UV and visible photoconductivity and electrical features of undoped diamond thin films grown by microwave plasma-assisted chemical vapour deposition (MP-CVD) on silicon and copper substrates are studied. The results are correlated with morphology properties analysed by atomic force microscopy (AFM) and micro-Raman. The photoconductivity presents several bands from 1.8 to 3.8 eV that are dependent on the substrate used to grow the samples in spite of some common bands observed. The J-V curve tin DC) in samples grown on Si has a rectifier behaviour (Schottky emission) in opposition to the samples grown on Cu that have no rectification (SCLC conduction). With these results we can conclude that diamond based optoelectronic devices behaviour is controlled by two kinds of structural defects localized in microcrystal and in its boundaries. A general structure model for the optoelectronic behaviour is discussed. (C) 2000 Elsevier Science S.A. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The properties of microelectrical conduction in microwave plasma assisted chemical vapour deposition (MPCVD) diamond films were investigated using an atomic force microscopy probe, giving a morphological map of the electrical conduction with a spatial resolution better than 500 nm. Also, a cathodoluminescence map with a spatial resolution of about 1 mu m was obtained, giving the possibility of correlating the defects involved in the different carrier transport phenomena. Using micro-Raman analysis several bands could be identified. It is found that the defects responsible for the cathodoluminescence (CL) blue band are responsible for the major part of the electrical conduction in diamond films, while the defects localised in < 111 > surfaces, responsible for the green CL emission, could be involved in a less conductive process. (C) 2000 Elsevier Science S.A. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work metal - Microwave Plasma CVD diamond Schottky devices were studied. The current density vs. applied voltage reveals rectification ratios up to 10(4) at \ +/- 2V \. Under illumination an inversion and increase of the rectification is observed. The carrier density is 10(15) cm(-3) and the ideality factors near 1.5. The dark current vs. temperature shows that below 150 K the bulk transport is controlled by a hopping process with a density of defects of 10(16) cm(-3). For higher temperatures an extrinsic ionisation with activation energy of 0.3 eV takes place. The correlation with the polycrystalline nature of the samples is focused.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Free standing diamond films were used to study the effect of diamond surface morphology and microstructure on the electrical properties of Schottky barrier diodes. By using free standing films both the rough top diamond surface and the very smooth bottom surface are available for post-metal deposition. Rectifying electrical contacts were then established either with the smooth or the rough surface. The estimate of doping density from the capacitance-voltage plots shows that the smooth surface has a lower doping density when compared with the top layers of the same film. The results also show that surface roughness does not contribute significantly to the frequency dispersion of the small signal capacitance. The electrical properties of an abrupt asymmetric n(+)(silicon)-p(diamond) junction have also been measured. The I-V curves exhibit at low temperatures a plateau near zero bias, and show inversion of rectification. Capacitance-voltage characteristics show a capacitance minimum with forward bias, which is dependent on the environment conditions. It is proposed that this anomalous effect arises from high level injection of minority carriers into the bulk.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The electrical and photoconductive features of as-grown microwave-plasma-assisted chemical-vapour deposition (MPCVD) diamond films are studied in correlation with magnetic results obtained from electron paramagnetic resonance (EPR). Also, the morphology is analysed by atomic force microscopy (AFM) showing [111] crystals with a good uniformity of the deposit. The photoresponse as well the current-voltage features observed show an efficient photogeneration of carriers while the optoelectronic characteristics of the metal-diamond junction have an ideality factor of 1.6 together with a rectification ratio of about 10(4) at +/-2.5 V. The nature of the mechanisms responsible for the conduction is discussed. (C) 1998 Elsevier Science S.A.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effects of an increase in cod end mesh size from 55 to 60 and 70 mm and a change of mesh configuration from 55 mm diamond to 55 turn square mesh on the size selectivity of four by-catch species (the red shrimp Aristeus antennatus, the European hake Merluccius merluccius, the horse mackerel Trachurus trachurus and the blue whiting Micromesistius poutassou) commonly captured in the crustacean fishery off the Portuguese south coast, were evaluated. Selectivity parameters for blue whiting, the most abundant species in the catches, were estimated taking into account between-haul variation, while for the remaining species, captured in much lower quantities, the selectivity estimates were based on pooled data by length class for all hauls within the same cod end. Length at 50% retention, L-50, was found to increase with mesh size and with the change in mesh configuration for all the studied species. For blue whiting trawling depth and cod end catch were found to play a role in between-haul variation by increasing L-50 as well. The results suggest that an increase in the current minimum mesh size of 55-70 mm would be advisable to be compatible with the minimum landing sizes (MLSs) of 29 mm carapace length and 27 cm total length for red shrimp and hake, respectively, while it would greatly reduce the amount of discards, particularly those for blue whiting, that accounted for approximately 50% of the total catch weight. Horse mackerel was the only species for which the use of a larger mesh size would result in a significant escapement of individuals above the MLS of 15 cm. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effects of an increase in cod end mesh size from 55 to 60 and 70 mm and a change of mesh configuration from diamond to square mesh on the size selectivity for rose shrimp Parapenaeus longirostris and Norway lobster Nephrops norvegicus captured off the Portuguese south coast were evaluated. The results were analysed taking into account between-haul variation in selectivity, and indicate a significant increase in L-50 for rose shrimp with an increase in mesh size or with the use of a square mesh cod end, while for Norway lobster only mesh configuration was found to affect this parameter. Two other important external variables were identified; the trawling depth and the cod end catch, which influence between-haul variation, by increasing the selection range for rose shrimp and Norway lobster, respectively. The results obtained suggest that an increase in the current minimum mesh size of 55 mm would be advisable for rose shrimp in order to respect the minimum landing size of 24 mm carapace length presently established for this species. Moreover, trawling for rose shrimp should be avoided at depths above 200 m, in order to avoid catches consisting almost exclusively of juveniles. Such an increase in mesh size would have a minor impact in terms of losses of individuals above the minimum landing size for Norway lobster and would contribute to reducing the amount of discards in this fishery. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Tese de dout., Ciências e Tecnologias das Pescas, Faculdade de Ciências do Mar e do Ambiente, Univ. do Algarve, 2003