pressure die cast components was determined with the aid of in-cavity pressure sensors. In particular, the effects of set intensification pressure, delay time, and casting velocity have been investigated. The in-cavity pressure sensor has been used to determine how conditions within the die-cavity are related to the process parameters regulated by the die casting machine, and in turn the effect of variations in these parameters on the integrity of the final part. Porosity was found to decrease with increasing intensification pressure and increase with increasing casting velocity. The delay time before the application of the intensification pressure was not observed to have a significant effect on porosity levels. (c) 2006 Elsevier B.V. All rights reserved.