66 resultados para magnesium-based alloys
Resumo:
Hydrogen storage in traditional metallic hydrides can deliver about 1.5 to 2.0 wt pct hydrogen but magnesium hydrides can achieve more than 7 wt pct. However, these systems suffer from high temperature release drawback and chemical instability problems. Recently, big improvements of reducing temperature and increasing kinetics of hydrogenation have been made in nanostructured Mg-based composites. This paper aims to provide an overview of the science and engineering of Mg materials and their nanosized composites with nanostructured carbon for hydrogen storage. The needs in research including preparation of the materials, processing and characterisation and basic mechanisms will be explored. The preliminary experimental results indicated a promising future for chemically stable hydrogen storage using carbon nanotubes modified metal hydrides under lower temperatures.
Resumo:
A magnesium alloy of eutectic composition (33 wt-'%Al) was directionally solidified in mild steel tubes at two growth rates, 32 and 580 mum s(-1,) in a temperature gradient between 10 and 20 K mm(-1). After directional solidification, the composition of each specimen varied dramatically, from 32'%Al in the region that had remained solid to 18%Al (32 mum s(-1) specimen) and 13%Al (580 mum s(-1) specimen) at the plane that had been quenched from the eutectic temperature. As the aluminium content decreased, the microstructure contained an increasing volume fraction of primary magnesium dendrites and the eutectic morphology gradually changed from lamellar to partially divorced. The reduction in aluminium content was caused by the growth of an Al-Fe phase ahead of the Mg-Al growth front. Most of the growth of the Al-Fe phase occurred during the remelting period before directional solidification. The thickness of the Al-Fe phase increased with increased temperature and time of contact with the molten Mg-Al alloy. (C) 2003 Maney Publishing.
Resumo:
The effect of increasing levels of silicon on the microstructure and creep properties of high-pressure die-cast Mg-Al-Si (AS) alloys has been investigated. The morphology of the Mg2Si phase in die-cast AS alloys was found to be a function of the silicon content. The Mg2Si particles in castings with up to 1.14 wt pct Si have a Chinese script morphology. For AS21 alloys with silicon contents greater than 1.4 wt pet Si (greater than the alpha-Mg2Si binary eutectic point), some Mg2Si particles have a coarse blocky shape. Increasing the silicon content above the eutectic level results in an increase in the number of coarse faceted Mg2Si particles in the microstructure. Creep rates at 100 hours were found to decrease with increasing silicon content in AS-type alloys. The decrease in creep rate was most dramatic for silicon contents up to 1.1 wt pct. Further additions of silicon of up to 2.64 wt pct also resulted in significant decreases in creep rate.
Resumo:
The effect of the beta phase in Mg-Al alloys on the corrosion performance of an anodised coating was studied. It was found that the corrosion resistance of the anodised coating was closely associated with the corrosion performance of the substrate alloy. In particular, Mg alloys with a dual phase microstructure of alpha + beta with intermediate aluminium contents (namely 5%, 10% and 22% Al) after anodisation had the highest corrosion rate and the worst corrosion resistance provide by the anodised coating. The poor performance of an anodised coating was attributed partly to lower corrosion resistance of the substrate alloy and partly to the higher porosity of the anodised coating. (c) 2004 Elsevier Ltd. All rights reserved.
Resumo:
This paper investigates the relationship between mechanical properties and microstructure in high pressure die cast binary Mg-Al alloys. As-cast test bars produced using high pressure die casting have been tested in tension in order to determine the properties for castings produced using this technique. It has been shown that increasing aluminium levels results in increases in yield strength and a decrease in ductility for these alloys. Higher aluminium levels also result in a decrease in creep rate at 150 degrees C. It has also been shown that an increase in aluminium levels results in an increase in the volume fraction of eutectic Mg17Al12 in the microstructure.
Resumo:
Manganese is a grain refiner for high purity Mg-3%Al, Mg-6%Al, Mg-9%Al, and commercial AZ31 (Mg-3%Al-1%Zn) alloys when introduced in the form of an Al-60%Mn master alloy splatter but the use of pure Mn flakes and ALTAB (TM) Mn75 tablets shows no grain refinement. Long time holding of the melt at 730 degrees C leads to an increase in grain size. The mechanism is attributed to the presence of all epsilon-AlMn phase (hexagonal close-packed) in the master alloy splatter. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
This review aims to provide a foundation for the safe and effective use of magnesium (Mg) alloys, including practical guidelines for the service use of Mg alloys in the atmosphere and/or in contact with aqueous solutions. This is to provide support for the rapidly increasing use of Mg in industrial applications, particularly in the automobile industry. These guidelines should be firmly based on a critical analysis of our knowledge of SCC based on (1) service experience, (2) laboratory testing and (3) understanding of the mechanism of SCC, as well as based on an understanding of the Mg corrosion mechanism.
Resumo:
Magnesium and its alloys have shown a great potential in effective hydrogen storage due to their advantages of high volumetric/ gravimetric hydrogen storage capacity and low cost. However, the use of these materials in fuel cells for automotive applications at the present time is limited by high hydrogenation temperature and sluggish sorption kinetics. This paper presents the recent results of design and development of magnesium-based nanocomposites demonstrating the catalytic effects of carbon nanotubes and transition metals on hydrogen adsorption in these materials. The results are promising for the application of magnesium materials for hydrogen storage, with significantly reduced absorption temperatures and enhanced ab/desorption kinetics. High level Density Functional Theory calculations support the analysis of the hydrogenation mechanisms by revealing the detailed atomic and molecular interactions that underpin the catalytic roles of incorporated carbon and titanium, providing clear guidance for further design and development of such materials with better hydrogen storage properties.
Resumo:
The yield strength of high-pressure diecast (hpdc) test bars of alloy AZ91 increases with decreasing section thickness while its hardness remains approximately constant. This behaviour is in contrast with that of the gravity cast alloy, whose hardness scales with the yield strength. Vickers hardness measured on the surface of hpdc test bars using increasing loads shows that the subsurface porosity layer usually found in hpdc material may gradually collapse under the indent, lowering the hardness. However, this is insufficient to explain the lack of correlation between hardness and yield strength. It is argued that the low strain-hardening rate of high-pressure diecast material leads to lower than expected hardness values. In addition, it is shown that the plastic zone under a macro indentation is largely contained by the softer core of the castings, rendering hardness insensitive to the casting thickness. It is concluded that macrohardness is too coarse a tool for a meaningful determination of the strength of hpdc material. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Microhardness maps of cross-sections of high-pressure diecast test bars of AZ91 have been determined. Specimens with rectangular cross-sections, 1, 2 and 3 mm thick, or with a circular cross-section 6.4 mm in diameter, have been studied. The hardness is generally higher near the edges in all specimens, and more so near the corners of the rectangular specimens. The hardness at the center of the castings is generally lower, due to a coarser solidification microstructure and the concentration of porosity. The evidence confirms that the surface of the castings is harder than the core, but it does not support the concept of a skin with a sharp. and definable boundary. This harder layer is irregular in hardness and depth and is not equally hard on opposite sides of the casting. The mean hardness obtained by integrating the microhardness maps over the entire cross-section increased with decreasing thickness of the bars, and was found to be in good correlation with each bar's yield strength. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
This paper reports a study on nanostructured magnesium composites with carbon nanotubes (CNTs) and catalytic transition metals with high H-2 adsorption capacity and fast adsorption kinetics at reduced hydrogenation temperatures. Nanostructures in such a composite are shown to be responsible for improvements in both adsorption capacity and kinetics. It is found that the carbon nanotubes significantly increase the hydrogen storage capacity, and the catalytic transition metals (Fe and Ti) greatly improve the kinetics. This could be understood from the enhancement of diffusion by CNTs and decrease in energy barrier of hydrogen dissociation at the magnesium surface.
Resumo:
Optical metallographic techniques for grain-size measurement give unreliable results for high pressure diecast Mg-Al alloys and electron back-scattered diffraction mapping (EBSD) provides a good tool for improving the quality of these measurements. An application of EBSD mapping to this question is described, and data for some castings are presented. Ion-beam milling was needed to prepare suitable samples, and this technique is detailed. As is well-known for high pressure die castings, the grain size distribution comprises at least two populations. The mean grain size of the fine-grained population was similar in both AZ91 and AM60 and in two casting thicknesses (2 mm and 5 mm) and, contrary to previously published reports, it did not vary with depth below the surface.