55 resultados para COLD-FORMED STEEL


Relevância:

20.00% 20.00%

Publicador:

Resumo:

This paper reports on measurements of crack growth by environmental assisted fracture (EAF) for 4340 steel in water and in air at various relative humidities. Of most interest is the observation of slow crack propagation in dry air. Fractographic analysis leads to the strong suggestion that this slow crack propagation is due to hydrogen cracking caused by internal hydrogen in solid solution inside the sample material.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The aim of this project was to investigate the properties of copper rich Cu-Fe-Cr alloys for the purpose of developing a new cost effective, high-strength, high-conductivity copper alloy. This paper reports on the influence of cold work. The age hardening response of the Cu-0.7%Cr-2.0%Fe alloy was minimal, but the resistance to softening was superior to that reported for any commercial high-strength, high-conductivity (HSHC) copper alloy with comparable mechanical and electrical properties. For example, an excess of 85% of the original hardness of the 40% cold worked alloy is retained after holding at 700 degreesC for 1 hour, whereas commercial HSHC Cu-Fe-P alloys have been reported to soften significantly after 1 hours exposure at less than 500 degreesC. The Cu-0.7Cr-2.0Fe alloy would therefore be expected to be more suitable for applications with a significant risk of exposure to elevated temperatures. Optical microscope examination of cold worked and aged microstructures confirmed the high resistance to recrystallization for Cu-0.7%Cr-2.0%Fe. The Zener-Smith drag term, predicting the pinning effect of second phase particles on dislocations in cold worked microstructures, was calculated using the precipitate characteristics obtained from TEM, WDS and resistivity measurements. The pinning effect of the precipitate dispersions in the peak-aged condition was determined to be essentially equivalent for the Cu-0.7%Cr-0.3%Fe and Cu-0.7%Cr-2.0%Fe alloys. A lower recrystallisation temperature in the Cu-0.7%Cr-0.3%Fe alloy was therefore attributed to faster coarsening kinetics of the secondary precipitates resulting from a higher Cr concentration in the precipitates at lower iron content. (C) 2001 Kluwer Academic Publishers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The dynamic theological behaviour of gamma-irradiated 12.8 wt% poly(vinyl alcohol) (PVA), 12.8 wt% poly(vinyl pyrrolidone) (PVP), and a blend of 8 wt% PVA and 4.8 wt% PVP aqueous solutions have been studied pre- and post-gelation. The non-irradiated solutions displayed theological behaviour typical of dilute to semi-dilute polymer solutions, with the complex viscosity being independent of the frequency and shear rate (i.e. Newtonian behaviour) over the range of frequencies tested and the loss modulus G(omega) and storage modulus G(omega) being nearly proportional to omega and omega(2) respectively. After a set of doses of gamma-radiation, the magnitudes of the dynamic moduli G'(omega) and G(omega) increased as the absorbed dose increased, with notable differences between the two homopolymers and the blend. The stages of gelation were effectively monitored by means of dynamic theological measurements, allowing the possible mechanisms of network formation to be elucidated. The doses required for gelation of the PVA, PVP, and blend samples, determined on the basis of the Winter and Chambon criteria for gelation, were found to be 12 kGy for the 12.8 wt% PVA, 4 kGy for the 12.8 wt% PVP, and 5 kGy for the 8 wt% PVA/4.8 wt% PVP solutions. The unexpected lower gelation dose demonstrated by the blend sample, compared with predictions based on the blend composition, and the associated gelation mechanism are also discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The paper presents methods for measurement of convective heat transfer distributions in a cold flow, supersonic blowdown wind tunnel. The techniques involve use of the difference between model surface temperature and adiabatic wall temperature as the driving temperature difference for heat transfer and no active heating or cooling of the test gas or model is required. Thermochromic liquid crystals are used for surface temperature indication and results presented from experiments in a Mach 3 flow indicate that measurements of the surface heat transfer distribution under swept shock wave boundary layer interactions can be made. (C) 2002 Elsevier Science Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of test temperature, which controls the stability of austenite, on the impact toughness of a low carbon Fe-Ni-Mn-C austenitic steel and 304 stainless steel, has been investigated. Under impact conditions, stress-induced martensitic transformation occurred, in a region near the fracture surface, at test temperatures below 80degreesC for the Fe-Ni-Mn-C steel and below -25degreesC for 304 stainless steel. The former shows significant transformation toughening and the highest impact toughness was obtained at 10degreesC, which corresponds to the maximum amount of martensite formed by stress-induced transformation above the Ms temperature. The stress-induced martensitic transformation contributes negatively to the impact toughness in the 304 stainless steel. Increasing the amount of stress-induced transformation to martensite, lowered the impact toughness. The experimental results can be well explained by the Antolovich theory through the analysis of metallography and fractography. The different effect of stress-induced transformation on the impact toughness in Fe-Ni-Mn-C steel and 304 stainless steel has been further understood by applying the crystallographic model for stress-induced martensitic transformation to these two steels. (C) 2002 Kluwer Academic Publishers.

Relevância:

20.00% 20.00%

Publicador:

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Injury to endothelial calls is thought to be important to the development of the vascular lesion of chronic rejection. It was the aim of this study to develop a semiquantitative method to assess endothelial injury in arterial grafts and to document the injury produced by cold storage preservation and additional warm ischaemia. Twelve- and 24-h cold preservation of rat aortic segments, together with an additional 1 h of warm ischaemia, were assessed. Electron micrographs of representative endothelial cells were scored for cytoplasmic, nuclear and mitochondrial injury. The overall injury score was obtained by addition of the individual scores. Storage for up to 24 h in University of Wisconsin (UW) and Terasaki did not produce any injury. Twenty-four hours of storage in Euro-Collins resulted in endothelial cell death. Injury occurred after 12 h of storage in Ross, Collins and normal saline, and the injury increased following 24 h of storage. One hour of warm ischaemia did not increase the injury. Injury to endothelial cells varies with the preservation solution used and the time of cold storage, so that both the type of solution and the storage time should be taken into account in clinical studies looking at the influence of cold ischaemia time and graft outcome.

Relevância:

20.00% 20.00%

Publicador: