93 resultados para styrene-divinylbenzene-vinylpyridine copolymers


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Simultaneous and preirradiation grafting of styrene onto fluorinated polyolefins does not enable control of the molecular weights or polydispersities of the styrene grafts. The nitroxide-mediated grafting of styrene onto PFA with TEMPO and TEISO using a preirradiation method has been investigated as a means of controlling the graft properties and especially to produce grafts with improved suitability for SPOC. The yields of graft were found to be in the range 15-20% for nitroxide concentrations between 5 x 10(-3) and 2 x 10(-2) M and were similar for the two nitroxides studied. Raman mapping was used to obtain the depth profile for the styrene grafts. The grafts were found to be principally located within the PFA substrate, and little graft was formed at the PFA surface. Fmoc loading tests were performed to assess the suitability of the grafted PFA as a support for SPOC, but these showed no significant loading was achieved, thus indicating that the graft properties are not suitable for SPOC. However, the study has important implications for the applications of PFA-grafted polymers in other areas, such as chemically resistant ion-exchange and separation membranes.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Well-mixed blends of poly(ethylene) and poly(styrene) have been synthesized using supercritical carbon dioxide as a solvent. The morphology of the blends has been conclusively characterized using differential scanning calorimetry (DSC), small-angle X-ray scattering (SAXS), Raman microprobe microscopy, and C-13 solid-state cross-polarization magic angle spinning NMR (C-13 CPMAS NMR). DSC measurements demonstrate that poly(styrene) in the blends resides solely in the amorphous regions of the poly(ethylene) matrix; however, corroborative evidence from the SAXS experiments shows that poly(styrene) resides within the interlamellar spaces. The existence of nanometer-sized domains of poly(styrene) was shown within a blend of poly(styrene) and poly(ethylene) when formed in supercritical carbon dioxide using Raman microprobe microscopy and C-13 CPMAS NMR spectroscopy coupled with a spin diffusion model. This contrasts with blends formed at ambient pressure in the absence of solvent, in which domains of poly(styrene) in the micrometer size range are formed. This apparent improved miscibility of the two components was attributed to better penetration of the monomer prior to polymerization and increased swelling of the polymer substrate by the supercritical carbon dioxide solvent.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Block copolymers have become an integral part of the preparation of complex architectures through self-assembly. The use of reversible addition-fragmentation chain transfer (RAFT) allows blocks ranging from functional to nonfunctional polymers to be made with predictable molecular weight distributions. This article models block formation by varying many of the kinetic parameters. The simulations provide insight into the overall polydispersities (PDIs) that will be obtained when the chain-transfer constants in the main equilibrium steps are varied from 100 to 0.5. When the first dormant block [polymer-S-C(Z)=S] has a PDI of 1 and the second propagating radical has a low reactivity to the RAFT moiety, the overall PDI will be greater than 1 and dependent on the weight fraction of each block. When the first block has a PDI of 2 and the second propagating radical has a low reactivity to the RAFT moiety, the PDI will decrease to around 1.5 because of random coupling of two broad distributions. It is also shown how we can in principle use only one RAFT agent to obtain block copolymers with any desired molecular weight distribution. We can accomplish this by maintaining the monomer concentration at a constant level in the reactor over the course of the reaction. (c) 2005 Wiley Periodicals, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The use of phenyldithioacetic acid (PDA) in homopolymerizations of styrene or methyl acrylate produced only a small fraction of chains with dithioester end groups. The polymerizations using 1-phenylentyl phenyldithioacetate (PEPDTA) and PDA in the same reaction showed that PDA had little or no influence on the rate or molecular weight distribution even when a 1:1 ratio is used. The mechanistic pathway for the polymerizations in the presence of PDA seemed to be different for each monomer. Styrene favors addition of styrene to PDA via a Markovnikov type addition to form a reactive RAFT agent. The polymer was shown by double detection SEC to contain dithioester end groups over the whole distribution. This polymer was then used in a chain extension experiment and the M-n was close to theory. A unique feature of this work was that PDA could be used to form a RAFT agent in situ by heating a mixture of styrene and PDA for 24 h at 70 degrees C and then polymerizing in the presence of AIBN to give a linear increase in Mn and low values of PDI (< 1.14). In the case of the polymerization of MA with PDA, the mechanism was proposed to be via degradative chain transfer. (c) 2005 Wiley Periodicals, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The radiolysis of a poly(ethylene-co-propylene), Elpro, marketed by Thai Polypropylene Co. Ltd for the manufacture of medical goods has been investigated at 77 K. Calcium stearate was blended with the Elpro as a processing aid; and dioctyl phthalate, DOP, was added in various amounts as a radiation stabilizer. The ESR spectra of Elpro and Elpro+Ca were very similar and characterized principally by the presence of PP a-carbon radicals. The spectra of the samples containing DOP were similar to those for Elpro but with an additional narrow singlet arising from DOP radicals. On annealing the irradiated polymers to higher temperatures, the singlet was lost between 250 and 270 K, and at room temperature the principal radicals remaining were allyl radicals. The G-values for radical formation at 77 K for Elpro and Elpro+Ca at 77 K were 3.0 and 3.2, respectively, but incorporation of DOP resulted in lower G-values, ranging from 1.6 to 1.4 for 0.5 and 2.5 phr DOP, respectively.(c) 2005 Wiley Periodicals, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Expanded polytetrafluoroethylene (ePTFE) membranes were modified by graft copolymerization with methacryloxyethyl phosphate (MOEP) in methanol and 2-butanone (methyl ethyl ketone (MEK)) at ambient temperature using gamma irradiation. The effect of dose rate (0.46 and 4.6 kGyh(-1)), monomer concentration (1-40 %) and solvent were studied and the modified membranes were characterized by weight increase, X-ray photoelectron spectroscopy (XPS), Fourier transform infrared spectroscopy (FTIR) and scanning electron microscopy (SEM). XPS was used to determine the % degree of surface coverage using the C-F (ePTFE membrane) and the C-C (MOEP graft copolymer) peaks. Grafting yield, as well as surface coverage, were found to increase with increasing monomer concentration and were significantly higher for samples grafted in MEK than in methanol solution. SEM images showed distinctly different surface morphologies for the membranes grafted in methanol (smooth) and MEK (globular), hence indicating phase separation of the homopolymer in MEK. We propose that in our system, the non-solvent properties of MEK for the homopolymer play a more important role than solvent chain transfer reactions in determining grafting outcomes. (c) 2005 Society of Chemical Industry.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This article reports thermoset blends of bisphenol A-type epoxy resin (ER) and two amphiphilic four-arm star-shaped diblock copolymers based on hydrophilic poly(ethylene oxide) (PEO) and hydrophobic poly(propylene oxide) (PPO). 4,4'-Methylenedianiline (MDA) was used as a curing agent. The first star-shaped diblock copolymer with 70 wt% ethylene oxide (EO), denoted as (PPO-PEO)(4), consists of four PPO-PEO diblock arms with PPO blocks attached on an ethylenediamine core; the second one with 40 wt% EO, denoted as (PEO-PPO)(4), contains four PEO-PPO diblock arms with PEO blocks attached on an ethylenediamine core. The phase behavior, crystallization, and nanoscale structures were investigated by differential scanning calorimetry, transmission electron microscopy, and small-angle X-ray scattering. It was found that the MDA-cured ER/(PPO-PEO)(4) blends are not macroscopically phase-separated over the entire blend composition range. There exist, however, two microphases in the ER/(PPO-PEO)(4) blends. The PPO blocks form a separated microphase, whereas the ER and the PEO blocks, which are miscible, form another microphase. The ER/(PPO-PEO)(4) blends show composition-dependent nanostructures on the order of 10-30 nm. The 80/20 ER/(PPO-PEO)(4) blend displays spherical PPO micelles uniformly dispersed in a continuous ER-rich matrix. The 60/40 ER/(PPO-PEO)(4) blend displays a combined morphology of worm-like micelles and spherical micelles with characteristic of a bicontinuous microphase structure. Macroscopic phase separation took place in the MDA-cured ER/(PEO-PPO)(4) blends. The MDA-cured ER/(PEO-PPO)(4) blends with (PEO-PPO)(4) content up to 50 wt% exhibit phase-separated structures on the order of 0.5-1 mu m. This can be considered to be due to the different EO content and block sequence of the (PEO-PPO)(4) copolymer. (c) 2006 Wiley Periodicals, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report the successful RAFT-mediated emulsion polymerization of styrene using a non-ionic surfactant (Brij98), the highly reactive 1-phenylethyl phenyldithioacetate (PEPDTA) RAFT agent, and water-soluble initiator ammonium persulfate (APS). The molar ratio of RAFT agent to APS was identical in all experiments. Most of the monomer was contained within the micelles, analogous to microemulsion or miniemulsion systems but without the need of shear, sonication, cosurfactant, or a hydrophobe. The number-average molecular weight increased with conversion and the polydispersity index was below 1.2. This ideal 'living' behavior was only found when molecular weights of 9000 and below were targeted. It was postulated that the rapid transportation of RAFT agent from the monomer swollen micelles to the growing particles was fast on the polymerization timescale, and most if not all the RAFT agent is consumed within the first 10% conversion. In addition, it was postulated that the high nucleation rate from the high rate of exit ( of the R radical from the RAFT agent) and high entry rate from water-phase radicals ( high APS concentration) reduced the effects of 'superswelling' and therefore a similar molar ratio of RAFT agent to monomer was maintained in all growing particles. The high polydispersity indexes found when targeting molecular weights greater than 9000 were postulated to be due to the lower nucleation rate from the lower weight fractions of both APS and RAFT agent. In these cases, 'superswelling' played a dominant role leading to a heterogeneous distribution of RAFT to monomer ratios among the particles nucleated at different times.