2 resultados para 3R REGENERATION
em Repositório Institucional da Universidade de Aveiro - Portugal
Resumo:
This thesis aims at improving the knowledge on the post-fire vegetation regeneration. For that, forests and shrublands were studied, after forest fires and experimental fires. Maritime Pine (Pinus pinaster) recruitment after fire was studied. Fire severity was evidenced as a major effect on this process. High crown fire severity can combust the pines, destroying the seed bank and impeding post fire pine recruitment. However, crown combustion also influences the post-fire conditions on the soil surface, since high crown combustion (HCC) will decrease the postfire needle cast. After low crown combustion (LCC) (scorched rather than torched crowns), a considerable needle cover was observed, along with a higher density of pine seedlings. The overall trends of post-fire recruitment among LCC and HCC areas could be significantly attributed to cover by needles, as well by the estimation of fire severity using the diameters of the burned twigs (TSI). Fire increased the germination from the soil seed bank of a Pinus pinaster forest, and the effects were also related with fire severity. The densities of seedlings of the dominant taxa (genus Erica and Calluna vulgaris) were contrastingly affected in relation to the unburned situation, depending on fire severity, as estimated from the degree of fire-induced crown damage (LCC/HCC), as well as using a severity index based on the diameters of remaining twigs (TSI). Low severity patches had an increase in germination density relatively to the control, while high severity patches suffered a reduction. After an experimental fire in a heathland dominated by Pterospartum tridentatum, Erica australis and E. umbellata, no net differences in seedling emergence were observed, in relation to the pre-fire situation. However, rather than having no effect, the heterogeneity of temperatures caused by fire promoted caused divergent effects over the burned plot in terms of Erica australis germination – a progressive increased was observed in the plots were maximum temperature recorded ranged from 29 to 42.5ºC and decreased in plots with maximum temperature ranging from 51.5 to 74.5ºC. In this heathland, the seed density of two of the main species (E. australis and E. umbellata) was higher under their canopies, but the same was not true for P. tridentatum. The understory regeneration in pine and eucalypt stands, 5 to 6 years post fire, has been strongly associated with post-fire management practices. The effect of forest type was, comparatively, insignificant. Soil tilling, tree harvesting and shrub clearance, were linked to lower soil cover percentages. However, while all these management operations negatively affected the cover of resprouters, seeders were not affected by soil tilling. A strong influence of biogeographic region was identified, suggesting that more vulnerable regions may suffer higher effects of management, even under comparatively lower management pressure than more productive regions. This emphasizes the need to adequate post-fire management techniques to the target regions.
Resumo:
Bioactive glasses and glass-ceramics are a class of third generation biomaterials which elicit a special response on their surface when in contact with biological fluids, leading to strong bonding to living tissues. The purpose of the present study was to develop diopside based alkali-free bioactive glasses in order to achieve good sintering behaviour, high bioactivity, and a dissolution/ degradation rates compatible with the target applications in bone regeneration and tissue engineering. Another aim was to understand the structure-property relationships in the investigated bioactive glasses. In this quest, various glass compositions within the Diopside (CaMgSi2O6) – Fluorapatite (Ca5(PO4)3F) – Tricalcium phosphate (3CaO•P2O5) system have been investigated. All the glasses were prepared by melt-quenching technique and characterized by a wide array of complementary characterization techniques. The glass-ceramics were produced by sintering of glass powders compacts followed by a suitable heat treatment to promote the nucleation and crystallization phenomena. Furthermore, selected parent glass compositions were doped with several functional ions and an attempt to understand their effects on the glass structure, sintering ability and on the in vitro bio-degradation and biomineralization behaviours of the glasses was made. The effects of the same variables on the devitrification (nucleation and crystallization) behaviour of glasses to form bioactive glass-ceramics were also investigated. Some of the glasses exhibited high bio-mineralization rates, expressed by the formation of a surface hydroxyapatite layer within 1–12 h of immersion in a simulated body fluid (SBF) solution. All the glasses showed relatively lower degradation rates in comparison to that of 45S5 Bioglass®. Some of the glasses showed very good in vitro behaviour and the glasses co-doped with zinc and strontium showed an in vitro dose dependent behaviour. The as-designed bioactive glasses and glass–ceramic materials are excellent candidates for applications in bone regeneration and for the fabrication of scaffolds for tissue engineering.