2 resultados para LIQUID-METAL

em Repositório Institucional da Universidade de Aveiro - Portugal


Relevância:

60.00% 60.00%

Publicador:

Resumo:

The current project assesses potential molten alloy anodes for Solid Oxide Fuel Cells (SOFC) running on solid waste. A detailed phase diagram study was performed to locate probable anode systems. The molten metal oxide system PbO-Sb2O3 was selected as a possible molten alloy anode for this application. A detailed vapour pressure study of this system was performed. Several cells were fabricated to experimentally assess the electrochemical properties of this system. The work reveals several unexpected limiting features such as the incompatibility between the platinum and the chosen alloy. A second cell was built, this time using rhenium wires instead, preventing such reaction. However, the rhenium wire sublimes under oxidizing conditions (air) and the sealing glass and the chosen alloy system react with each other under long term use. Considering all these issues, a third cell design was conceived, surpassing some obstacles and providing some initial information regarding the electrochemical behaviour. The current project shows that many parameters need to be taken into account to ensure materials compatibility. For the PbOSb2O3 system, the high volatility of Sb2O3 was a serious limitation that can only be addressed through the application of new contact wires or sealing materials and conditions. Nonetheless, the project highlights several other potential systems that can be considered, such as Pb11Ge3O17, Pb3GeO5, Pb5Ge3O11, Bi2CuO4, Bi2PdO4, Bi12GeO20.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The main objective of this work is the development of a hardmetal components (WC-6%Co) recovery method by thermal deposition process. The thermal deposition technique used was HVOF (high velocity oxygen-fuel). The HVOF enables depositions of thick coatings (100-500 µm) with low porosity levels, high hardness and excellent adhesion. Before deposition, hardmetal samples with different geometries (plates and cylinders) were finished in order to have different roughness. The influence of these parameters in adhesion was studied. After this step, different re-sintering temperatures were used, in order to determine which one allows to obtain the maxima densification, elements distribution and metallurgical bonding. The re-sintering promotes the densification of the coating, with an increase of its hardness and metallurgical bonding formation. The inclusion of an intermetallic layer was tested along with different layer parameters. In liquid phase sintering (1383 and 1455 ºC) a complete densification of the coating occurred, while a bonding between the substrate and the coating only partially happened. The results of SEM/EDS show low levels of porosity and a complete and uniform distribution of the elements of the alloy. The cylindrical samples without intermetallic layer showed the lowest level of porosity and best metallurgical bonding. When the substrate surface was polished (Ra = 0.05 mm) lower levels of porosity and greater metallurgical bonding were found for both geometries. Taking into account the results obtained in this study, we can conclude that the implementation of this process is appropriate for cylindrical components with a polished surface. In these components the intermetallic layer is unnecessary and punctual defects like pores can be repaired with this process.